{"title":"镍及镍磷合金镀层的耐磨性","authors":"C. A. Holden, R. Opila, H. H. Law, G. R. Crane","doi":"10.1109/33.19014","DOIUrl":null,"url":null,"abstract":"The wear resistance of gray Ni/Cl and Ni/P deposits was evaluated using a crossed-wire test method that stimulates the wear that develops on plug-in type printed wiring boards. All wear samples were lubricated with 2-wt.% five- or six-ring polyphenylether fluid. Some samples plated with a thin layer of cobalt-hardened gold were also examined. Wear test results showed that: (1) gray Ni/P deposits plated from a neutral ammoniacal bath are more wear-resistant for up to 100 wear cycles than nickel deposits plated from an acid chloride bath; (2) hard-gold-flashed Ni/P deposits are more wear-resistant for up to 5000 wear cycles at a 200-g load than hard-gold-flashed nickel deposits plated from an acid chloride bath. A minimum of 5 mu in. hard gold provides this wear protection.<<ETX>>","PeriodicalId":191800,"journal":{"name":"Electrical Contacts, 1988., Proceedings of the Thirty Fourth Meeting of the IEEE Holm Conference on Electrical Contacts","volume":"518 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1900-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"8","resultStr":"{\"title\":\"Wear resistance of nickel and nickel phosphorus alloy electrodeposits\",\"authors\":\"C. A. Holden, R. Opila, H. H. Law, G. R. Crane\",\"doi\":\"10.1109/33.19014\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The wear resistance of gray Ni/Cl and Ni/P deposits was evaluated using a crossed-wire test method that stimulates the wear that develops on plug-in type printed wiring boards. All wear samples were lubricated with 2-wt.% five- or six-ring polyphenylether fluid. Some samples plated with a thin layer of cobalt-hardened gold were also examined. Wear test results showed that: (1) gray Ni/P deposits plated from a neutral ammoniacal bath are more wear-resistant for up to 100 wear cycles than nickel deposits plated from an acid chloride bath; (2) hard-gold-flashed Ni/P deposits are more wear-resistant for up to 5000 wear cycles at a 200-g load than hard-gold-flashed nickel deposits plated from an acid chloride bath. A minimum of 5 mu in. hard gold provides this wear protection.<<ETX>>\",\"PeriodicalId\":191800,\"journal\":{\"name\":\"Electrical Contacts, 1988., Proceedings of the Thirty Fourth Meeting of the IEEE Holm Conference on Electrical Contacts\",\"volume\":\"518 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1900-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"8\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Electrical Contacts, 1988., Proceedings of the Thirty Fourth Meeting of the IEEE Holm Conference on Electrical Contacts\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/33.19014\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Electrical Contacts, 1988., Proceedings of the Thirty Fourth Meeting of the IEEE Holm Conference on Electrical Contacts","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/33.19014","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 8

摘要

灰色Ni/Cl和Ni/P沉积层的耐磨性使用交叉线测试方法进行评估,该方法刺激在插入式印刷线路板上产生的磨损。所有磨损样品都用2-wt润滑。五环或六环聚苯醚液体。一些镀有一层钴硬化金的样品也被检查了。磨损试验结果表明:(1)中性氨浴镀的灰色Ni/P镀层比酸性氯化物浴镀的镍镀层具有更高的耐磨性,耐磨性可达100次;(2)硬金闪蒸镍/P镀层在200克载荷下的耐磨性优于硬金闪蒸镍镀层。至少5亩。硬金提供这种磨损保护
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Wear resistance of nickel and nickel phosphorus alloy electrodeposits
The wear resistance of gray Ni/Cl and Ni/P deposits was evaluated using a crossed-wire test method that stimulates the wear that develops on plug-in type printed wiring boards. All wear samples were lubricated with 2-wt.% five- or six-ring polyphenylether fluid. Some samples plated with a thin layer of cobalt-hardened gold were also examined. Wear test results showed that: (1) gray Ni/P deposits plated from a neutral ammoniacal bath are more wear-resistant for up to 100 wear cycles than nickel deposits plated from an acid chloride bath; (2) hard-gold-flashed Ni/P deposits are more wear-resistant for up to 5000 wear cycles at a 200-g load than hard-gold-flashed nickel deposits plated from an acid chloride bath. A minimum of 5 mu in. hard gold provides this wear protection.<>
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信