Long-Term Hygroscopic Thickness Swelling Rate of Hydrothermally Treated Beech Wood / Polypropylene Composites

IF 0.7 4区 农林科学 Q4 MATERIALS SCIENCE, PAPER & WOOD
S. K. Hosseinihashemi, Farhad Arwi̇nfar, A. Najafi, F. Özdemir, N. Ayrilmiş, A. Tamjidi
{"title":"Long-Term Hygroscopic Thickness Swelling Rate of Hydrothermally Treated Beech Wood / Polypropylene Composites","authors":"S. K. Hosseinihashemi, Farhad Arwi̇nfar, A. Najafi, F. Özdemir, N. Ayrilmiş, A. Tamjidi","doi":"10.5552/drvind.2022.2104","DOIUrl":null,"url":null,"abstract":"Long-term hygroscopic thickness swelling rate of polypropylene (PP) composites filled with thermally treated wood flour was investigated. The beech wood chips were heat treated at 120 °C, 150 °C or 180 °C for 30 or 120 min using saturated steam in a digester. The composites based on PP, beech wood flour (BF), and coupling agents (PP-g-MA) were made by melt compounding and injection molding. The weight ratio of BF to PP was controlled at 50/47 for all blends. The amount of coupling agent was fixed at 3 wt.% for all formulations. Further study was conducted to model thickness swelling of the composites, a swelling rate parameter (KSR). The thickness swelling of thermally-treated samples at 120 ºC for 30 min and at 150 ºC for 30 min were lower than that of control samples, followed by thermally-treated samples at 180 ºC for 120 min, at 180 ºC for 30 min, at 120 ºC for 120 min, and at 150 ºC for 120 min, respectively. Furthermore, the thickness swelling of the BF/PP composites decreased with increasing time and temperature of the thermal-treatment. In addition, at 120 ºC for 30 min, the composites showed a lower swelling rate than control samples. The KSR of the composites was influenced both by the time and temperature of thermal treatment.","PeriodicalId":11427,"journal":{"name":"Drvna Industrija","volume":" ","pages":""},"PeriodicalIF":0.7000,"publicationDate":"2022-03-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Drvna Industrija","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.5552/drvind.2022.2104","RegionNum":4,"RegionCategory":"农林科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q4","JCRName":"MATERIALS SCIENCE, PAPER & WOOD","Score":null,"Total":0}
引用次数: 1

Abstract

Long-term hygroscopic thickness swelling rate of polypropylene (PP) composites filled with thermally treated wood flour was investigated. The beech wood chips were heat treated at 120 °C, 150 °C or 180 °C for 30 or 120 min using saturated steam in a digester. The composites based on PP, beech wood flour (BF), and coupling agents (PP-g-MA) were made by melt compounding and injection molding. The weight ratio of BF to PP was controlled at 50/47 for all blends. The amount of coupling agent was fixed at 3 wt.% for all formulations. Further study was conducted to model thickness swelling of the composites, a swelling rate parameter (KSR). The thickness swelling of thermally-treated samples at 120 ºC for 30 min and at 150 ºC for 30 min were lower than that of control samples, followed by thermally-treated samples at 180 ºC for 120 min, at 180 ºC for 30 min, at 120 ºC for 120 min, and at 150 ºC for 120 min, respectively. Furthermore, the thickness swelling of the BF/PP composites decreased with increasing time and temperature of the thermal-treatment. In addition, at 120 ºC for 30 min, the composites showed a lower swelling rate than control samples. The KSR of the composites was influenced both by the time and temperature of thermal treatment.
水热处理榉木/聚丙烯复合材料的长期吸湿厚度膨胀率
研究了热处理木粉填充聚丙烯(PP)复合材料的长期吸湿厚度膨胀率。山毛榉木屑在120°C, 150°C或180°C下加热30或120分钟,在蒸煮器中使用饱和蒸汽。以聚丙烯(PP)、山毛榉粉(BF)和偶联剂(PP-g- ma)为基材,通过熔融复合和注塑成型制备了复合材料。所有共混物的BF / PP重量比控制在50/47。所有配方的偶联剂用量均固定在3 wt.%。进一步研究了复合材料的厚度膨胀模型,即膨胀率参数(KSR)。热处理样品在120℃下30 min、150℃下30 min的厚度膨胀小于对照样品,其次是180℃下120 min、180℃下30 min、120℃下120 min、150℃下120 min的厚度膨胀。随着热处理时间和温度的增加,BF/PP复合材料的厚度膨胀减小。此外,在120℃下保温30 min,复合材料的膨胀率低于对照样品。复合材料的KSR受热处理时间和温度的影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Drvna Industrija
Drvna Industrija MATERIALS SCIENCE, PAPER & WOOD-
CiteScore
1.80
自引率
9.10%
发文量
32
审稿时长
>12 weeks
期刊介绍: "Drvna industrija" ("Wood Industry") journal publishes original scientific and review papers, short notes, professional papers, conference papers, reports, professional information, bibliographical and survey articles and general notes relating to the forestry exploitation, biology, chemistry, physics and technology of wood, pulp and paper and wood components, including production, management and marketing aspects in the woodworking industry.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信