掺杂 Nb2O5 对 TiO2-Al2O3 陶瓷低温烧结的影响

IF 2.9 Q1 MATERIALS SCIENCE, CERAMICS
Huei-Jyun Shih , Ying-Chieh Lee , Yu-De Li , Chang-Ting Yang
{"title":"掺杂 Nb2O5 对 TiO2-Al2O3 陶瓷低温烧结的影响","authors":"Huei-Jyun Shih ,&nbsp;Ying-Chieh Lee ,&nbsp;Yu-De Li ,&nbsp;Chang-Ting Yang","doi":"10.1016/j.oceram.2024.100635","DOIUrl":null,"url":null,"abstract":"<div><p>This study investigates the effects of Nb<sub>2</sub>O<sub>5</sub> as a dopant in TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics to lower sintering temperature and enhance performance, including the physical, mechanical, and dielectric properties of the ceramics at sintering temperatures 1250 °C–1350 °C. Specifically, TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics doped with 1.5 wt% Nb<sub>2</sub>O<sub>5</sub> and sintered at 1350 °C exhibit remarkable density 94 %, compressive strength 1372 MPa, and abrasion resistance 1.36 × 10<sup>−4</sup> mm<sup>3</sup>/N·m, surpassing those of pure alumina ceramics. This improvement is attributed to enhanced grain boundary diffusion and strain energy resulting from Nb<sup>5+</sup> cation substitution. The incorporation of Nb<sub>2</sub>O<sub>5</sub> in TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics reduce sintering temperatures by 150–200 °C. The dielectric constant of TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics doped with 1.5 wt% Nb<sub>2</sub>O<sub>5</sub> sintered at 1350 °C is found to be 13.4, with a dielectric loss of 2.56 × 10<sup>−2</sup> and insulation resistance 7.3 × 10<sup>12</sup> Ω. Nb<sub>2</sub>O<sub>5</sub> is an effective additive for reducing sintering temperatures in Al<sub>2</sub>O<sub>3</sub> based ceramic.</p></div>","PeriodicalId":34140,"journal":{"name":"Open Ceramics","volume":null,"pages":null},"PeriodicalIF":2.9000,"publicationDate":"2024-07-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.sciencedirect.com/science/article/pii/S2666539524000993/pdfft?md5=b93a1afe2e27d962b9facb5f4dbca5fc&pid=1-s2.0-S2666539524000993-main.pdf","citationCount":"0","resultStr":"{\"title\":\"Effect of Nb2O5 doping on low-temperature sintering of TiO2-Al2O3 ceramics\",\"authors\":\"Huei-Jyun Shih ,&nbsp;Ying-Chieh Lee ,&nbsp;Yu-De Li ,&nbsp;Chang-Ting Yang\",\"doi\":\"10.1016/j.oceram.2024.100635\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>This study investigates the effects of Nb<sub>2</sub>O<sub>5</sub> as a dopant in TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics to lower sintering temperature and enhance performance, including the physical, mechanical, and dielectric properties of the ceramics at sintering temperatures 1250 °C–1350 °C. Specifically, TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics doped with 1.5 wt% Nb<sub>2</sub>O<sub>5</sub> and sintered at 1350 °C exhibit remarkable density 94 %, compressive strength 1372 MPa, and abrasion resistance 1.36 × 10<sup>−4</sup> mm<sup>3</sup>/N·m, surpassing those of pure alumina ceramics. This improvement is attributed to enhanced grain boundary diffusion and strain energy resulting from Nb<sup>5+</sup> cation substitution. The incorporation of Nb<sub>2</sub>O<sub>5</sub> in TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics reduce sintering temperatures by 150–200 °C. The dielectric constant of TiO<sub>2</sub>–Al<sub>2</sub>O<sub>3</sub> ceramics doped with 1.5 wt% Nb<sub>2</sub>O<sub>5</sub> sintered at 1350 °C is found to be 13.4, with a dielectric loss of 2.56 × 10<sup>−2</sup> and insulation resistance 7.3 × 10<sup>12</sup> Ω. Nb<sub>2</sub>O<sub>5</sub> is an effective additive for reducing sintering temperatures in Al<sub>2</sub>O<sub>3</sub> based ceramic.</p></div>\",\"PeriodicalId\":34140,\"journal\":{\"name\":\"Open Ceramics\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":2.9000,\"publicationDate\":\"2024-07-03\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://www.sciencedirect.com/science/article/pii/S2666539524000993/pdfft?md5=b93a1afe2e27d962b9facb5f4dbca5fc&pid=1-s2.0-S2666539524000993-main.pdf\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Open Ceramics\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S2666539524000993\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q1\",\"JCRName\":\"MATERIALS SCIENCE, CERAMICS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Open Ceramics","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2666539524000993","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, CERAMICS","Score":null,"Total":0}
引用次数: 0

摘要

本研究探讨了在 TiO2-Al2O3 陶瓷中掺杂 Nb2O5 对降低烧结温度和提高性能的影响,包括烧结温度为 1250 °C-1350 °C 时陶瓷的物理、机械和介电性质。具体来说,掺杂了 1.5 wt% Nb2O5 并在 1350 °C 下烧结的 TiO2-Al2O3 陶瓷显示出显著的密度 94 %、抗压强度 1372 MPa 和耐磨性 1.36 × 10-4 mm3/N-m,超过了纯氧化铝陶瓷。这种改善归因于 Nb5+ 阳离子替代增强了晶界扩散和应变能。在 TiO2-Al2O3 陶瓷中加入 Nb2O5 可使烧结温度降低 150-200 ℃。在 1350 ℃ 下烧结的掺有 1.5 wt% Nb2O5 的 TiO2-Al2O3 陶瓷的介电常数为 13.4,介电损耗为 2.56 × 10-2,绝缘电阻为 7.3 × 1012 Ω。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Effect of Nb2O5 doping on low-temperature sintering of TiO2-Al2O3 ceramics

Effect of Nb2O5 doping on low-temperature sintering of TiO2-Al2O3 ceramics

This study investigates the effects of Nb2O5 as a dopant in TiO2–Al2O3 ceramics to lower sintering temperature and enhance performance, including the physical, mechanical, and dielectric properties of the ceramics at sintering temperatures 1250 °C–1350 °C. Specifically, TiO2–Al2O3 ceramics doped with 1.5 wt% Nb2O5 and sintered at 1350 °C exhibit remarkable density 94 %, compressive strength 1372 MPa, and abrasion resistance 1.36 × 10−4 mm3/N·m, surpassing those of pure alumina ceramics. This improvement is attributed to enhanced grain boundary diffusion and strain energy resulting from Nb5+ cation substitution. The incorporation of Nb2O5 in TiO2–Al2O3 ceramics reduce sintering temperatures by 150–200 °C. The dielectric constant of TiO2–Al2O3 ceramics doped with 1.5 wt% Nb2O5 sintered at 1350 °C is found to be 13.4, with a dielectric loss of 2.56 × 10−2 and insulation resistance 7.3 × 1012 Ω. Nb2O5 is an effective additive for reducing sintering temperatures in Al2O3 based ceramic.

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
Open Ceramics
Open Ceramics Materials Science-Materials Chemistry
CiteScore
4.20
自引率
0.00%
发文量
102
审稿时长
67 days
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信