不影响尺寸和铁电性能的BaTiO3多晶陶瓷致密化

M. Taheri, B. Zanca, S. J. Villegas, M. Dolgos, S. Bryant, S. Trudel
{"title":"不影响尺寸和铁电性能的BaTiO3多晶陶瓷致密化","authors":"M. Taheri, B. Zanca, S. J. Villegas, M. Dolgos, S. Bryant, S. Trudel","doi":"10.1109/IFCS-ISAF41089.2020.9234947","DOIUrl":null,"url":null,"abstract":"High pressure and high temperature sintering (on the order of several MPa and up to 1400 °C) is the conventional process employed to achieve dense ceramics from polycrystalline materials. This traditional process influences microstructure and grain morphology of samples, affecting their physical properties and device performance. Here, we present the variation of grain size through the conventional one-step and compare it to two-step sintering for micron- and nano-sized particles. The effect of grain size on the spontaneous electric polarization and dielectric constant of BaTiO3 ceramics are investigated. We find that two-step sintering can achieve high relative densities, while minimizing grain growth. Such a study is of significant importance to enable the measurement of as-prepared samples, easing the understanding of size-dependent properties.","PeriodicalId":6872,"journal":{"name":"2020 Joint Conference of the IEEE International Frequency Control Symposium and International Symposium on Applications of Ferroelectrics (IFCS-ISAF)","volume":"63 1","pages":"1-4"},"PeriodicalIF":0.0000,"publicationDate":"2020-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Densifying BaTiO3 Polycrystalline Ceramics Without Affecting Size and Ferroelectric Properties\",\"authors\":\"M. Taheri, B. Zanca, S. J. Villegas, M. Dolgos, S. Bryant, S. Trudel\",\"doi\":\"10.1109/IFCS-ISAF41089.2020.9234947\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"High pressure and high temperature sintering (on the order of several MPa and up to 1400 °C) is the conventional process employed to achieve dense ceramics from polycrystalline materials. This traditional process influences microstructure and grain morphology of samples, affecting their physical properties and device performance. Here, we present the variation of grain size through the conventional one-step and compare it to two-step sintering for micron- and nano-sized particles. The effect of grain size on the spontaneous electric polarization and dielectric constant of BaTiO3 ceramics are investigated. We find that two-step sintering can achieve high relative densities, while minimizing grain growth. Such a study is of significant importance to enable the measurement of as-prepared samples, easing the understanding of size-dependent properties.\",\"PeriodicalId\":6872,\"journal\":{\"name\":\"2020 Joint Conference of the IEEE International Frequency Control Symposium and International Symposium on Applications of Ferroelectrics (IFCS-ISAF)\",\"volume\":\"63 1\",\"pages\":\"1-4\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-07-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2020 Joint Conference of the IEEE International Frequency Control Symposium and International Symposium on Applications of Ferroelectrics (IFCS-ISAF)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/IFCS-ISAF41089.2020.9234947\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2020 Joint Conference of the IEEE International Frequency Control Symposium and International Symposium on Applications of Ferroelectrics (IFCS-ISAF)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/IFCS-ISAF41089.2020.9234947","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

高压和高温烧结(约为几兆帕和高达1400°C)是用于从多晶材料中获得致密陶瓷的常规工艺。这种传统工艺影响了样品的微观结构和晶粒形态,影响了样品的物理性能和器件性能。在这里,我们展示了常规一步烧结的晶粒尺寸变化,并将其与两步烧结的微米级和纳米级颗粒进行了比较。研究了晶粒尺寸对BaTiO3陶瓷自发电极化和介电常数的影响。我们发现两步烧结可以获得较高的相对密度,同时最小化晶粒生长。这样的研究对制备样品的测量具有重要意义,有助于理解尺寸相关性质。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Densifying BaTiO3 Polycrystalline Ceramics Without Affecting Size and Ferroelectric Properties
High pressure and high temperature sintering (on the order of several MPa and up to 1400 °C) is the conventional process employed to achieve dense ceramics from polycrystalline materials. This traditional process influences microstructure and grain morphology of samples, affecting their physical properties and device performance. Here, we present the variation of grain size through the conventional one-step and compare it to two-step sintering for micron- and nano-sized particles. The effect of grain size on the spontaneous electric polarization and dielectric constant of BaTiO3 ceramics are investigated. We find that two-step sintering can achieve high relative densities, while minimizing grain growth. Such a study is of significant importance to enable the measurement of as-prepared samples, easing the understanding of size-dependent properties.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信