Deformation modes and fracture behaviors of peak-aged Mg-Gd-Y alloys with different grain structures

IF 15.8 1区 材料科学 Q1 METALLURGY & METALLURGICAL ENGINEERING
Jiangli Ning , Jialiao Zhou , Bosong Gao , Chunlei Zhang , Hailong Shi , Liansheng Chen , Xiaojun Wang
{"title":"Deformation modes and fracture behaviors of peak-aged Mg-Gd-Y alloys with different grain structures","authors":"Jiangli Ning ,&nbsp;Jialiao Zhou ,&nbsp;Bosong Gao ,&nbsp;Chunlei Zhang ,&nbsp;Hailong Shi ,&nbsp;Liansheng Chen ,&nbsp;Xiaojun Wang","doi":"10.1016/j.jma.2023.09.020","DOIUrl":null,"url":null,"abstract":"<div><div>The ductility and toughness of peak-aged (PA) Mg-RE alloys are significantly influenced by their grain structure characteristics. To investigate this issue, we examined PA Mg-8.24Gd-2.68Y (wt.%) alloys with two distinct grain structures: an extruded-PA sample with dynamic recrystallized (DRXed) fine grains and coarse hot-worked grains, and an extrusion-solution treated and PA sample with grown large equiaxed grains. The results showed that the extruded-PA sample demonstrated a favorable combination of tensile strength (426 MPa) and ductility (7.0 %). Although intergranular microcracks nucleated in the DRXed region due to strain incompatibility, crack propagation was impeded by the DRXed fine grains, inducing intrinsic and extrinsic toughening mechanisms. On the other hand, the hot-worked grains in the extruded-PA sample initiated transgranular cracks after a relatively high strain, attributed to the strain partitioning effect, ultimately leading to failure. In comparison, the solution-treated-PA sample exhibited lower tensile strength and ductility (338 MPa and 3.7 %, respectively). Intergranular cracks nucleated in the CG sample before necking, and the readily formed critical crack, facilitated by the large grain size, exhibited unstable crack growth, resulting in premature failure. This work offers valuable insights for designing high-performance PA Mg-RE alloys and preventing premature failure in practical applications.</div></div>","PeriodicalId":16214,"journal":{"name":"Journal of Magnesium and Alloys","volume":"12 10","pages":"Pages 4140-4156"},"PeriodicalIF":15.8000,"publicationDate":"2024-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Magnesium and Alloys","FirstCategoryId":"88","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2213956723002086","RegionNum":1,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"METALLURGY & METALLURGICAL ENGINEERING","Score":null,"Total":0}
引用次数: 0

Abstract

The ductility and toughness of peak-aged (PA) Mg-RE alloys are significantly influenced by their grain structure characteristics. To investigate this issue, we examined PA Mg-8.24Gd-2.68Y (wt.%) alloys with two distinct grain structures: an extruded-PA sample with dynamic recrystallized (DRXed) fine grains and coarse hot-worked grains, and an extrusion-solution treated and PA sample with grown large equiaxed grains. The results showed that the extruded-PA sample demonstrated a favorable combination of tensile strength (426 MPa) and ductility (7.0 %). Although intergranular microcracks nucleated in the DRXed region due to strain incompatibility, crack propagation was impeded by the DRXed fine grains, inducing intrinsic and extrinsic toughening mechanisms. On the other hand, the hot-worked grains in the extruded-PA sample initiated transgranular cracks after a relatively high strain, attributed to the strain partitioning effect, ultimately leading to failure. In comparison, the solution-treated-PA sample exhibited lower tensile strength and ductility (338 MPa and 3.7 %, respectively). Intergranular cracks nucleated in the CG sample before necking, and the readily formed critical crack, facilitated by the large grain size, exhibited unstable crack growth, resulting in premature failure. This work offers valuable insights for designing high-performance PA Mg-RE alloys and preventing premature failure in practical applications.
具有不同晶粒结构的峰值时效 Mg-Gd-Y 合金的变形模式和断裂行为
峰值时效 (PA) Mg-RE 合金的延展性和韧性受到其晶粒结构特征的显著影响。为了研究这个问题,我们研究了具有两种不同晶粒结构的 PA Mg-8.24Gd-2.68Y(重量百分比)合金:一种是具有动态再结晶(DRX)细晶粒和粗热加工晶粒的挤压-PA 样品,另一种是经过挤压-溶液处理并具有长大等轴晶粒的 PA 样品。结果表明,挤压-PA 样品具有良好的抗拉强度(426 兆帕)和延展性(7.0%)。虽然由于应变不相容性导致晶间微裂纹在 DRX 化区域成核,但 DRX 化细粒阻碍了裂纹的扩展,从而诱发了内在和外在增韧机制。另一方面,由于应变分配效应,挤压-PA 样品中的热加工晶粒在相对较高的应变后产生跨晶格裂纹,最终导致破坏。相比之下,经过溶液处理的聚苯乙烯样品的抗拉强度和延展性较低(分别为 338 兆帕和 3.7%)。CG 样品中的晶间裂纹在缩颈之前就已成核,而由于晶粒尺寸较大,容易形成的临界裂纹表现出不稳定的裂纹生长,导致过早失效。这项研究为设计高性能 PA Mg-RE 合金以及在实际应用中防止过早失效提供了宝贵的见解。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Journal of Magnesium and Alloys
Journal of Magnesium and Alloys Engineering-Mechanics of Materials
CiteScore
20.20
自引率
14.80%
发文量
52
审稿时长
59 days
期刊介绍: The Journal of Magnesium and Alloys serves as a global platform for both theoretical and experimental studies in magnesium science and engineering. It welcomes submissions investigating various scientific and engineering factors impacting the metallurgy, processing, microstructure, properties, and applications of magnesium and alloys. The journal covers all aspects of magnesium and alloy research, including raw materials, alloy casting, extrusion and deformation, corrosion and surface treatment, joining and machining, simulation and modeling, microstructure evolution and mechanical properties, new alloy development, magnesium-based composites, bio-materials and energy materials, applications, and recycling.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信