{"title":"Optimizing carbon sequestration and performance of concrete masonry blocks containing alkaline industrial waste","authors":"Jad Bawab ,&nbsp;Hilal El-Hassan ,&nbsp;Amr El-Dieb ,&nbsp;Jamal Khatib","doi":"10.1016/j.clet.2025.100943","DOIUrl":null,"url":null,"abstract":"<div><div>This study aims to optimize the carbon sequestration, compressive strength, and water transport properties (i.e., water absorption and volume of permeable voids) of concrete masonry blocks incorporating calcium carbide residue (CCR) as a partial cement replacement. The Taguchi design of experiments was utilized to study the influence of CCR replacement percentage, initial air curing duration, carbonation duration, and CO<sub>2</sub> gas pressure on the performance responses. These response criteria include CO<sub>2</sub> uptake, carbonation depth, compressive strength, water absorption, and volume of permeable voids. The concrete mixture proportions were then optimized for superior performance. The results highlight that a CCR replacement level of 10 % was required for optimum carbon sequestration potential, while only 5 % was optimum for superior strength and water transport properties. To maximize each performance criterion, the carbonation process parameters comprised an initial air curing duration of 20 h, a carbonation curing duration of 20 h, and a CO<sub>2</sub> pressure of 5 bars. Analysis of variance showed that the initial air curing duration was the most contributing factor to the CO<sub>2</sub> sequestration potential. In contrast, the CCR content was decisive for strength and water transport properties. Microstructural analysis unveiled that calcite formed abundantly in optimum mixes with the consumption of calcium hydroxide. Compared to a hydrated counterpart, using the optimum mix containing 10 % CCR in concrete masonry applications would emit a 31 % lower carbon footprint, sequester 50 million tons of CO<sub>2</sub>, consume 10 % less cement, and valorize up to 23 million tons of CCR industrial waste.</div></div>","PeriodicalId":34618,"journal":{"name":"Cleaner Engineering and Technology","volume":"26 ","pages":"Article 100943"},"PeriodicalIF":5.3000,"publicationDate":"2025-03-21","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Cleaner Engineering and Technology","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2666790825000667","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"ENGINEERING, ENVIRONMENTAL","Score":null,"Total":0}
引用次数: 0

Abstract

This study aims to optimize the carbon sequestration, compressive strength, and water transport properties (i.e., water absorption and volume of permeable voids) of concrete masonry blocks incorporating calcium carbide residue (CCR) as a partial cement replacement. The Taguchi design of experiments was utilized to study the influence of CCR replacement percentage, initial air curing duration, carbonation duration, and CO2 gas pressure on the performance responses. These response criteria include CO2 uptake, carbonation depth, compressive strength, water absorption, and volume of permeable voids. The concrete mixture proportions were then optimized for superior performance. The results highlight that a CCR replacement level of 10 % was required for optimum carbon sequestration potential, while only 5 % was optimum for superior strength and water transport properties. To maximize each performance criterion, the carbonation process parameters comprised an initial air curing duration of 20 h, a carbonation curing duration of 20 h, and a CO2 pressure of 5 bars. Analysis of variance showed that the initial air curing duration was the most contributing factor to the CO2 sequestration potential. In contrast, the CCR content was decisive for strength and water transport properties. Microstructural analysis unveiled that calcite formed abundantly in optimum mixes with the consumption of calcium hydroxide. Compared to a hydrated counterpart, using the optimum mix containing 10 % CCR in concrete masonry applications would emit a 31 % lower carbon footprint, sequester 50 million tons of CO2, consume 10 % less cement, and valorize up to 23 million tons of CCR industrial waste.
求助全文
约1分钟内获得全文 求助全文
来源期刊
Cleaner Engineering and Technology
Cleaner Engineering and Technology Engineering-Engineering (miscellaneous)
CiteScore
9.80
自引率
0.00%
发文量
218
审稿时长
21 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信