{"title":"SiC-AlON陶瓷复合材料的高温抗氧化性能","authors":"Lai Xiao, Yu-de Xiao, Xiao-long Zhao, Xing Li, Lv Chen, T. Xuan, Ya Zhang, Z. Cai, Xiao Wang","doi":"10.2298/pac2202097x","DOIUrl":null,"url":null,"abstract":"The microstructure and oxidation behaviour of the pure AlON ceramics and 8 wt.% SiC-AlON composite were investigated at 700-1500?C. With increasing oxidation temperature, the surface morphology of two ceramics showed a change from acicular to flaky-like and then to granular features. With the addition of nanosized SiC particles, the oxidation resistance of the ceramics was remarkably enhanced above 1100?C. This is attributed to the formation of a dense oxide layer composed of Al2O3, SiO2 and mullite, which could cover the whole matrix and suppress further penetration of oxygen. Due to the dense oxide layer, the oxidation kinetics of the 8 wt.% SiC-AlON composites conformed to a parabolic law, while that of the pure AlON conformed to a linear law. After oxidation at 1500 ?C for 40 h, the weight gain of the 8 wt.% SiC-AlON composites was 3.07mg/cm2, which was only 22.5% of that of the pure AlON.","PeriodicalId":20596,"journal":{"name":"Processing and Application of Ceramics","volume":null,"pages":null},"PeriodicalIF":0.9000,"publicationDate":"2022-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":"{\"title\":\"Oxidation resistance performance of SiC-AlON ceramic composites at high temperature\",\"authors\":\"Lai Xiao, Yu-de Xiao, Xiao-long Zhao, Xing Li, Lv Chen, T. Xuan, Ya Zhang, Z. Cai, Xiao Wang\",\"doi\":\"10.2298/pac2202097x\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The microstructure and oxidation behaviour of the pure AlON ceramics and 8 wt.% SiC-AlON composite were investigated at 700-1500?C. With increasing oxidation temperature, the surface morphology of two ceramics showed a change from acicular to flaky-like and then to granular features. With the addition of nanosized SiC particles, the oxidation resistance of the ceramics was remarkably enhanced above 1100?C. This is attributed to the formation of a dense oxide layer composed of Al2O3, SiO2 and mullite, which could cover the whole matrix and suppress further penetration of oxygen. Due to the dense oxide layer, the oxidation kinetics of the 8 wt.% SiC-AlON composites conformed to a parabolic law, while that of the pure AlON conformed to a linear law. After oxidation at 1500 ?C for 40 h, the weight gain of the 8 wt.% SiC-AlON composites was 3.07mg/cm2, which was only 22.5% of that of the pure AlON.\",\"PeriodicalId\":20596,\"journal\":{\"name\":\"Processing and Application of Ceramics\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.9000,\"publicationDate\":\"2022-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"1\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Processing and Application of Ceramics\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://doi.org/10.2298/pac2202097x\",\"RegionNum\":4,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Processing and Application of Ceramics","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.2298/pac2202097x","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 1

摘要

在700 ~ 1500℃温度下,研究了纯AlON陶瓷和8wt % SiC-AlON复合材料的微观结构和氧化行为。随着氧化温度的升高,两种陶瓷的表面形貌呈现出由针状到片状再到粒状的变化。在1100℃以上,纳米SiC颗粒的加入显著提高了陶瓷的抗氧化性能。这是由于形成了由Al2O3、SiO2和莫来石组成的致密氧化层,覆盖了整个基体,抑制了氧的进一步渗透。由于氧化层致密,8wt .% SiC-AlON复合材料的氧化动力学服从抛物线规律,而纯AlON的氧化动力学服从线性规律。在1500℃氧化40 h后,8 wt.%的SiC-AlON复合材料增重3.07mg/cm2,仅为纯AlON的22.5%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Oxidation resistance performance of SiC-AlON ceramic composites at high temperature
The microstructure and oxidation behaviour of the pure AlON ceramics and 8 wt.% SiC-AlON composite were investigated at 700-1500?C. With increasing oxidation temperature, the surface morphology of two ceramics showed a change from acicular to flaky-like and then to granular features. With the addition of nanosized SiC particles, the oxidation resistance of the ceramics was remarkably enhanced above 1100?C. This is attributed to the formation of a dense oxide layer composed of Al2O3, SiO2 and mullite, which could cover the whole matrix and suppress further penetration of oxygen. Due to the dense oxide layer, the oxidation kinetics of the 8 wt.% SiC-AlON composites conformed to a parabolic law, while that of the pure AlON conformed to a linear law. After oxidation at 1500 ?C for 40 h, the weight gain of the 8 wt.% SiC-AlON composites was 3.07mg/cm2, which was only 22.5% of that of the pure AlON.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Processing and Application of Ceramics
Processing and Application of Ceramics MATERIALS SCIENCE, CERAMICS-
CiteScore
1.90
自引率
9.10%
发文量
14
审稿时长
10 weeks
期刊介绍: Information not localized
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信