{"title":"阐明油棕(Elaeis guineensis)生物质中木质纤维素成分和物理化学变化对酶糖化产量的相关性","authors":"Tannimalay Hemashini, Chee Keong Lee, Choon Fu Goh, Ying Ying Tye, Maya Ismayati, Yin Ying H’ng, Cheu Peng Leh","doi":"10.1007/s12155-024-10762-3","DOIUrl":null,"url":null,"abstract":"<div><p>This study investigates the correlation between both the chemical compositions and physicochemical properties of pretreated oil palm empty fruit bunch (OPEFB) fibre and their enzymatic saccharification/total glucose yield (TGY). Twenty OPEFB samples, pretreated with various aqueous pretreatments, with diverse cellulose (25.63–44.23%), hemicellulose (0.01–42.49%), and lignin (3.7–47.1%) levels, were examined for their correlation with TGY (8.5–40%). The quadratic regression model was verified significant (<i>p-</i>value = 0.0006, <i>R</i><sup>2</sup> = 0.8006). It was found that the pre-refined OPEFB experienced greater cellulose loss (35%) compared to unrefined ones (9%), adversely affecting TGY. Among physicochemical properties analysed using SEM, FTIR, XRD, Py-GCMS, and XPS, only crystallinity index (CrI) was significantly correlated with TGY based on theoretical glucose concentration (TGC) (<i>R</i><sup>2</sup> = 0.77, 0.91). Other characteristics (morphology, functional groups, crystallite size, S/G ratio, and O/C ratio) exhibited no significant correlation to saccharification efficiency, exhibiting random trends (<i>R</i><sup>2</sup> < 0.5). OPEFB fibres with CrI of 30–40 could achieve 100% TGY based on TGC. In conclusion, regardless of pretreatments, chemical compositions predominantly affected TGY in the enzymatic saccharification of biomass. Among commonly used physicochemical analytical methods, CrI is most significant in this evaluation and OPEFB should be unrefined before treatment to avoid cellulose loss.</p><h3>Graphical Abstract</h3>\n<div><figure><div><div><picture><source><img></source></picture></div></div></figure></div></div>","PeriodicalId":487,"journal":{"name":"BioEnergy Research","volume":"17 3","pages":"1612 - 1630"},"PeriodicalIF":3.1000,"publicationDate":"2024-05-08","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Elucidating the Correlation of Lignocellulosic Compositions and Physicochemical Alterations in Oil Palm (Elaeis guineensis) Biomass on Enzymatic Saccharification Yield\",\"authors\":\"Tannimalay Hemashini, Chee Keong Lee, Choon Fu Goh, Ying Ying Tye, Maya Ismayati, Yin Ying H’ng, Cheu Peng Leh\",\"doi\":\"10.1007/s12155-024-10762-3\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>This study investigates the correlation between both the chemical compositions and physicochemical properties of pretreated oil palm empty fruit bunch (OPEFB) fibre and their enzymatic saccharification/total glucose yield (TGY). Twenty OPEFB samples, pretreated with various aqueous pretreatments, with diverse cellulose (25.63–44.23%), hemicellulose (0.01–42.49%), and lignin (3.7–47.1%) levels, were examined for their correlation with TGY (8.5–40%). The quadratic regression model was verified significant (<i>p-</i>value = 0.0006, <i>R</i><sup>2</sup> = 0.8006). It was found that the pre-refined OPEFB experienced greater cellulose loss (35%) compared to unrefined ones (9%), adversely affecting TGY. Among physicochemical properties analysed using SEM, FTIR, XRD, Py-GCMS, and XPS, only crystallinity index (CrI) was significantly correlated with TGY based on theoretical glucose concentration (TGC) (<i>R</i><sup>2</sup> = 0.77, 0.91). Other characteristics (morphology, functional groups, crystallite size, S/G ratio, and O/C ratio) exhibited no significant correlation to saccharification efficiency, exhibiting random trends (<i>R</i><sup>2</sup> < 0.5). OPEFB fibres with CrI of 30–40 could achieve 100% TGY based on TGC. In conclusion, regardless of pretreatments, chemical compositions predominantly affected TGY in the enzymatic saccharification of biomass. Among commonly used physicochemical analytical methods, CrI is most significant in this evaluation and OPEFB should be unrefined before treatment to avoid cellulose loss.</p><h3>Graphical Abstract</h3>\\n<div><figure><div><div><picture><source><img></source></picture></div></div></figure></div></div>\",\"PeriodicalId\":487,\"journal\":{\"name\":\"BioEnergy Research\",\"volume\":\"17 3\",\"pages\":\"1612 - 1630\"},\"PeriodicalIF\":3.1000,\"publicationDate\":\"2024-05-08\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"BioEnergy Research\",\"FirstCategoryId\":\"5\",\"ListUrlMain\":\"https://link.springer.com/article/10.1007/s12155-024-10762-3\",\"RegionNum\":3,\"RegionCategory\":\"工程技术\",\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"Q3\",\"JCRName\":\"ENERGY & FUELS\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"BioEnergy Research","FirstCategoryId":"5","ListUrlMain":"https://link.springer.com/article/10.1007/s12155-024-10762-3","RegionNum":3,"RegionCategory":"工程技术","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"ENERGY & FUELS","Score":null,"Total":0}
Elucidating the Correlation of Lignocellulosic Compositions and Physicochemical Alterations in Oil Palm (Elaeis guineensis) Biomass on Enzymatic Saccharification Yield
This study investigates the correlation between both the chemical compositions and physicochemical properties of pretreated oil palm empty fruit bunch (OPEFB) fibre and their enzymatic saccharification/total glucose yield (TGY). Twenty OPEFB samples, pretreated with various aqueous pretreatments, with diverse cellulose (25.63–44.23%), hemicellulose (0.01–42.49%), and lignin (3.7–47.1%) levels, were examined for their correlation with TGY (8.5–40%). The quadratic regression model was verified significant (p-value = 0.0006, R2 = 0.8006). It was found that the pre-refined OPEFB experienced greater cellulose loss (35%) compared to unrefined ones (9%), adversely affecting TGY. Among physicochemical properties analysed using SEM, FTIR, XRD, Py-GCMS, and XPS, only crystallinity index (CrI) was significantly correlated with TGY based on theoretical glucose concentration (TGC) (R2 = 0.77, 0.91). Other characteristics (morphology, functional groups, crystallite size, S/G ratio, and O/C ratio) exhibited no significant correlation to saccharification efficiency, exhibiting random trends (R2 < 0.5). OPEFB fibres with CrI of 30–40 could achieve 100% TGY based on TGC. In conclusion, regardless of pretreatments, chemical compositions predominantly affected TGY in the enzymatic saccharification of biomass. Among commonly used physicochemical analytical methods, CrI is most significant in this evaluation and OPEFB should be unrefined before treatment to avoid cellulose loss.
期刊介绍:
BioEnergy Research fills a void in the rapidly growing area of feedstock biology research related to biomass, biofuels, and bioenergy. The journal publishes a wide range of articles, including peer-reviewed scientific research, reviews, perspectives and commentary, industry news, and government policy updates. Its coverage brings together a uniquely broad combination of disciplines with a common focus on feedstock biology and science, related to biomass, biofeedstock, and bioenergy production.