Bonding to Demineralized Dentin: Impact of Immediate and Delayed Dentin Sealing over Time.

IF 3.1 Q2 DENTISTRY, ORAL SURGERY & MEDICINE
Erika Pérez-Soto, Rim Bourgi, Louis Hardan, Carlos Enrique Cuevas-Suarez, Ana Josefina Monjáras-Ávila, Miguel Ángel Fernández-Barrera, Nicolas Nassar, Monika Lukomska-Szymanska, Rima Daoui, Naji Kharouf, Youssef Haikel
{"title":"Bonding to Demineralized Dentin: Impact of Immediate and Delayed Dentin Sealing over Time.","authors":"Erika Pérez-Soto, Rim Bourgi, Louis Hardan, Carlos Enrique Cuevas-Suarez, Ana Josefina Monjáras-Ávila, Miguel Ángel Fernández-Barrera, Nicolas Nassar, Monika Lukomska-Szymanska, Rima Daoui, Naji Kharouf, Youssef Haikel","doi":"10.3390/dj13080354","DOIUrl":null,"url":null,"abstract":"<p><p><b>Background/Objectives:</b> Immediate dentin sealing (IDS) has been widely investigated in sound dentin; however, its efficacy on demineralized dentin remains insufficiently explored. This in vitro experimental study aimed to evaluate the shear bond strength (SBS) of indirect composite resin restorations bonded to demineralized dentin using IDS, assessed at 24 h and after 6 months of aging. <b>Methods:</b> Twenty-five extracted premolars were randomly divided into five groups: (1) control (no sealing), (2) IDS applied to sound dentin (sound-IDS), (3) IDS applied to demineralized dentin (carious-IDS), (4) delayed dentin sealing (DDS) on sound dentin (sound-DDS), and (5) DDS on demineralized dentin (carious-DDS). SBS values were analyzed using a three-way analysis of variance (ANOVA) with dentin condition (sound vs. demineralized), aging time (24 h vs. 6 months), and sealing strategy (control, IDS, DDS) as independent variables. Statistical analyses were performed using SigmaPlot 12.0, with significance set at <i>p</i> < 0.05. <b>Results:</b> The results showed that IDS led to significantly higher SBS than DDS (<i>p</i> < 0.05). Bond strength was significantly influenced by dentin condition (<i>p</i> < 0.05), and all interactions between variables-particularly between dentin condition and sealing strategy, and between aging time and treatment-were statistically significant (<i>p</i> < 0.001). Overall, bond strength was higher at 24 h than after 6 months. IDS showed optimal performance in sound dentin, while DDS resulted in better long-term outcomes in demineralized dentin. <b>Conclusions:</b> These findings suggest that DDS may be the more effective approach in cases of carious or demineralized dentin.</p>","PeriodicalId":11269,"journal":{"name":"Dentistry Journal","volume":"13 8","pages":""},"PeriodicalIF":3.1000,"publicationDate":"2025-08-05","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC12385143/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Dentistry Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.3390/dj13080354","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0

Abstract

Background/Objectives: Immediate dentin sealing (IDS) has been widely investigated in sound dentin; however, its efficacy on demineralized dentin remains insufficiently explored. This in vitro experimental study aimed to evaluate the shear bond strength (SBS) of indirect composite resin restorations bonded to demineralized dentin using IDS, assessed at 24 h and after 6 months of aging. Methods: Twenty-five extracted premolars were randomly divided into five groups: (1) control (no sealing), (2) IDS applied to sound dentin (sound-IDS), (3) IDS applied to demineralized dentin (carious-IDS), (4) delayed dentin sealing (DDS) on sound dentin (sound-DDS), and (5) DDS on demineralized dentin (carious-DDS). SBS values were analyzed using a three-way analysis of variance (ANOVA) with dentin condition (sound vs. demineralized), aging time (24 h vs. 6 months), and sealing strategy (control, IDS, DDS) as independent variables. Statistical analyses were performed using SigmaPlot 12.0, with significance set at p < 0.05. Results: The results showed that IDS led to significantly higher SBS than DDS (p < 0.05). Bond strength was significantly influenced by dentin condition (p < 0.05), and all interactions between variables-particularly between dentin condition and sealing strategy, and between aging time and treatment-were statistically significant (p < 0.001). Overall, bond strength was higher at 24 h than after 6 months. IDS showed optimal performance in sound dentin, while DDS resulted in better long-term outcomes in demineralized dentin. Conclusions: These findings suggest that DDS may be the more effective approach in cases of carious or demineralized dentin.

Abstract Image

Abstract Image

Abstract Image

与脱矿牙本质的结合:即刻和延迟牙本质封闭随时间的影响。
背景/目的:即刻牙本质密封(IDS)在健全牙本质中得到了广泛的研究;然而,其对脱矿牙本质的作用尚未得到充分的探讨。本体外实验研究旨在利用IDS评估间接复合树脂修复体与脱矿牙本质的剪切结合强度(SBS),分别在老化24 h和6个月后进行评估。方法:将取出的25颗前磨牙随机分为5组:(1)对照组(不封闭),(2)牙本质封闭(sound-IDS),(3)牙本质脱矿封闭(龋齿-IDS),(4)牙本质封闭(sound-DDS)延迟牙本质封闭(DDS),(5)牙本质脱矿封闭(龋齿-DDS)。SBS值采用三向方差分析(ANOVA),以牙本质状态(健全vs脱矿)、老化时间(24小时vs 6个月)和密封策略(对照、IDS、DDS)为自变量。采用SigmaPlot 12.0进行统计学分析,p < 0.05为显著性。结果:IDS导致SBS显著高于DDS (p < 0.05)。牙本质状态显著影响牙本质粘结强度(p < 0.05),所有变量之间的相互作用,特别是牙本质状态和密封策略之间,以及老化时间和处理之间的相互作用,均具有统计学意义(p < 0.001)。总体而言,24 h时的粘结强度高于6个月后。IDS在健康牙本质中表现最佳,而DDS在脱矿牙本质中表现更好。结论:这些结果提示DDS可能是治疗牙本质龋齿或脱矿的更有效方法。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Dentistry Journal
Dentistry Journal Dentistry-Dentistry (all)
CiteScore
3.70
自引率
7.70%
发文量
213
审稿时长
11 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信