{"title":"介孔分子筛MCM-41固载磷钨酸催化苯并三氮唑与查尔酮的氮杂迈克加成反应研究 Aza-Michael Addition of Chalcone with Benzotriazole Catalyzed by MCM-41 Immobilized H3PW12O40","authors":"杨敬辉, 邢刘庄, 谢绍雷, 邢雪建, 侯亚东, 吴阳, 惠永海","doi":"10.12677/JOCR.2017.52014","DOIUrl":null,"url":null,"abstract":"以介孔分子筛MCM-41固载磷钨酸为催化剂,对苯并三氮唑与查尔酮进行了氮杂迈克加成的催化研究。经过条件筛选,发现MCM-41中的磷钨酸负载量对该反应体系有很大的影响,其中50 wt%的磷钨酸负载量更有利于反应的进行,产率可达98%。通过NMR对产物结构进行了表征,并且催化剂具有一定的回收再利用效果。 In this paper, mesoporous siliceous material MCM-41 supported H3PW12O40 (PW) could act as an efficient catalyst for the aza-Michael addition reaction of chalcone with benzotriazole. As can be seen from a serial of reaction conditions, the ratio of PW and MCM-41 plays a critical role in the reaction, and the best catalyzed result was achieved when using 50 wt% PW/MCM-41, and the yield was up to 98%. All the products were confirmed by NMR techniques. Moreover, the catalyst was also found to exhibit better recyclability.","PeriodicalId":16596,"journal":{"name":"Journal of Organic Chemistry Research","volume":"32 1","pages":"107-113"},"PeriodicalIF":0.0000,"publicationDate":"2017-05-17","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Organic Chemistry Research","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.12677/JOCR.2017.52014","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
以介孔分子筛MCM-41固载磷钨酸为催化剂,对苯并三氮唑与查尔酮进行了氮杂迈克加成的催化研究。经过条件筛选,发现MCM-41中的磷钨酸负载量对该反应体系有很大的影响,其中50 wt%的磷钨酸负载量更有利于反应的进行,产率可达98%。通过NMR对产物结构进行了表征,并且催化剂具有一定的回收再利用效果。 In this paper, mesoporous siliceous material MCM-41 supported H3PW12O40 (PW) could act as an efficient catalyst for the aza-Michael addition reaction of chalcone with benzotriazole. As can be seen from a serial of reaction conditions, the ratio of PW and MCM-41 plays a critical role in the reaction, and the best catalyzed result was achieved when using 50 wt% PW/MCM-41, and the yield was up to 98%. All the products were confirmed by NMR techniques. Moreover, the catalyst was also found to exhibit better recyclability.
介孔分子筛MCM-41固载磷钨酸催化苯并三氮唑与查尔酮的氮杂迈克加成反应研究 Aza-Michael Addition of Chalcone with Benzotriazole Catalyzed by MCM-41 Immobilized H3PW12O40
以介孔分子筛MCM-41固载磷钨酸为催化剂,对苯并三氮唑与查尔酮进行了氮杂迈克加成的催化研究。经过条件筛选,发现MCM-41中的磷钨酸负载量对该反应体系有很大的影响,其中50 wt%的磷钨酸负载量更有利于反应的进行,产率可达98%。通过NMR对产物结构进行了表征,并且催化剂具有一定的回收再利用效果。 In this paper, mesoporous siliceous material MCM-41 supported H3PW12O40 (PW) could act as an efficient catalyst for the aza-Michael addition reaction of chalcone with benzotriazole. As can be seen from a serial of reaction conditions, the ratio of PW and MCM-41 plays a critical role in the reaction, and the best catalyzed result was achieved when using 50 wt% PW/MCM-41, and the yield was up to 98%. All the products were confirmed by NMR techniques. Moreover, the catalyst was also found to exhibit better recyclability.