基于等效氮化物/氧化物(N/O)堆模型的氮化栅极氧化物优化及结垢极限预测

V. Chang, C. Chen, Y. Jin, C. Chen, T. Lee, S. Chen, M. Liang
{"title":"基于等效氮化物/氧化物(N/O)堆模型的氮化栅极氧化物优化及结垢极限预测","authors":"V. Chang, C. Chen, Y. Jin, C. Chen, T. Lee, S. Chen, M. Liang","doi":"10.1109/ICICDT.2004.1309983","DOIUrl":null,"url":null,"abstract":"A semi-empirical model was developed to calculate the equivalent oxide thickness (EOT) and leakage current of nitrided gate oxide by hypothetically dividing the nitrided oxide into a nitride/oxide (N/O) stack. The calculations agree well with the experimental data (R/sup 2/ > 0.99) for various nitrided oxides with EOT ranging from 12 to 23 /spl Aring/. A model-based strategy for the optimization of nitrided oxide is presented and demonstrated by a nitrided oxide sample which meets both the EOT and leakage current requirements of ITRS 65-nm low standby power (LSTP) technology and shows no electron mobility degradation. The model forecasts that a nitrogen concentration of 20% approximately the maximum from Oxide nitridation processes - satisfies the ITRS requirements for production until Year 2007. The production afterwards will require alternative dielectrics such as N/O stack or high-k materials for greater leakage current reductions.","PeriodicalId":158994,"journal":{"name":"2004 International Conference on Integrated Circuit Design and Technology (IEEE Cat. No.04EX866)","volume":"91 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2004-10-04","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Optimization and scaling limit forecast of nitrided gate oxide using an equivalent nitride/oxide (N/O) stack model\",\"authors\":\"V. Chang, C. Chen, Y. Jin, C. Chen, T. Lee, S. Chen, M. Liang\",\"doi\":\"10.1109/ICICDT.2004.1309983\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"A semi-empirical model was developed to calculate the equivalent oxide thickness (EOT) and leakage current of nitrided gate oxide by hypothetically dividing the nitrided oxide into a nitride/oxide (N/O) stack. The calculations agree well with the experimental data (R/sup 2/ > 0.99) for various nitrided oxides with EOT ranging from 12 to 23 /spl Aring/. A model-based strategy for the optimization of nitrided oxide is presented and demonstrated by a nitrided oxide sample which meets both the EOT and leakage current requirements of ITRS 65-nm low standby power (LSTP) technology and shows no electron mobility degradation. The model forecasts that a nitrogen concentration of 20% approximately the maximum from Oxide nitridation processes - satisfies the ITRS requirements for production until Year 2007. The production afterwards will require alternative dielectrics such as N/O stack or high-k materials for greater leakage current reductions.\",\"PeriodicalId\":158994,\"journal\":{\"name\":\"2004 International Conference on Integrated Circuit Design and Technology (IEEE Cat. No.04EX866)\",\"volume\":\"91 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2004-10-04\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2004 International Conference on Integrated Circuit Design and Technology (IEEE Cat. No.04EX866)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/ICICDT.2004.1309983\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2004 International Conference on Integrated Circuit Design and Technology (IEEE Cat. No.04EX866)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ICICDT.2004.1309983","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 2

摘要

建立了一种半经验模型,通过假设将氮化栅极氧化物划分为氮化物/氧化物(N/O)堆,计算了等效氧化物厚度(EOT)和漏电流。计算结果与实验数据吻合较好(R/sup 2/ > 0.99), EOT范围为12 ~ 23 /spl /。提出了一种基于模型的氮化氧化物优化策略,并通过氮化氧化物样品进行了验证,该氮化氧化物样品既满足ITRS 65纳米低待机功率(LSTP)技术的EOT要求,又满足漏电流要求,且没有电子迁移率下降。该模型预测,20%的氮浓度(约为氧化物氮化过程的最大值)可以满足ITRS到2007年的生产要求。之后的生产将需要替代介质,如N/O堆叠或高k材料,以更大程度地降低泄漏电流。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Optimization and scaling limit forecast of nitrided gate oxide using an equivalent nitride/oxide (N/O) stack model
A semi-empirical model was developed to calculate the equivalent oxide thickness (EOT) and leakage current of nitrided gate oxide by hypothetically dividing the nitrided oxide into a nitride/oxide (N/O) stack. The calculations agree well with the experimental data (R/sup 2/ > 0.99) for various nitrided oxides with EOT ranging from 12 to 23 /spl Aring/. A model-based strategy for the optimization of nitrided oxide is presented and demonstrated by a nitrided oxide sample which meets both the EOT and leakage current requirements of ITRS 65-nm low standby power (LSTP) technology and shows no electron mobility degradation. The model forecasts that a nitrogen concentration of 20% approximately the maximum from Oxide nitridation processes - satisfies the ITRS requirements for production until Year 2007. The production afterwards will require alternative dielectrics such as N/O stack or high-k materials for greater leakage current reductions.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信