J. L. Marshall, J. Calderon, D. Miiller, M. Desimone, J. Sees, G. Lucey, J. Hwang
{"title":"Composite solders","authors":"J. L. Marshall, J. Calderon, D. Miiller, M. Desimone, J. Sees, G. Lucey, J. Hwang","doi":"10.1109/ECTC.1991.163948","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163948","url":null,"abstract":"Development of composite solders has been performed utilizing an intermetallic compound interspersed in a solder matrix. The principal work has been done on Cu/sub 6/Sn/sub 5/ intermetallic in 60/40 Sn/Pb. The composite solder was prepared by mixing powdered intermetallic in solder paste, with subsequent reflow. Formulations of 10-40% intermetallic (by weight) were investigated. Optical inspection of cross sections demonstrates that the differentiation of the three phases (Sn, Pb, Cu/sub 6/Sn/sub 5/) is not easy, owing to the similar appearance of Sn and Cu/sub 6/Sn/sub 5/; however, etching with ammonium fluoride/hydrogen peroxide preferentially removes the tin and darkens the lead, making characterization facile. Alternatively, scanning electron micrographs/energy dispersive X-ray (SEM/EDX) analysis of cross sections, using the backscattered detection mode, is an excellent tool for microcharacterization. The mechanical properties of composite solder were examined and were found to be superior to those of standard tin/lead solder. Solder joints were readily prepared utilizing the composite solder and were forced to failure by thermocyclic fatigue; the mechanism of failure was the same as for 60/40 Sn/Pb solder, i.e., heterogeneous coarsening.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"7 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"121183230","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
S. Ito, T. Nishioka, S. Oizumi, K. Ikemura, K. Igarashi
{"title":"Molding compounds for thin surface mount packages and large chip semiconductor devices","authors":"S. Ito, T. Nishioka, S. Oizumi, K. Ikemura, K. Igarashi","doi":"10.1109/ECTC.1991.163875","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163875","url":null,"abstract":"It is noted that surface mounted devices have two major requirements: (1) resistance to the 'popcorn' phenomenon during the solder application process: and (2) minimization of stresses to the chip during the thermal shock process. Generally, there is a tradeoff relationship between these two properties. The range of importance of these two properties depends on the package types. Thicker surface mounted devices such as the PLCC (plastic leaded chip carrier) shows very little or no effect of the popcorn phenomenon. Cracks in passivation glass easily occur during thermal shock cycling. On the other hand TSOP or VQFP packages crack easily when subjected to the soldering process, while chip stresses are reduced during temperature shock cycling when compared to thicker packages such as PQFP and PLCC. The authors present analytical and experimental results for these two phenomena and discuss required properties for molding compounds or different types of surface mounted devices.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"116 3 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"124414805","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"Hermetic sealing process with atmospheric pressure vibration for LSI packages","authors":"Y. Fujita, M. Tokuda, K. Mizuishi","doi":"10.1109/33.105122","DOIUrl":"https://doi.org/10.1109/33.105122","url":null,"abstract":"The authors present a novel hermetic soldering technique, the atmospheric pressure vibration process, which periodically changes the ambient pressure while the solder is fused at the sealing area of the LSI package. The kinetic energy induced by the ambient pressure change improves the wettability of the fused solder, which results in realizing a good hermeticity of the sealing area without mechanically handling the package. The sealing apparatus is made to control the two key parameters of the kinetic energy, the amplitude and the risetime of the ambient pressure change. The mechanism of this process to improve the hermeticity is investigated with a soft X-ray micrograph analysis for the sealed packages.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"144 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"123281242","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"Qualification and reliability of thermoelectric coolers for use in laser modules","authors":"T. A. Corser","doi":"10.1109/ECTC.1991.163868","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163868","url":null,"abstract":"Reviews extensive data on both environmental testing and life testing (greater than one-million device hours of biased aging) of thermoelectric coolers (TECs) and discusses the dominant failure modes possible during a typical 20-year lifetime. Results indicate that the proper procurement, packaging, and screening of TECs can provide failure rates much less than the 1300 FITs quoted by Bellcore. The overall reliability of standard 18 couple TECs installed in the Astrotec Laser Module are found to be 359 FITs at 10 years, assuming a 40 degrees C T/sub HOT/ and a 20 degrees C Delta T. The random failure rate is 140 FITs at 60% confidence limit based on laboratory aging data alone.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"25 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"125324475","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"A multilevel epoxy substrate for flip-chip hybrid multichip module applications","authors":"E. Tsunashima, A. Okuno","doi":"10.1109/ECTC.1991.163939","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163939","url":null,"abstract":"A multilevel substrate consisting of two portions of a multiple multilayer is discussed. One portion is thicker than the other, reinforced by organic fiber in each layer; the other is an unreinforced thick film which forms low dielectric-constant layers. A sophisticated epoxy-resin two-dimensional support, but its adhesion strength between the epoxy layers, stabilizes the elongation, shrink and warp by one-order smaller compared to the substrate of FR-4 with inorganic reinforcement. The resin of an aromatic-amine adducted type may lower the dielectric constant making it suitable for high-frequency circuits and it is an excellent acceptor of both copper-foil and copper-plated electrodes. This two-portion substrate enables ideal flip-chip bonding on thick-film hybrid circuits, gives the necessary impedance of semiconductor-circuit, and leaves a compatible zone for wire bonding and a reflow soldering.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"12 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"125439740","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
F. Perezalonso, B. Crawford, R. Bernard, R. Kaw, S. Thomas, E. Bogatin
{"title":"Electrical characterization of VLSI packages","authors":"F. Perezalonso, B. Crawford, R. Bernard, R. Kaw, S. Thomas, E. Bogatin","doi":"10.1109/ECTC.1991.163855","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163855","url":null,"abstract":"The authors define, verify, and demonstrate measurement instruments and test fixtures required to successfully characterize IC packages electrically for low-frequency applications (<50 MHz). Three fundamentally different measurement techniques were evaluated. One uses the HP 4191A RF Impedance Analyzer instrument, which measures the frequency-domain reflection coefficient and phase angle of any load and calculates its impedance. Another measurement technique uses the HP 4194A Impedance/Gain Phase Analyzer, which measures the frequency-domain voltage across the test load generated by the current through its magnitude and phase shift. The other measurement technique is called ramp-derivative; its measurement principle is based on the time domain transient response and the fundamental definition of resistance, inductance, and capacitance to determine their respective values.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"28 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"116077291","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
C. Yeh, K. Banerjee, T. Martin, C. Umeagukwu, R. Fulton, J. Stafford, K. Wyatt
{"title":"Experimental and analytical investigation of thermally induced warpage for printed wiring boards","authors":"C. Yeh, K. Banerjee, T. Martin, C. Umeagukwu, R. Fulton, J. Stafford, K. Wyatt","doi":"10.1109/ECTC.1991.163904","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163904","url":null,"abstract":"An analytical approach using finite-element techniques has been developed to simulate PWB (printed wiring board) thermo-mechanical behavior. To validate the analytical approach, a separate experimental approach is being conducted. Four different experimental techniques were investigated for their suitability for PWB warpage measurements: ultrasonics, laser, projection speckle (using vision system), and shadow moire. The shadow moire method has been chosen for measuring warpage of PWBs because it offers good resolution and full-field measurement. Seven test samples with different configurations were carefully designed and fabricated to ensure that the thermally induced warpage would be sufficient for measurement. These test samples consist of copper layers and various FR-4 dielectric layers. Two specimen configurations were tested for a temperature range from 25 degrees C to 100 degrees C. Attempts have also been made to correlate the experimental results with the analytical results, although accurate material properties are not known. A good match was obtained for a set of material properties extracted from a number of publications.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"18 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"128625651","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"Packaging of a polarization independent optical isolator","authors":"C. A. Jack, W. Emkey","doi":"10.1109/ECTC.1991.163869","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163869","url":null,"abstract":"The authors describe the design, packaging and performance of a polarization-independent, pigtailed optical isolator. The design consists of two birefringent wedges sandwiching a Faraday rotator crystal. This sandwich is bonded into the centre of a cylindrical SmCo magnet. The isolator is packaged in a metallic package consisting of stainless steel and Kovar. All critical interfaces are either soldered, resistance-welded, or laser-welded. The resulting package is shown to be both mechanically and environmentally stable. Typical performance values are: insertion loss, nominally 1.7 dB, peak isolations >40 dB, and return loss > 60 dB. Principal applications of the isolator include direct attachment to laser packages, semiconductor amplifier packages, and fiber amplifiers.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"20 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"131791935","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"Failure analysis of a hybrid device exhibiting copper dendrite growth on thick film resistors","authors":"J. Dixon, M. Northrup, D. Rooney","doi":"10.1109/ECTC.1991.163862","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163862","url":null,"abstract":"The authors discuss the failure analysis performed on several hybrid devices submitted to Oneida Research Services, Inc. The analysis was initiated because of electrical testing failures-a voltage divider exhibited an out-of-specification value during burn-in at elevated temperature. This voltage divider compared the outputs of two thick-film resistors. Analysis of the hybrid failures revealed a copper dendritic growth propagating across the laser trims in the thick film resistor. The authors describe the hybrid materials construction, environmental testing, and electrical testing performed in examining the factors which led to the dendrite growth and overall failure of the hybrids. A detailed description of the analytical equipment and methodology used in identifying the cause of the copper dendrite growth as a result of processing is presented. The authors conclude with a discussion of the failure analysis.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"1 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"131149912","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
{"title":"Concatenated high wavelength isolation WDM and 4*4 wavelength-flattened coupler","authors":"Jisen Xu, Y. Zhang, Xiang Zhang","doi":"10.1109/ECTC.1991.163851","DOIUrl":"https://doi.org/10.1109/ECTC.1991.163851","url":null,"abstract":"A novel WDM (wavelength division multiplexer) with high wavelength isolation integrated with three WDMs, and a 4*4 single-mode wavelength-flattened star coupler integrated with four 2*2 wavelength flattened couplers (WFCs), as single assemblies, are presented. These assemblies are fabricated by fusing the couplers or WDMs directly at the same fibers. Without any splices, and packaging in small compact packages, these integrated assemblies not only show better performance, less excess loss, and smaller package dimension with no additional splices than the concatenated ones, but also have environmental stability and reliability similar to that of the single fused components.<<ETX>>","PeriodicalId":199552,"journal":{"name":"1991 Proceedings 41st Electronic Components & Technology Conference","volume":"290 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1991-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"131680583","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}