The effects of diffusion depth and heat-affected zone in NE-GMAW process on SUH 310S steel using an Image processing method 采用图像处理方法研究了NE-GMAW工艺对SUH 310S钢扩散深度和热影响区的影响
international journal of iron and steel society of iran Pub Date : 2021-01-20 DOI: 10.22034/IJISSI.2021.243772
H. Tagimalek, M. Azargoman, M. R. Maraki, M. Mahmoodi
{"title":"The effects of diffusion depth and heat-affected zone in NE-GMAW process on SUH 310S steel using an Image processing method","authors":"H. Tagimalek, M. Azargoman, M. R. Maraki, M. Mahmoodi","doi":"10.22034/IJISSI.2021.243772","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.243772","url":null,"abstract":"In this research, the effect of Diffusion Depth and Heat-Affected Zone (HAZ) in Nanoparticles-Electrode Gas Metal Arc Welding (NE-GMAW) process with carbon dioxide protection on Heat Resistance Steel (SUH 310S) was investigated using the Image Processing (IP) and Simulation software. Welding speed (S), wire feed rate (F) and voltage (V) as effective parameters were considered for experimental tests. The Design of Experiment (DoE) was using the Taguchi method and performed in L11 without experiment replication. According to a Scanning Electron Microscope (SEM) images from the experiments, changes in three effective parameters were obtained. The voltage and wire feed rate had the most significant impact on increasing HAZ and ultimately the diffusion depth due to the increase of heat generated and the creation of a more comprehensive Weld Pool (WP). Experimental 11-samples was used by NI vision IP software to find the diffusion depth and surface zone of the HAZ. Results of the effect parameters in Image Processing and Simulation software showed validation for evaluating changes in HAZ.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"60 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2021-01-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"124409422","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 2
Simulation of water-circulating path and heat transfer in blast-furnace tuyeres with simple and spiral double-chamfer design 简单螺旋式双倒角设计的高炉风口水循环路径及传热模拟
international journal of iron and steel society of iran Pub Date : 2021-01-20 DOI: 10.22034/IJISSI.2021.243774
M. Sharifi, Sirus Parchami Borjoui Raky, Soroush Parchami Borjoui Raky, Salman Mardani
{"title":"Simulation of water-circulating path and heat transfer in blast-furnace tuyeres with simple and spiral double-chamfer design","authors":"M. Sharifi, Sirus Parchami Borjoui Raky, Soroush Parchami Borjoui Raky, Salman Mardani","doi":"10.22034/IJISSI.2021.243774","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.243774","url":null,"abstract":"Tuyeres or air-blowing nozzles are considered sensitive parts of blast furnaces responsible for blowing hot air into the furnace, and their proper operation has a direct effect on the iron-melting process in the blast furnace. These parts are usually damaged or destroyed by exposure to high temperatures, radiation, slag or molten iron scattering, improper design of the water-circulating system, low thermal conductivity, operator problems, etc.In this paper, the two simple and spiral water-circulating designs are simulated and examined in heat transfer and fluid pressure drop under furnace conditions. Based on the results obtained from the spiral design, water is directed to the critical areas of the body at a lower temperature and passes through these areas quicker than the simple design.; Additionally, the cooling power of the spiral design is more efficient for the body of the tuyeres and will help prevent this part from burning in these areas. According to the simulation, the spiral design’s water pressure will drop slightly further than the simple design.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"36 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2021-01-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"127713279","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
Oxidation Behavior of AISI 316 Steel Coated with Ni-P-TiO2-Al2O3 Composite Coating Ni-P-TiO2-Al2O3复合涂层对AISI 316钢氧化性能的影响
international journal of iron and steel society of iran Pub Date : 2021-01-20 DOI: 10.22034/IJISSI.2021.243775
H. Ebrahimifar, F. Mohsenifar
{"title":"Oxidation Behavior of AISI 316 Steel Coated with Ni-P-TiO2-Al2O3 Composite Coating","authors":"H. Ebrahimifar, F. Mohsenifar","doi":"10.22034/IJISSI.2021.243775","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.243775","url":null,"abstract":"Austenitic steels have numerous applications in high-temperature environments. The thermally-grown chromia scale on the steel surface may be-come unstable at high temperatures and as a result, oxidation resistance of steel will decrease. A potentially method for improving oxidation properties is the use of composite coatings using techniques such as electroplating. In the present study, Ni-P-TiO2-Al2O3 composite coating was deposited on AISI 316 steel sub-strate by electroplating. The as-coated samples were examined with scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS). X-Ray diffraction (XRD) was also used to identify the formed phases in the as-coated structures. In order to evaluate oxidation behavior, isothermal oxidation and cy-clic oxidation were conducted at 800 oC. Isothermal oxidation of uncoated steels revealed higher weight gain in comparison with Ni-P-TiO2-Al2O3 composite-coated samples. The coating layer limited the outward diffusion of Cr cation and the inward diffusion of oxygen anion and resulted in better oxidation resistance. According to the results of cyclic oxidation, coated substrates demonstrated excel-lent resistance against spallation and cracking.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"6 6","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2021-01-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"132089428","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
Investigation of the Effect of the Efficiency of Catalysts on Early Destruction of Direct Reduction Reformer Tubes. 催化剂效率对直接还原炉管早期破坏影响的研究。
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.523378.1181
M. Sadeghi, S. Abdollahi, H. M. Abadi
{"title":"Investigation of the Effect of the Efficiency of Catalysts on Early Destruction of Direct Reduction Reformer Tubes.","authors":"M. Sadeghi, S. Abdollahi, H. M. Abadi","doi":"10.22034/IJISSI.2021.523378.1181","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.523378.1181","url":null,"abstract":"The catalysts of the direct reduction unit play a critical key role in producing reducing gases and the lifetime of the reformer tubes. In this paper, the effect of reducing the efficiency of catalysts on the early destruction of direct reduction reformer tubes is investigated. Cold compressive strength test, XRF and BET analysis were performed on intact and used catalysts. Also, the microstructure of the destroyed tube was examined by a scanning electron microscope and the amount of sulfur was measured. The results show that in used catalysts compared to intact catalysts, the specific surface area is reduced, and the amount of access to areas containing nickel is reduced. Access to nickel-rich areas will be drastically decreased and reforming reactions will not be performed well. This lessens the efficiency of the catalysts and breaks them down hence several reformer tubes are exposed to higher temperatures and their service life will be considerably reduced. Due to the presence of precipitations, the sulfur amount available in the destructed tube is equal to 0.1%, which is ten times the allowable sulfur content in the reformer tube alloy.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"44 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"126152839","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
The effects of vanadium on microstructure and wear resistance of high manganese steels 钒对高锰钢组织和耐磨性的影响
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.530512.1198
Arash Bagheriyeh, S. Kaviani
{"title":"The effects of vanadium on microstructure and wear resistance of high manganese steels","authors":"Arash Bagheriyeh, S. Kaviani","doi":"10.22034/IJISSI.2021.530512.1198","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.530512.1198","url":null,"abstract":"The high Mn steels (HMS) are currently used in transportation components, large-scale grinders and crusher, and grinding wheels. This study is dedicated to the effects of vanadium content on the properties and wear behavior of Fe-12Mn-1.2C-0.8Si steels containing 0, 0.3, and 0.6 wt.% vanadium as an alloying element. The samples were cast and then subjected to annealing heat treatment and followed by water quenching. The test samples were then cut via an electrical discharge machine. Characterization methods, including phase analysis via XRD and microstructural investigations by scanning electron and optical microscopes, were carried out. The samples were also subjected to hardness and wear tests. The obtained results indicated that the addition of V to the HMS leads to the increased hardness and improved wear properties. Such outcomes were attributed to the role of vanadium in altering the precipitation sites of carbides,from grain boundaries to the grains, and its effect distribution of the carbides.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"7 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"132311907","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
A Detailed Failure Analysis of Vertically Suspended Diffuser Pump Caused by Hex Head Bolt Fracture: The Marine Service Condition 垂直悬浮扩散泵内六角螺栓断裂的详细失效分析:海上服役情况
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.527610.1188
M. Etminanfar, M. S. Safavi, Saeedeh Masumi, Sahel Khanmohammadi, Jafar Seied-Hamzeh, J. Khalil-Allafi
{"title":"A Detailed Failure Analysis of Vertically Suspended Diffuser Pump Caused by Hex Head Bolt Fracture: The Marine Service Condition","authors":"M. Etminanfar, M. S. Safavi, Saeedeh Masumi, Sahel Khanmohammadi, Jafar Seied-Hamzeh, J. Khalil-Allafi","doi":"10.22034/IJISSI.2021.527610.1188","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.527610.1188","url":null,"abstract":"Vertically suspended diffuser pumps play a significant role in the seawater cooling systems of the petrochemical and refinery industries. The present work deals with providing a detailed analysis of mechanisms involved in the early failure of hex head bolt used in the vertically suspended diffuser pump framework, which has served three years in the marine condition. The morphological and microstructural characteristics of the failed bolt were evaluated by optical microscope, scanning electron microscope (SEM), spark-optical emission spectroscopy (spark-OES), and X-ray diffraction (XRD) methods. Besides, microhardness test was performed to assess the mechanical properties of the samples. The results demonstrated the presence of Cr, Fe, Mn, and Si elements in the microstructure of failed bolt, which coincides with the composition of stainless steel (X5CrMnN17-8). While there exist sulfur and oxide inclusions in the parts close to the surface, no surface-related defects were detected in the central part. Moreover, the microstructural assay showed that the failed sample was composed of austenite-martensite micro-duplex structure. The microhardness values of regions close to the surface of the failed bolt were higher than that of the central part by ≈20 %, since there is higher martensite content. Fractography images revealed a brittle fracture mechanism in the parts close to the surface, while ductile fracture was observed at the center of the bolt. In general, the main factor governing the failure of the bolt can be attributed to the lack of precise control over the chemical composition of the bolt and the application of inappropriate fabrication process.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"58 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"126259967","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
Investigation of Corrosion Behavior of Drain Pipes of Process Compressors in Direct Reduction Unit. 直接还原机组过程压缩机排水管腐蚀行为研究。
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.524484.1185
S. Abdollahi, M. Sadeghi
{"title":"Investigation of Corrosion Behavior of Drain Pipes of Process Compressors in Direct Reduction Unit.","authors":"S. Abdollahi, M. Sadeghi","doi":"10.22034/IJISSI.2021.524484.1185","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.524484.1185","url":null,"abstract":"Corrosion is a natural process in the destruction of industrial components. Corrosion can be intensified and finally led to destruction where there are temperature increase and microbial agents in addition to the main causes of corrosion. Process compressors were employed in order to meet the gas pressure and flow of the process in the direct reduction unit, and carbon steel pipes were used to separate water from the gas. However, these pipes are punctured and leak water and gas in less time in comparison with the other units. In order to examine the destruction reasons, several samples of the destructed pipe were provided, and they were studied by scanning electron microscopy (SEM) and EDS. The results showed that, besides regular agents like high temperature and acidic medium, microbial corrosion by sulfate-reducing bacteria and H2S gas effect lead to intensifying local and sub-sediment corrosion so that the component will be destructed in less time. The presence of FeS layer will result in severe local corrosion.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"63 1-2","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"114120625","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 0
Using the artificial neural network to investigate the effect of parameters in square cup deep drawing of aluminum-steel laminated sheets 利用人工神经网络研究了铝钢层合板方杯拉深过程中各参数的影响
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.528568.1196
M. Mahmoodi, H. Tagimalek, H. Sohrabi, M. R. Maraki
{"title":"Using the artificial neural network to investigate the effect of parameters in square cup deep drawing of aluminum-steel laminated sheets","authors":"M. Mahmoodi, H. Tagimalek, H. Sohrabi, M. R. Maraki","doi":"10.22034/IJISSI.2021.528568.1196","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.528568.1196","url":null,"abstract":"In this study, the effective parameters involved in the deep drawing of double-layer metal sheets in a die ofsquare cross-section were investigated through artificial neural network (ANN) modeling. For this purpose,first, the deep drawing of double-layer (Al1200 / ST14) sheets was carried out experimentally. Also, the finiteelement simulation of the process was performed, and the results validated through experimental tests. A setof 46 different experimental data were employed in this paper. The ANN was trained by using a mean squareerror of 10-4. The input parameters, i.e., punch radius, die radius, blank holder force, clearance, and the permutationlayers were set to the network. The surface response method (RSM); was employed to evaluate theresults of the ANN model, and the input parameters of the deep drawing process on the thinning of Al1200and ST14 composite layers were analyzed. The obtained results indicate that the punch edge radius has themost significant influence on the thinning of the Al1200 layer. Increasing the gap between the punch and dieto 1/4 of the sheet thickness, increased the cup wall layers thickness of the Al1200 and ST14 respectively by3.38% and 0.5%. The performance of the ANN model demonstrates that it can estimate the amount of thinningin the composite layers with satisfactory accuracy.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"42-43 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"134038668","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 3
Investigation of carbon and silicon partitioning on ferrite hardening in a medium silicon low alloy ferrite-martensite dual-phase steel 中硅低合金铁素体-马氏体双相钢铁素体硬化过程中碳硅分配的研究
international journal of iron and steel society of iran Pub Date : 2020-08-22 DOI: 10.22034/IJISSI.2021.527641.1189
A. Khajesarvi, S. S. G. Banadkouki
{"title":"Investigation of carbon and silicon partitioning on ferrite hardening in a medium silicon low alloy ferrite-martensite dual-phase steel","authors":"A. Khajesarvi, S. S. G. Banadkouki","doi":"10.22034/IJISSI.2021.527641.1189","DOIUrl":"https://doi.org/10.22034/IJISSI.2021.527641.1189","url":null,"abstract":"In this paper, the micromechanical behavior of ferrite microphase was evaluated in conjunction with carbon and silicon partitioning occurred during prior austenite to ferrite phase transformation using microhardness measurements supplemented by light observation and field-emission scanning electron microscopy equipped with X-ray energy dispersive spectroscopy (EDS). For this purpose, at first, the samples were austenitized at 900°C for 15 min and then air-cooled (normalized) to room temperature in order to develop more starting homogeneous microstructural features in the proposed heat-treated samples. The wide variety of ferrite-martensite dual-phase (DP) samples containing different volume fractions of ferrite and martensite microphases developed using step-quenching heat treatment processes at 750, 720, 700, and 680°C for 5 min isothermal holding time with the subsequent water quenching after being austenitized at 900°C for 15 min in the same conditions as to the direct water-quenched (WQ) samples. The experimental results showed that, for a particular ferrite grain in a particular ferrite-martensite DP samples, the ferrite location nearer to the ferrite-martensite interfaces was accompanied with a significantly lower carbon and silicon centrations, while the associated ferrite hardening response was abnormally higher in comparison to that of the central regions of ferrite grains. This abnormal higher trend in ferrite hardness with lower carbon and silicon concentrations was attributed to the higher ferrite/martensite interaction of ferrite area adjacent to the martensite generated during martensitic phase transformation.","PeriodicalId":131024,"journal":{"name":"international journal of iron and steel society of iran","volume":"17 1","pages":"0"},"PeriodicalIF":0.0,"publicationDate":"2020-08-22","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":null,"resultStr":null,"platform":"Semanticscholar","paperid":"130639346","PeriodicalName":null,"FirstCategoryId":null,"ListUrlMain":null,"RegionNum":0,"RegionCategory":"","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":"","EPubDate":null,"PubModel":null,"JCR":null,"JCRName":null,"Score":null,"Total":0}
引用次数: 1
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
相关产品
×
本文献相关产品
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信
小红书