K. Umezawa, M. Inukai, S. Mori, T. Sato, I. Mizushima, H. Tomita, A. Yomoda
{"title":"采用超32nm节点外延硅锗(SiGe)工艺的先进表面清洁度评价技术","authors":"K. Umezawa, M. Inukai, S. Mori, T. Sato, I. Mizushima, H. Tomita, A. Yomoda","doi":"10.1109/ISSM.2007.4446888","DOIUrl":null,"url":null,"abstract":"Epitaxial growth process strongly depends on the substrate surface cleanliness. In this study, advanced surface cleanness evaluation techniques for 32 nm node and beyond such as light point defects (LPDs) and haze measurements are studied using epitaxial silicon germanium (SiGe) process on 300 mm wafers. Small water marks formed during wafer drying can be detected as small LPDs just after pre-cleaning. These water marks inhibit SiGe growth during the epitaxial process. In addition, SiGe film LPDs increase drastically with increasing queue time between pre-cleaning process and SiGe CVD process. Finally, SURFimage haze measurement is shown to be a powerful advanced technique to monitor the localized \"abnormal growth defects\" and the surface morphology of the SiGe CVD film over the full wafer surface.","PeriodicalId":325607,"journal":{"name":"2007 International Symposium on Semiconductor Manufacturing","volume":"19 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2007-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":"{\"title\":\"Advanced surface cleanness evaluation technique using epitaxial silicon germanium (SiGe) process beyond 32nm node\",\"authors\":\"K. Umezawa, M. Inukai, S. Mori, T. Sato, I. Mizushima, H. Tomita, A. Yomoda\",\"doi\":\"10.1109/ISSM.2007.4446888\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Epitaxial growth process strongly depends on the substrate surface cleanliness. In this study, advanced surface cleanness evaluation techniques for 32 nm node and beyond such as light point defects (LPDs) and haze measurements are studied using epitaxial silicon germanium (SiGe) process on 300 mm wafers. Small water marks formed during wafer drying can be detected as small LPDs just after pre-cleaning. These water marks inhibit SiGe growth during the epitaxial process. In addition, SiGe film LPDs increase drastically with increasing queue time between pre-cleaning process and SiGe CVD process. Finally, SURFimage haze measurement is shown to be a powerful advanced technique to monitor the localized \\\"abnormal growth defects\\\" and the surface morphology of the SiGe CVD film over the full wafer surface.\",\"PeriodicalId\":325607,\"journal\":{\"name\":\"2007 International Symposium on Semiconductor Manufacturing\",\"volume\":\"19 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2007-10-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"4\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2007 International Symposium on Semiconductor Manufacturing\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/ISSM.2007.4446888\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2007 International Symposium on Semiconductor Manufacturing","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ISSM.2007.4446888","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Advanced surface cleanness evaluation technique using epitaxial silicon germanium (SiGe) process beyond 32nm node
Epitaxial growth process strongly depends on the substrate surface cleanliness. In this study, advanced surface cleanness evaluation techniques for 32 nm node and beyond such as light point defects (LPDs) and haze measurements are studied using epitaxial silicon germanium (SiGe) process on 300 mm wafers. Small water marks formed during wafer drying can be detected as small LPDs just after pre-cleaning. These water marks inhibit SiGe growth during the epitaxial process. In addition, SiGe film LPDs increase drastically with increasing queue time between pre-cleaning process and SiGe CVD process. Finally, SURFimage haze measurement is shown to be a powerful advanced technique to monitor the localized "abnormal growth defects" and the surface morphology of the SiGe CVD film over the full wafer surface.