Salmiah Mohd. Nor, W. Ahmad, J. Salleh, N. Zakaria, R. Ismail
{"title":"棉织物和涤纶/棉织物的耐用压力机参考资料","authors":"Salmiah Mohd. Nor, W. Ahmad, J. Salleh, N. Zakaria, R. Ismail","doi":"10.1109/CSSR.2010.5773896","DOIUrl":null,"url":null,"abstract":"A Durable Press (DP) finish of NuDURA PRESS® was applied on light and medium weight cotton and polyester/cotton (65/35) fabrics after dyeing and in a single bath process of combined dyeing and finishing. The DP formulation consisted of low formaldehyde durable press agent with polysiloxane softener, applied by the pad-dry-cure method in a manufacturing process at the textile mill. The finished fabrics have improved properties of wrinkle resistance and draping quality. The wrinkle resistance was determined by the wrinkle recovery angle (WRA) and appearance, while that of the draping quality by the stiffness and drape coefficient. A Durable Press Reference (DPR) was formulated using values of wrinkle resistance and draping quality. The DPR for finished fabrics after dyeing was 3.46 to 7.15, while that in a single bath process of combined dyeing and finishing was 3.39 to 6.04, differently for each fabric. The DPR formula can be used to evaluate objectively the DP performances of fabrics.","PeriodicalId":236344,"journal":{"name":"2010 International Conference on Science and Social Research (CSSR 2010)","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2010-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Durable Press Reference for cotton and polyester/cotton fabrics\",\"authors\":\"Salmiah Mohd. Nor, W. Ahmad, J. Salleh, N. Zakaria, R. Ismail\",\"doi\":\"10.1109/CSSR.2010.5773896\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"A Durable Press (DP) finish of NuDURA PRESS® was applied on light and medium weight cotton and polyester/cotton (65/35) fabrics after dyeing and in a single bath process of combined dyeing and finishing. The DP formulation consisted of low formaldehyde durable press agent with polysiloxane softener, applied by the pad-dry-cure method in a manufacturing process at the textile mill. The finished fabrics have improved properties of wrinkle resistance and draping quality. The wrinkle resistance was determined by the wrinkle recovery angle (WRA) and appearance, while that of the draping quality by the stiffness and drape coefficient. A Durable Press Reference (DPR) was formulated using values of wrinkle resistance and draping quality. The DPR for finished fabrics after dyeing was 3.46 to 7.15, while that in a single bath process of combined dyeing and finishing was 3.39 to 6.04, differently for each fabric. The DPR formula can be used to evaluate objectively the DP performances of fabrics.\",\"PeriodicalId\":236344,\"journal\":{\"name\":\"2010 International Conference on Science and Social Research (CSSR 2010)\",\"volume\":\"1 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2010-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2010 International Conference on Science and Social Research (CSSR 2010)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/CSSR.2010.5773896\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2010 International Conference on Science and Social Research (CSSR 2010)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/CSSR.2010.5773896","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Durable Press Reference for cotton and polyester/cotton fabrics
A Durable Press (DP) finish of NuDURA PRESS® was applied on light and medium weight cotton and polyester/cotton (65/35) fabrics after dyeing and in a single bath process of combined dyeing and finishing. The DP formulation consisted of low formaldehyde durable press agent with polysiloxane softener, applied by the pad-dry-cure method in a manufacturing process at the textile mill. The finished fabrics have improved properties of wrinkle resistance and draping quality. The wrinkle resistance was determined by the wrinkle recovery angle (WRA) and appearance, while that of the draping quality by the stiffness and drape coefficient. A Durable Press Reference (DPR) was formulated using values of wrinkle resistance and draping quality. The DPR for finished fabrics after dyeing was 3.46 to 7.15, while that in a single bath process of combined dyeing and finishing was 3.39 to 6.04, differently for each fabric. The DPR formula can be used to evaluate objectively the DP performances of fabrics.