多面体低聚硅氧烷/多壁碳纳米管(MWCNT/POSS)杂化填料在乙丙二烯单体/苯乙烯丁二烯橡胶(EPDM/SBR)纳米复合材料中的制备及性能

IF 3.3 3区 材料科学 Q3 CHEMISTRY, PHYSICAL
Silicon Pub Date : 2025-06-09 DOI:10.1007/s12633-025-03360-1
B. Dhanasakkaravarthi, S. Vishvanathperumal, S. Arunkumar, A. Arunkumar
{"title":"多面体低聚硅氧烷/多壁碳纳米管(MWCNT/POSS)杂化填料在乙丙二烯单体/苯乙烯丁二烯橡胶(EPDM/SBR)纳米复合材料中的制备及性能","authors":"B. Dhanasakkaravarthi,&nbsp;S. Vishvanathperumal,&nbsp;S. Arunkumar,&nbsp;A. Arunkumar","doi":"10.1007/s12633-025-03360-1","DOIUrl":null,"url":null,"abstract":"<div><p>In this study, ethylene-propylene-diene monomer/styrene-butadiene rubber (EPDM/SBR) nanocomposites were prepared using a two-roll mill mixing method, incorporating a hybrid filler of polyhedral oligomeric silsesquioxane (POSS) and multiwalled carbon nanotubes (MWCNT). The composites were evaluated for their cure characteristics, mechanical properties, abrasion resistance, compression set, swelling resistance, and crosslinking density. The results indicated that as the hybrid filler content increased, minimum torque, maximum torque, delta torque, and cure rate index decreased, whereas scorch time and optimum cure time increased. Mechanical testing revealed that tensile strength and stress at 100% elongation improved up to a filler concentration of 4 phr but declined beyond this level. Hardness and tear strength showed a continuous increase with higher filler loading, while elongation at break and rebound resilience decreased. Additionally, compression set increased with rising filler content. Swelling resistance and abrasion resistance were optimized at 4 phr of hybrid filler but deteriorated when the filler concentration exceeded this threshold.</p></div>","PeriodicalId":776,"journal":{"name":"Silicon","volume":"17 11","pages":"2479 - 2497"},"PeriodicalIF":3.3000,"publicationDate":"2025-06-09","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Polyhedral Oligomeric Silsesquioxane/Multiwalled Carbon Nanotube (MWCNT/POSS) Hybrid Filler in Ethylene-Propylene-Diene Monomer/Styrene-Butadiene Rubber (EPDM/SBR) Nanocomposites: Preparation and Properties\",\"authors\":\"B. Dhanasakkaravarthi,&nbsp;S. Vishvanathperumal,&nbsp;S. Arunkumar,&nbsp;A. Arunkumar\",\"doi\":\"10.1007/s12633-025-03360-1\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>In this study, ethylene-propylene-diene monomer/styrene-butadiene rubber (EPDM/SBR) nanocomposites were prepared using a two-roll mill mixing method, incorporating a hybrid filler of polyhedral oligomeric silsesquioxane (POSS) and multiwalled carbon nanotubes (MWCNT). The composites were evaluated for their cure characteristics, mechanical properties, abrasion resistance, compression set, swelling resistance, and crosslinking density. The results indicated that as the hybrid filler content increased, minimum torque, maximum torque, delta torque, and cure rate index decreased, whereas scorch time and optimum cure time increased. Mechanical testing revealed that tensile strength and stress at 100% elongation improved up to a filler concentration of 4 phr but declined beyond this level. Hardness and tear strength showed a continuous increase with higher filler loading, while elongation at break and rebound resilience decreased. Additionally, compression set increased with rising filler content. Swelling resistance and abrasion resistance were optimized at 4 phr of hybrid filler but deteriorated when the filler concentration exceeded this threshold.</p></div>\",\"PeriodicalId\":776,\"journal\":{\"name\":\"Silicon\",\"volume\":\"17 11\",\"pages\":\"2479 - 2497\"},\"PeriodicalIF\":3.3000,\"publicationDate\":\"2025-06-09\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Silicon\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://link.springer.com/article/10.1007/s12633-025-03360-1\",\"RegionNum\":3,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"CHEMISTRY, PHYSICAL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Silicon","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s12633-025-03360-1","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"CHEMISTRY, PHYSICAL","Score":null,"Total":0}
引用次数: 0

摘要

采用双辊混炼法制备了乙烯-丙烯-二烯单体/苯乙烯-丁二烯橡胶(EPDM/SBR)纳米复合材料,并将多面体低聚硅氧烷(POSS)和多壁碳纳米管(MWCNT)作为杂化填料。对复合材料的固化特性、力学性能、耐磨性、压缩集、抗膨胀性和交联密度进行了评价。结果表明:随着杂化填料含量的增加,最小转矩、最大转矩、增量转矩和固化率指数降低,焦化时间和最佳固化时间增加;力学测试表明,100%伸长率下的拉伸强度和应力在填充剂浓度为4 phr时有所提高,但超过此水平后就会下降。随着填料负荷的增加,材料的硬度和撕裂强度不断增加,而断裂伸长率和回弹回弹率下降。此外,压缩集随着填料含量的增加而增加。混合填料的抗膨胀性和耐磨性在4 phr时达到最佳,但当填料浓度超过该阈值时,其抗膨胀性和耐磨性就会下降。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Polyhedral Oligomeric Silsesquioxane/Multiwalled Carbon Nanotube (MWCNT/POSS) Hybrid Filler in Ethylene-Propylene-Diene Monomer/Styrene-Butadiene Rubber (EPDM/SBR) Nanocomposites: Preparation and Properties

In this study, ethylene-propylene-diene monomer/styrene-butadiene rubber (EPDM/SBR) nanocomposites were prepared using a two-roll mill mixing method, incorporating a hybrid filler of polyhedral oligomeric silsesquioxane (POSS) and multiwalled carbon nanotubes (MWCNT). The composites were evaluated for their cure characteristics, mechanical properties, abrasion resistance, compression set, swelling resistance, and crosslinking density. The results indicated that as the hybrid filler content increased, minimum torque, maximum torque, delta torque, and cure rate index decreased, whereas scorch time and optimum cure time increased. Mechanical testing revealed that tensile strength and stress at 100% elongation improved up to a filler concentration of 4 phr but declined beyond this level. Hardness and tear strength showed a continuous increase with higher filler loading, while elongation at break and rebound resilience decreased. Additionally, compression set increased with rising filler content. Swelling resistance and abrasion resistance were optimized at 4 phr of hybrid filler but deteriorated when the filler concentration exceeded this threshold.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Silicon
Silicon CHEMISTRY, PHYSICAL-MATERIALS SCIENCE, MULTIDISCIPLINARY
CiteScore
5.90
自引率
20.60%
发文量
685
审稿时长
>12 weeks
期刊介绍: The journal Silicon is intended to serve all those involved in studying the role of silicon as an enabling element in materials science. There are no restrictions on disciplinary boundaries provided the focus is on silicon-based materials or adds significantly to the understanding of such materials. Accordingly, such contributions are welcome in the areas of inorganic and organic chemistry, physics, biology, engineering, nanoscience, environmental science, electronics and optoelectronics, and modeling and theory. Relevant silicon-based materials include, but are not limited to, semiconductors, polymers, composites, ceramics, glasses, coatings, resins, composites, small molecules, and thin films.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信