The Effect of Acid Concentration on the Chemical Leaching of El-Gedida High-Ba Iron Ore, El-Bahariya Oasis, Western Desert, Egypt

G. El-Habaak, M. Askalany, M. Farghaly, M. Abdel-Hakeem
{"title":"The Effect of Acid Concentration on the Chemical Leaching of El-Gedida High-Ba Iron Ore, El-Bahariya Oasis, Western Desert, Egypt","authors":"G. El-Habaak, M. Askalany, M. Farghaly, M. Abdel-Hakeem","doi":"10.12983/ijsrk-2017-p0020-0026","DOIUrl":null,"url":null,"abstract":"El-Gedida high-Ba iron ore was subjected to microscopic, mineralogical and chemical characterizations followed by chemical leaching using HCl. The microscopic investigations revealed that the textural relationships between barite and iron minerals are complicated, resulting in a difficult liberation during the comminution process. XRD analysis of the studied ore indicated the presence of hematite and goethite as the dominant iron minerals and barite, quartz and halite as gangue minerals. Chemical assays using XRF showed that the investigated ore contains 42.29% Fe2O3 (29.58% Fe total), 36.99% BaO and 16.95% SO3. The pre-treatment operations involved crushing and milling up to -150μm particle size. The processing operation included chemical leaching of 15 gm representative sample of the ground ore using acidic medium of HCl at fixed agitation speed 900 r/m. The leaching was followed by filtration, solvent extraction and precipitation processes. The resultant dual concentrate is divided into iron fraction containing 66.11% Fe with 99.84% iron recovery and barite concentrate containing 66.85% BaO (99.81% recovery) and 30.53% SO3 (99.47% recovery). The resultant iron fraction is accepted as a blast furnace feed charge for the Egyptian Iron & Steel Company, while barite fraction can be used for the oil industry and glassmaking.","PeriodicalId":14310,"journal":{"name":"International Journal of Scientific Research in Knowledge","volume":"37 1","pages":"20-26"},"PeriodicalIF":0.0000,"publicationDate":"2017-03-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Scientific Research in Knowledge","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.12983/ijsrk-2017-p0020-0026","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

El-Gedida high-Ba iron ore was subjected to microscopic, mineralogical and chemical characterizations followed by chemical leaching using HCl. The microscopic investigations revealed that the textural relationships between barite and iron minerals are complicated, resulting in a difficult liberation during the comminution process. XRD analysis of the studied ore indicated the presence of hematite and goethite as the dominant iron minerals and barite, quartz and halite as gangue minerals. Chemical assays using XRF showed that the investigated ore contains 42.29% Fe2O3 (29.58% Fe total), 36.99% BaO and 16.95% SO3. The pre-treatment operations involved crushing and milling up to -150μm particle size. The processing operation included chemical leaching of 15 gm representative sample of the ground ore using acidic medium of HCl at fixed agitation speed 900 r/m. The leaching was followed by filtration, solvent extraction and precipitation processes. The resultant dual concentrate is divided into iron fraction containing 66.11% Fe with 99.84% iron recovery and barite concentrate containing 66.85% BaO (99.81% recovery) and 30.53% SO3 (99.47% recovery). The resultant iron fraction is accepted as a blast furnace feed charge for the Egyptian Iron & Steel Company, while barite fraction can be used for the oil industry and glassmaking.
酸浓度对埃及西部沙漠El-Bahariya绿洲El-Gedida高钡铁矿化学浸出的影响
对El-Gedida高钡铁矿进行了显微、矿物学和化学表征,并用HCl进行了化学浸出。显微研究表明,重晶石与铁矿物的结构关系复杂,在粉碎过程中难以解离。研究矿石的XRD分析表明,主要铁矿物为赤铁矿和针铁矿,脉石矿物为重晶石、石英和岩盐。XRF化学分析表明,该矿石的Fe2O3含量为42.29%(总Fe含量为29.58%),BaO含量为36.99%,SO3含量为16.95%。预处理操作包括破碎和磨铣至-150μm的粒度。工艺操作为:采用酸性盐酸介质,以固定搅拌速度900 r/m,化学浸出15 gm磨矿代表性样品。浸出后进行过滤、溶剂萃取和沉淀。所得双精矿分为含铁66.11%、铁回收率99.84%的铁段和含钡66.85%(回收率99.81%)、SO3 30.53%(回收率99.47%)的重晶石精矿。所得铁馏分可作为埃及钢铁公司的高炉进料,而重晶石馏分可用于石油工业和玻璃制造。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信