热处理对7CrMoVTiB10-10钢焊接接头组织和硬度的影响

A. Rzeźnikiewicz, Mateusz Żołnierek
{"title":"热处理对7CrMoVTiB10-10钢焊接接头组织和硬度的影响","authors":"A. Rzeźnikiewicz, Mateusz Żołnierek","doi":"10.17729/ebis.2020.2/4","DOIUrl":null,"url":null,"abstract":"The article presents results of tests concerning the effect of heat treatment on the structure and hardness of submerged arc welded joints made in steel 7CrMoVTiB10-10 (T24). The tests revealed that the welds made of steel 7CrMoVTiB10-10 required post-weld heat treatment at a temperature 750°C. The heat treatment was performed in order to protect welded structures from cracking during transport and operation as well as to prevent the development of secondary hardness.","PeriodicalId":184101,"journal":{"name":"Biuletyn Instytutu Spawalnictwa","volume":"50 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2020-04-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"The Effect of Heat Treatment on the Structure and Hardness of Welded Joints in Steel 7CrMoVTiB10-10\",\"authors\":\"A. Rzeźnikiewicz, Mateusz Żołnierek\",\"doi\":\"10.17729/ebis.2020.2/4\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The article presents results of tests concerning the effect of heat treatment on the structure and hardness of submerged arc welded joints made in steel 7CrMoVTiB10-10 (T24). The tests revealed that the welds made of steel 7CrMoVTiB10-10 required post-weld heat treatment at a temperature 750°C. The heat treatment was performed in order to protect welded structures from cracking during transport and operation as well as to prevent the development of secondary hardness.\",\"PeriodicalId\":184101,\"journal\":{\"name\":\"Biuletyn Instytutu Spawalnictwa\",\"volume\":\"50 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-04-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Biuletyn Instytutu Spawalnictwa\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.17729/ebis.2020.2/4\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Biuletyn Instytutu Spawalnictwa","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.17729/ebis.2020.2/4","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

本文介绍了热处理对7CrMoVTiB10-10 (T24)钢埋弧焊接头组织和硬度影响的试验结果。试验表明,7CrMoVTiB10-10钢的焊缝需要在750℃下进行焊后热处理。进行热处理是为了防止焊接结构在运输和操作过程中开裂,并防止二次硬度的产生。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
The Effect of Heat Treatment on the Structure and Hardness of Welded Joints in Steel 7CrMoVTiB10-10
The article presents results of tests concerning the effect of heat treatment on the structure and hardness of submerged arc welded joints made in steel 7CrMoVTiB10-10 (T24). The tests revealed that the welds made of steel 7CrMoVTiB10-10 required post-weld heat treatment at a temperature 750°C. The heat treatment was performed in order to protect welded structures from cracking during transport and operation as well as to prevent the development of secondary hardness.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信