{"title":"利用回收的分子可分解油墨实现梯度耐蚀铜","authors":"Saurabh Khuje,&nbsp;Abdullah Islam,&nbsp;Long Zhu,&nbsp;Jun Zhang,&nbsp;Zhongxuan Wang,&nbsp;Thomas Parker,&nbsp;Jian Yu* and Shenqiang Ren*,&nbsp;","doi":"10.1021/acsaelm.4c0125910.1021/acsaelm.4c01259","DOIUrl":null,"url":null,"abstract":"<p >Oxidation and corrosion present significant challenges for copper in critical applications such as electronics. Graphene-like carbon materials hold promise for preventing oxidation and corrosion, but their application to metallic surfaces is hindered by a complex immobilization process. Herein, we describe copper-based molecular decomposable inks derived from recycling which enable <i>in situ</i> conversion to form a copper─graphitic carbon hierarchical structure. This structure withstands severe corrosive and oxidative environments and maintains stable performance across a wide temperature range, from cryogenic (−193 °C) to high temperature (500 °C) conditions. The graphitic carbon shell acts as an effective barrier, preventing oxidation and corrosion by creating lengthy diffusion routes within the hierarchical copper matrix. This enables the reliable operation of a printed antenna under a corrosive environment in a reliable fashion. The results show that the copper with a graphitic carbon shell has excellent oxidation and corrosion resistance capabilities, and the findings can be expanded to establish printed molecular decomposable materials as a platform for rapid prototyping of anticorrosion and antioxidation electronics suitable for different environmental conditions.</p>","PeriodicalId":4,"journal":{"name":"ACS Applied Energy Materials","volume":null,"pages":null},"PeriodicalIF":5.4000,"publicationDate":"2024-09-16","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Gradient Corrosion-Resistant Copper Using Molecular Decomposable Ink from Recycling\",\"authors\":\"Saurabh Khuje,&nbsp;Abdullah Islam,&nbsp;Long Zhu,&nbsp;Jun Zhang,&nbsp;Zhongxuan Wang,&nbsp;Thomas Parker,&nbsp;Jian Yu* and Shenqiang Ren*,&nbsp;\",\"doi\":\"10.1021/acsaelm.4c0125910.1021/acsaelm.4c01259\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p >Oxidation and corrosion present significant challenges for copper in critical applications such as electronics. Graphene-like carbon materials hold promise for preventing oxidation and corrosion, but their application to metallic surfaces is hindered by a complex immobilization process. Herein, we describe copper-based molecular decomposable inks derived from recycling which enable <i>in situ</i> conversion to form a copper─graphitic carbon hierarchical structure. This structure withstands severe corrosive and oxidative environments and maintains stable performance across a wide temperature range, from cryogenic (−193 °C) to high temperature (500 °C) conditions. The graphitic carbon shell acts as an effective barrier, preventing oxidation and corrosion by creating lengthy diffusion routes within the hierarchical copper matrix. This enables the reliable operation of a printed antenna under a corrosive environment in a reliable fashion. The results show that the copper with a graphitic carbon shell has excellent oxidation and corrosion resistance capabilities, and the findings can be expanded to establish printed molecular decomposable materials as a platform for rapid prototyping of anticorrosion and antioxidation electronics suitable for different environmental conditions.</p>\",\"PeriodicalId\":4,\"journal\":{\"name\":\"ACS Applied Energy Materials\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":5.4000,\"publicationDate\":\"2024-09-16\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"ACS Applied Energy Materials\",\"FirstCategoryId\":\"88\",\"ListUrlMain\":\"https://pubs.acs.org/doi/10.1021/acsaelm.4c01259\",\"RegionNum\":3,\"RegionCategory\":\"材料科学\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q2\",\"JCRName\":\"CHEMISTRY, PHYSICAL\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"ACS Applied Energy Materials","FirstCategoryId":"88","ListUrlMain":"https://pubs.acs.org/doi/10.1021/acsaelm.4c01259","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"CHEMISTRY, PHYSICAL","Score":null,"Total":0}
引用次数: 0

摘要

氧化和腐蚀给电子产品等关键应用中的铜带来了巨大挑战。类石墨烯碳材料有望防止氧化和腐蚀,但其在金属表面的应用受到复杂固定过程的阻碍。在本文中,我们介绍了从回收利用中提取的铜基分子可分解油墨,这种油墨可就地转化形成铜-石墨碳分层结构。这种结构可抵御严重的腐蚀和氧化环境,并在从低温(-193 °C)到高温(500 °C)的宽温度范围内保持稳定的性能。石墨碳外壳可作为有效的屏障,通过在分层铜基体中形成较长的扩散路径来防止氧化和腐蚀。这样,印刷天线就能在腐蚀环境下可靠地运行。研究结果表明,带有石墨碳外壳的铜具有出色的抗氧化和抗腐蚀能力,研究结果可扩展到建立可分解印刷分子材料,作为快速制作适用于不同环境条件的抗腐蚀和抗氧化电子器件原型的平台。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Gradient Corrosion-Resistant Copper Using Molecular Decomposable Ink from Recycling

Gradient Corrosion-Resistant Copper Using Molecular Decomposable Ink from Recycling

Oxidation and corrosion present significant challenges for copper in critical applications such as electronics. Graphene-like carbon materials hold promise for preventing oxidation and corrosion, but their application to metallic surfaces is hindered by a complex immobilization process. Herein, we describe copper-based molecular decomposable inks derived from recycling which enable in situ conversion to form a copper─graphitic carbon hierarchical structure. This structure withstands severe corrosive and oxidative environments and maintains stable performance across a wide temperature range, from cryogenic (−193 °C) to high temperature (500 °C) conditions. The graphitic carbon shell acts as an effective barrier, preventing oxidation and corrosion by creating lengthy diffusion routes within the hierarchical copper matrix. This enables the reliable operation of a printed antenna under a corrosive environment in a reliable fashion. The results show that the copper with a graphitic carbon shell has excellent oxidation and corrosion resistance capabilities, and the findings can be expanded to establish printed molecular decomposable materials as a platform for rapid prototyping of anticorrosion and antioxidation electronics suitable for different environmental conditions.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
ACS Applied Energy Materials
ACS Applied Energy Materials Materials Science-Materials Chemistry
CiteScore
10.30
自引率
6.20%
发文量
1368
期刊介绍: ACS Applied Energy Materials is an interdisciplinary journal publishing original research covering all aspects of materials, engineering, chemistry, physics and biology relevant to energy conversion and storage. The journal is devoted to reports of new and original experimental and theoretical research of an applied nature that integrate knowledge in the areas of materials, engineering, physics, bioscience, and chemistry into important energy applications.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信