{"title":"链索的脆性断裂","authors":"","doi":"10.31399/asm.fach.matlhand.c9001453","DOIUrl":null,"url":null,"abstract":"\n While a chain sling was being used to lift a casting one of the links ruptured. The sling, reputed to be of the electrically-welded steel type, was at least eight years old and had been overhauled several times during its working life. Examination showed the links were scarf-welded. Furthermore, the welds were at the ends and not at the sides as is usual in the case of electrically-welded chains. A transverse section from one side of a link was examined microscopically. This showed the material to be wrought-iron of satisfactory quality. It was concluded this chain sling had been made from wrought-iron, forge welded in the usual manner, and that it was not electrically-welded steel as had been supposed. Failure was attributed to embrittlement in service of the surface material of the links. If it had been realized that the sling was made from wrought-iron then it would doubtless have been subjected to periodical annealing in accordance with Statutory requirements, which would have restored the ductility of the surface material.","PeriodicalId":131762,"journal":{"name":"ASM Failure Analysis Case Histories: Material Handling Equipment","volume":"46 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2019-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Brittle Rupture of a Chain Sling\",\"authors\":\"\",\"doi\":\"10.31399/asm.fach.matlhand.c9001453\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"\\n While a chain sling was being used to lift a casting one of the links ruptured. The sling, reputed to be of the electrically-welded steel type, was at least eight years old and had been overhauled several times during its working life. Examination showed the links were scarf-welded. Furthermore, the welds were at the ends and not at the sides as is usual in the case of electrically-welded chains. A transverse section from one side of a link was examined microscopically. This showed the material to be wrought-iron of satisfactory quality. It was concluded this chain sling had been made from wrought-iron, forge welded in the usual manner, and that it was not electrically-welded steel as had been supposed. Failure was attributed to embrittlement in service of the surface material of the links. If it had been realized that the sling was made from wrought-iron then it would doubtless have been subjected to periodical annealing in accordance with Statutory requirements, which would have restored the ductility of the surface material.\",\"PeriodicalId\":131762,\"journal\":{\"name\":\"ASM Failure Analysis Case Histories: Material Handling Equipment\",\"volume\":\"46 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2019-06-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"ASM Failure Analysis Case Histories: Material Handling Equipment\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.31399/asm.fach.matlhand.c9001453\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"ASM Failure Analysis Case Histories: Material Handling Equipment","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.31399/asm.fach.matlhand.c9001453","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

当链条吊带被用来吊起一个铸件时,其中一个链环破裂了。吊索,被认为是电焊钢类型,至少有8年的历史,并在其工作寿命期间进行了几次大修。检查显示链接是带状焊接的。此外,焊缝是在末端,而不是在侧面,这是电焊链的常见情况。在显微镜下观察了一个连杆一侧的横切面。这表明这种材料是质量令人满意的熟铁。结论是,这条吊索是用熟铁做的,是用通常的方法锻造焊接而成的,而不是人们所认为的电焊钢。失效的原因是连杆表面材料在使用过程中发生脆化。如果人们意识到吊索是由熟铁制成的,那么毫无疑问,它将按照法定要求进行定期退火,这将恢复表面材料的延展性。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Brittle Rupture of a Chain Sling
While a chain sling was being used to lift a casting one of the links ruptured. The sling, reputed to be of the electrically-welded steel type, was at least eight years old and had been overhauled several times during its working life. Examination showed the links were scarf-welded. Furthermore, the welds were at the ends and not at the sides as is usual in the case of electrically-welded chains. A transverse section from one side of a link was examined microscopically. This showed the material to be wrought-iron of satisfactory quality. It was concluded this chain sling had been made from wrought-iron, forge welded in the usual manner, and that it was not electrically-welded steel as had been supposed. Failure was attributed to embrittlement in service of the surface material of the links. If it had been realized that the sling was made from wrought-iron then it would doubtless have been subjected to periodical annealing in accordance with Statutory requirements, which would have restored the ductility of the surface material.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信