M. Esteves-Oliveira, P. Jansen, M. Wehner, A. Dohrn, M. BeLLO-siLva, C. P. Eduardo, H. Meyer-Lueckel
{"title":"Surface Characterization and Short-term Adhesion to Zirconia after Ultra-short Pulsed Laser Irradiation.","authors":"M. Esteves-Oliveira, P. Jansen, M. Wehner, A. Dohrn, M. BeLLO-siLva, C. P. Eduardo, H. Meyer-Lueckel","doi":"10.3290/j.jad.a36918","DOIUrl":null,"url":null,"abstract":"PURPOSE To evaluate the suitability of an ultra-short pulsed laser (USPL) to treat zirconia ceramic surfaces and increase their adhesion to dual-curing resin cement. MATERIALS AND METHODS Twenty 10 × 10 × 5 mm³ blocks were prepared from a zirconia ceramic (Y-TZP). The specimens were polished and randomly assigned to four groups (n = 5) which received the following surface treatments: sandblasting (SB) with Al₂O₃ particles and silica coating (SC) with SiO₂ particles as positive controls; two groups received USPL irradiation, one with 10 scan repetitions (L10) and the other with 20 (L20). Laser irradiation was performed at 1030 nm, 2.3 J/cm², 6 ps pulse duration. The ceramic blocks were duplicated in composite resin and cemented with a dual-curing resin cement. Half of the blocks were then stored in water (37°C) for 24 h and the other half for 1 month. At each time, 40 to 60 sticks per group were subjected to microtensile bond strength testing. Data were analyzed statistically using the Kruskal-Wallis test (α = 0.05). RESULTS Laser-treated zirconia presented statistically significantly higher roughness than did SB and SC. After 24 h, the highest bond strength means (MPa) were achieved by L10 (42.3 ± 10.8) and L20 (37.9 ± 14.4), and both of them were statistically significantly higher than SB (22.0 ± 5.3) and SC (20.8 ± 7.1) (p < 0.05). After 1 month of storage, L10- and L20-treated zirconia still showed significantly higher bond strengths than did SB- and SC-treated zirconia (p < 0.05). CONCLUSION USPL irradiation significantly increases bond strength of zirconia ceramic to dual-curing resin cement and might be an alternative for improving adhesion to this material.","PeriodicalId":94234,"journal":{"name":"The journal of adhesive dentistry","volume":"24 1","pages":"483-492"},"PeriodicalIF":0.0000,"publicationDate":"2016-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"16","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"The journal of adhesive dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3290/j.jad.a36918","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 16
Abstract
PURPOSE To evaluate the suitability of an ultra-short pulsed laser (USPL) to treat zirconia ceramic surfaces and increase their adhesion to dual-curing resin cement. MATERIALS AND METHODS Twenty 10 × 10 × 5 mm³ blocks were prepared from a zirconia ceramic (Y-TZP). The specimens were polished and randomly assigned to four groups (n = 5) which received the following surface treatments: sandblasting (SB) with Al₂O₃ particles and silica coating (SC) with SiO₂ particles as positive controls; two groups received USPL irradiation, one with 10 scan repetitions (L10) and the other with 20 (L20). Laser irradiation was performed at 1030 nm, 2.3 J/cm², 6 ps pulse duration. The ceramic blocks were duplicated in composite resin and cemented with a dual-curing resin cement. Half of the blocks were then stored in water (37°C) for 24 h and the other half for 1 month. At each time, 40 to 60 sticks per group were subjected to microtensile bond strength testing. Data were analyzed statistically using the Kruskal-Wallis test (α = 0.05). RESULTS Laser-treated zirconia presented statistically significantly higher roughness than did SB and SC. After 24 h, the highest bond strength means (MPa) were achieved by L10 (42.3 ± 10.8) and L20 (37.9 ± 14.4), and both of them were statistically significantly higher than SB (22.0 ± 5.3) and SC (20.8 ± 7.1) (p < 0.05). After 1 month of storage, L10- and L20-treated zirconia still showed significantly higher bond strengths than did SB- and SC-treated zirconia (p < 0.05). CONCLUSION USPL irradiation significantly increases bond strength of zirconia ceramic to dual-curing resin cement and might be an alternative for improving adhesion to this material.