Microscopic Features of Ground Water-Induced Sulfate Attack in Highly Permeable Concretes 高渗透混凝土中地下水诱发硫酸盐侵蚀的微观特征
SP-192: 2000 Canmet/ACI Conference on Durability of Concrete Pub Date : 1900-01-01 DOI: 10.14359/5762
S. Diamond
{"title":"Microscopic Features of Ground Water-Induced Sulfate Attack in Highly Permeable Concretes","authors":"S. Diamond","doi":"10.14359/5762","DOIUrl":"https://doi.org/10.14359/5762","url":null,"abstract":"A number of unusual microscopic features have been documented in studies of the alteration of permeable concretes undergoing sulfate attack in semi-arid climates. The high W/C of the concretes examined here has permitted complete penetration of sulfate-bearing ground water through the concrete, and deposition of crystallized salts on evaporative surfaces, including the upper surfaces of slabs. The microstructural alterations observed in response to this penetration of sulfate-bearing ground water include the deposition of secondary ettringite and the accompanying local expansion and cracking, and the deposition of gypsum, but are much more extensive and complicated than that. Calcium hydroxide is often entirely removed throughout the concrete, leaving open areas, particularly in the interfacial zones around aggregates. Various new compounds are deposited in these spaces, and elsewhere within the paste. In addition to ettringite and gypsum, the substances deposited often include monosulfate; brucite and magnesium silicate hydrate may be formed where the ground water is rich in magnesium; and thaumasite may be developed where carbonation accompanies sulfate attack. Partial decalcification of the C-S-H gel is common, and magnesium silicate hydrate may locally replace it. Even the large residual unhydrated cement grains, usually stable indefinitely in most concretes, are profoundly altered. The C2S and C3S in such grains may be completely dissolved and the spaces thus provided within the outlines of the cement grains may also be filled by secondary deposits. It is evident that sulfate attack produces profound internal changes in the paste microstructure, leading to the softening, exfoliation, and other external symptoms of sulfate attack reported in the literature.","PeriodicalId":137341,"journal":{"name":"SP-192: 2000 Canmet/ACI Conference on Durability of Concrete","volume":"1246 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"129627630","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 5
Curing Time Estimator for Portland and Portland/Fly Ash Concretes 硅酸盐和硅酸盐/粉煤灰混凝土养护时间估算器
SP-192: 2000 Canmet/ACI Conference on Durability of Concrete Pub Date : 1900-01-01 DOI: 10.14359/5740
L. Parrott
{"title":"Curing Time Estimator for Portland and Portland/Fly Ash Concretes","authors":"L. Parrott","doi":"10.14359/5740","DOIUrl":"https://doi.org/10.14359/5740","url":null,"abstract":"The development of a curing time estimator is described. It is based upon an existing model of the microstructure and porosity gradients in the cover concrete that correlates well with relevant hydration and port structure measurements. The same model also yields capillary porosities that correlate with measurements of compressive strength and water absorption rate. The objective is to provide a single method to estimate curing times for CEM I and CEM II (portland and portland/flyash) concretes in a wide range of climatic conditions and achieve a consistent, well-defined measure of cover concrete performance. New hydration and pore structure measurements are briefly reviewed in relation to the existing model of microstructure and porosity in cover concrete. Recent developments regarding European standards for curing and concrete durability are considered. A criterion of capillary porosity in the matrix of cover concrete is used to unify the durability-related effects of curing period, cement type, water/binder and climatic conditions. The initial input to the estimator is the cement type to be employed. The next input is a maximum water/binder, as necessary to ensure durability under the expected exposure conditions; this automatically sets a target capillary porosity in the cover concrete, based upon recent curing period recommendations from European standards committees. Subsequent inputs define the climatic conditions in terms of exposure relative humidity and temperature history. The estimator calculates and tabulates capillary porosities in the cover concrete for a wide range of curing periods so that a period can be chosen without exceeding the target porosity. Capillary porosities for reduced water/binders, 95 and 90% of the input value, are also tabulated to illustrate the reductions in curing period that are possible with these higher concrete qualities. Examples are given to illustrate the effect of each of the eight inputs. Water/binder, exposure relative humidity and cement type are the most influential. It is evident that in many cases control of cover concrete performance via curing options is limited relative to the control offered via small changes in the concrete mix proportions or alternative cements.","PeriodicalId":137341,"journal":{"name":"SP-192: 2000 Canmet/ACI Conference on Durability of Concrete","volume":"22 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"129504035","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
In Place Durability Assessment for the Next Millennium-Long-Term Study 下一个千年长期研究的就地耐久性评估
SP-192: 2000 Canmet/ACI Conference on Durability of Concrete Pub Date : 1900-01-01 DOI: 10.14359/5757
Baroghel-Bouny, F. Larrard
{"title":"In Place Durability Assessment for the Next Millennium-Long-Term Study","authors":"Baroghel-Bouny, F. Larrard","doi":"10.14359/5757","DOIUrl":"https://doi.org/10.14359/5757","url":null,"abstract":"Within the framework of the \"BHP 2000\" French National Project, a long-term experimental study is carried out in order to assess the durability of fifteen concretes with 28-day compressive strength ranging from 20 to 130 MPa. The properties of these concretes are first studied on samples in laboratory conditions. Also, reinforced-concrete test specimens are monitored over the years at four different field exposure stations. The experimental results of compressive strength, gas permeability, and carbonation depth obtained in the laboratory on the water-cured 28-day old samples are compared here with some of the available field data. The ranking of the different concretes with respect to their durability is deduced in both cases. Other laboratory measurements, such as chloride diffusivity, capillary coefficient, and deicing-salt scaling resistance, are also presented and discussed in this paper. For each type of concretes, the influence of mixture-parameters, such as the water-to-cement ratio, the presence of entrained air or of pozzolanic admixtures, on the different properties is analyzed. The influence of the environmental conditions on the field data is also discussed. The various trends observed on the durability-related properties are interpreted on the basis of the microstructural characteristics of the materials. The paper focuses on the behavior of high-performance concretes. A superior ability to limit gas or liquid transfers within the material is observed for these concretes. But, it is found that the presence of entrained air increases their gas permeability, indicating an increased potential risk of corrosion of the reinforcement, without systematically enhancing the deicing-salt scaling resistance of the concrete. Most of the non-air-entrained high-performance concretes do not exhibit good performance when submitted to accelerated freezing and thawing cycles in the presence of salts. All of these results have to be confirmed by the long-term monitoring of the structural elements.","PeriodicalId":137341,"journal":{"name":"SP-192: 2000 Canmet/ACI Conference on Durability of Concrete","volume":"191 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"124324280","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 2
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
相关产品
×
本文献相关产品
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信
小红书