低温滚压、室温轧制和时效处理对 Cu-6Ni-6Sn 合金的机械、电气和磨损特性的影响

Zhibao Xie, Zhide Li, Delin Tang, Zhengyu Wang, Huijie Cui, Charlie Kong, Hailiang Yu
{"title":"低温滚压、室温轧制和时效处理对 Cu-6Ni-6Sn 合金的机械、电气和磨损特性的影响","authors":"Zhibao Xie, Zhide Li, Delin Tang, Zhengyu Wang, Huijie Cui, Charlie Kong, Hailiang Yu","doi":"10.1007/s11661-024-07466-w","DOIUrl":null,"url":null,"abstract":"<p>The effects of cryorolling (CR), room-temperature rolling (RTR), and subsequent aging on the mechanical, electrical, and wear characteristics of Cu-6Ni-6Sn alloys were examined. Compared to the RTR specimens, those subjected to CR displayed a higher dislocation density and a greater number of nanosized deformation twins. The CR facilitated the uniform and dense formation of precipitates, enabling the CR-treated alloys to achieve an optimal balance of strength (1004 MPa), electrical conductivity (11.8 pct IACS), and wear resistance.</p><h3 data-test=\"abstract-sub-heading\">Graphical Abstract</h3>\n","PeriodicalId":18504,"journal":{"name":"Metallurgical and Materials Transactions A","volume":"23 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-06-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Effects of Cryorolling, Room Temperature Rolling, and Aging Treatment on the Mechanical, Electrical, and Wear Properties of a Cu-6Ni-6Sn Alloy\",\"authors\":\"Zhibao Xie, Zhide Li, Delin Tang, Zhengyu Wang, Huijie Cui, Charlie Kong, Hailiang Yu\",\"doi\":\"10.1007/s11661-024-07466-w\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<p>The effects of cryorolling (CR), room-temperature rolling (RTR), and subsequent aging on the mechanical, electrical, and wear characteristics of Cu-6Ni-6Sn alloys were examined. Compared to the RTR specimens, those subjected to CR displayed a higher dislocation density and a greater number of nanosized deformation twins. The CR facilitated the uniform and dense formation of precipitates, enabling the CR-treated alloys to achieve an optimal balance of strength (1004 MPa), electrical conductivity (11.8 pct IACS), and wear resistance.</p><h3 data-test=\\\"abstract-sub-heading\\\">Graphical Abstract</h3>\\n\",\"PeriodicalId\":18504,\"journal\":{\"name\":\"Metallurgical and Materials Transactions A\",\"volume\":\"23 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2024-06-25\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Metallurgical and Materials Transactions A\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1007/s11661-024-07466-w\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metallurgical and Materials Transactions A","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1007/s11661-024-07466-w","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

研究了低温滚压(CR)、室温轧制(RTR)和后续时效对铜-6镍-6锑合金的机械、电气和磨损特性的影响。与 RTR 试样相比,CR 试样显示出更高的位错密度和更多的纳米级变形孪晶。CR促进了析出物均匀致密的形成,使CR处理过的合金在强度(1004兆帕)、导电性(11.8 pct IACS)和耐磨性之间达到了最佳平衡。
本文章由计算机程序翻译,如有差异,请以英文原文为准。

Effects of Cryorolling, Room Temperature Rolling, and Aging Treatment on the Mechanical, Electrical, and Wear Properties of a Cu-6Ni-6Sn Alloy

Effects of Cryorolling, Room Temperature Rolling, and Aging Treatment on the Mechanical, Electrical, and Wear Properties of a Cu-6Ni-6Sn Alloy

The effects of cryorolling (CR), room-temperature rolling (RTR), and subsequent aging on the mechanical, electrical, and wear characteristics of Cu-6Ni-6Sn alloys were examined. Compared to the RTR specimens, those subjected to CR displayed a higher dislocation density and a greater number of nanosized deformation twins. The CR facilitated the uniform and dense formation of precipitates, enabling the CR-treated alloys to achieve an optimal balance of strength (1004 MPa), electrical conductivity (11.8 pct IACS), and wear resistance.

Graphical Abstract

求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信