{"title":"Pt/K 2 La 2 Ti 3 O 10 催化剂的合成及其光催化分解甲醇水溶液制氢","authors":"崔文权, 刘利, 冯良荣, 徐成华, 李子健, 吕绍洁, 邱发礼","doi":"10.1360/032005-93","DOIUrl":null,"url":null,"abstract":"用高温固相法合成了具有类钙钛矿型结构的层状化合物K 2 La 2 Ti 3 O 10 , 用XRD, UV-DRS对其进行表征. 利用不同还原方法制备了Pt/K 2 La 2 Ti 3 O 10 光催化剂, 并且用脉冲氢氧滴定法(HOT)测定了K 2 La 2 Ti 3 O 10 表面Pt的分散度. 考察了Pt/K 2 La 2 Ti 3 O 10 光催化分解甲醇水溶液制氢的活性. 比较了负载Pt与负载Ni和纯的K 2 La 2 Ti 3 O 10 的光催化活性. 研究了Pt负载量、不同还原方法对光催化分解水制氢反应活性的影响. 在最佳的Pt负载量2%(质量百分比)下, 产氢速率达到233.88 mmol·h −1 . 讨论了该催化剂的能带结构及反应机理.","PeriodicalId":49128,"journal":{"name":"Science in China. Series B, Chemistry","volume":"51 1","pages":"139-144"},"PeriodicalIF":0.0000,"publicationDate":"2006-04-20","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Science in China. Series B, Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1360/032005-93","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
用高温固相法合成了具有类钙钛矿型结构的层状化合物K 2 La 2 Ti 3 O 10 , 用XRD, UV-DRS对其进行表征. 利用不同还原方法制备了Pt/K 2 La 2 Ti 3 O 10 光催化剂, 并且用脉冲氢氧滴定法(HOT)测定了K 2 La 2 Ti 3 O 10 表面Pt的分散度. 考察了Pt/K 2 La 2 Ti 3 O 10 光催化分解甲醇水溶液制氢的活性. 比较了负载Pt与负载Ni和纯的K 2 La 2 Ti 3 O 10 的光催化活性. 研究了Pt负载量、不同还原方法对光催化分解水制氢反应活性的影响. 在最佳的Pt负载量2%(质量百分比)下, 产氢速率达到233.88 mmol·h −1 . 讨论了该催化剂的能带结构及反应机理.
用高温固相法合成了具有类钙钛矿型结构的层状化合物K 2 La 2 Ti 3 O 10 , 用XRD, UV-DRS对其进行表征. 利用不同还原方法制备了Pt/K 2 La 2 Ti 3 O 10 光催化剂, 并且用脉冲氢氧滴定法(HOT)测定了K 2 La 2 Ti 3 O 10 表面Pt的分散度. 考察了Pt/K 2 La 2 Ti 3 O 10 光催化分解甲醇水溶液制氢的活性. 比较了负载Pt与负载Ni和纯的K 2 La 2 Ti 3 O 10 的光催化活性. 研究了Pt负载量、不同还原方法对光催化分解水制氢反应活性的影响. 在最佳的Pt负载量2%(质量百分比)下, 产氢速率达到233.88 mmol·h −1 . 讨论了该催化剂的能带结构及反应机理.