{"title":"Energy modeling and process mapping for defect-free hot-wire laser deposition of Inconel 718 single beads","authors":"Barkin Aydin,&nbsp;Christophe Tournier","doi":"10.1016/j.addlet.2026.100401","DOIUrl":null,"url":null,"abstract":"<div><div>Hot-wire laser additive manufacturing (DED-LHW) addresses key limitations of conventional cold-wire processes, where excessive laser energy overheats the melt pool and promotes columnar grain growth, degrading microstructural properties. In addition, a large fraction of the laser power is lost by reflection at the metallic surface, resulting in low overall energy efficiency. DED-LHW introduces electrical current for resistive wire preheating via the Joule effect, complementing laser energy to reduce required laser power and enhance deposition stability. This study develops a critical energy delivery model that quantifies the linear thermal energy supplied to the wire by both laser in a three-beam coaxial configuration and Joule heating. The model precisely predicts and prevents dripping and stubbing defects, as validated experimentally through comprehensive process mapping for Inconel 718. The effects of laser power, current, scanning speed, and wire feeding speed on bead morphology and dilution are extensively investigated. Results confirm that the laser must provide at least half of the total wire energy for optimal stability, with Joule heating as a complementary source. DED-LHW achieves twice the deposition rate at 50% laser power compared to cold-wire deposition, producing smoother beads, more refined contact angle control, and a finer microstructure. This directly reduces energy consumption and production time while eliminating defects.</div></div>","PeriodicalId":72068,"journal":{"name":"Additive manufacturing letters","volume":"18 ","pages":"Article 100401"},"PeriodicalIF":5.2000,"publicationDate":"2026-07-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Additive manufacturing letters","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2772369026000496","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2026/6/30 0:00:00","PubModel":"Epub","JCR":"Q2","JCRName":"ENGINEERING, MANUFACTURING","Score":null,"Total":0}
引用次数: 0

Abstract

Hot-wire laser additive manufacturing (DED-LHW) addresses key limitations of conventional cold-wire processes, where excessive laser energy overheats the melt pool and promotes columnar grain growth, degrading microstructural properties. In addition, a large fraction of the laser power is lost by reflection at the metallic surface, resulting in low overall energy efficiency. DED-LHW introduces electrical current for resistive wire preheating via the Joule effect, complementing laser energy to reduce required laser power and enhance deposition stability. This study develops a critical energy delivery model that quantifies the linear thermal energy supplied to the wire by both laser in a three-beam coaxial configuration and Joule heating. The model precisely predicts and prevents dripping and stubbing defects, as validated experimentally through comprehensive process mapping for Inconel 718. The effects of laser power, current, scanning speed, and wire feeding speed on bead morphology and dilution are extensively investigated. Results confirm that the laser must provide at least half of the total wire energy for optimal stability, with Joule heating as a complementary source. DED-LHW achieves twice the deposition rate at 50% laser power compared to cold-wire deposition, producing smoother beads, more refined contact angle control, and a finer microstructure. This directly reduces energy consumption and production time while eliminating defects.
无缺陷热线激光沉积Inconel 718单珠的能量建模和工艺映射
热丝激光增材制造(ed - lhw)解决了传统冷丝工艺的主要局限性,在冷丝工艺中,过多的激光能量使熔池过热,促进柱状晶粒生长,降低微观结构性能。此外,激光功率的很大一部分由于金属表面的反射而损失,导致整体能量效率较低。d - lhw通过焦耳效应为电阻丝预热引入电流,补充激光能量,降低所需激光功率,提高沉积稳定性。本研究开发了一个临界能量传递模型,该模型量化了三束同轴结构激光和焦耳加热提供给导线的线性热能。通过对Inconel 718的综合工艺图进行实验验证,该模型可以精确预测和防止滴漏和存根缺陷。研究了激光功率、电流、扫描速度和送丝速度对熔珠形貌和稀释度的影响。结果证实,激光必须提供至少一半的总导线能量,以获得最佳的稳定性,焦耳加热作为补充源。与冷丝沉积相比,在50%的激光功率下,DED-LHW的沉积速率是冷丝沉积的两倍,可以产生更光滑的珠粒,更精细的接触角控制和更精细的微观结构。这直接降低了能耗和生产时间,同时消除了缺陷。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Additive manufacturing letters
Additive manufacturing letters Materials Science (General), Industrial and Manufacturing Engineering, Mechanics of Materials
CiteScore
3.70
自引率
0.00%
发文量
0
审稿时长
37 days
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信
小红书