{"title":"The effect of bleaching agent on the compressive strength of orthodontic thermoplastic retainer materials.","authors":"Ailin Ehteshami, Saina Omidi, Maede Ghasemi","doi":"10.4103/drj.drj_216_24","DOIUrl":null,"url":null,"abstract":"<p><strong>Background: </strong>There is an increasing desire for teeth bleching after orthodontic treatment. Therefor, this study aims to evaluate the effect of carbamide peroxide 15% and thermocycling on the compressive strength of polyethylene terephthalate glycol (PETG) thermoplastic retainer material.</p><p><strong>Materials and methods: </strong>In this <i>in vitro</i> study, forty samples of PETG material were thermoformed over a plastic template (10 mm × 8 mm × 2 mm). The samples were divided into four groups, with ten samples in each group. Group I served as the control, Group II was exposed to carbamide peroxide 15% (5 h daily for 14 days), Group III underwent thermocycling (5000 times), and Group IV underwent thermocycling (5000 times) followed by exposure to carbamide peroxide 15% (5 h daily for 14 days). The compressive strength of the groups was then evaluated using one-way ANOVA and Tukey's HSD tests for statistical analysis. The significance level was set to 0.05.</p><p><strong>Results: </strong>The analysis showed a significant difference among the four groups. The compressive strength of all groups significantly decreased compared to the control group. Group II exhibited a significant decrease compared to Group III (<i>P</i> = 0.003). However, there was no significant difference between Group II and Group IV (<i>P</i> = 0.191). In addition, there was no significant difference observed between Group III and Group IV (<i>P</i> = 0.308). Group II had the lowest compressive strength (163.9 Mpa).</p><p><strong>Conclusion: </strong>It is not recommended to use a thermoplastic retainer as a bleaching tray during the initial phase of retention. However, since there were no further harmful effects of bleaching agents observed after thermocycling, it is possible to recommend the use of a thermoplastic retainer as a bleaching tray toward the end of the retention phase.</p>","PeriodicalId":11016,"journal":{"name":"Dental Research Journal","volume":"22 ","pages":"2"},"PeriodicalIF":0.0000,"publicationDate":"2025-01-24","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC11870327/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Dental Research Journal","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4103/drj.drj_216_24","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"2025/1/1 0:00:00","PubModel":"eCollection","JCR":"Q2","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 0
Abstract
Background: There is an increasing desire for teeth bleching after orthodontic treatment. Therefor, this study aims to evaluate the effect of carbamide peroxide 15% and thermocycling on the compressive strength of polyethylene terephthalate glycol (PETG) thermoplastic retainer material.
Materials and methods: In this in vitro study, forty samples of PETG material were thermoformed over a plastic template (10 mm × 8 mm × 2 mm). The samples were divided into four groups, with ten samples in each group. Group I served as the control, Group II was exposed to carbamide peroxide 15% (5 h daily for 14 days), Group III underwent thermocycling (5000 times), and Group IV underwent thermocycling (5000 times) followed by exposure to carbamide peroxide 15% (5 h daily for 14 days). The compressive strength of the groups was then evaluated using one-way ANOVA and Tukey's HSD tests for statistical analysis. The significance level was set to 0.05.
Results: The analysis showed a significant difference among the four groups. The compressive strength of all groups significantly decreased compared to the control group. Group II exhibited a significant decrease compared to Group III (P = 0.003). However, there was no significant difference between Group II and Group IV (P = 0.191). In addition, there was no significant difference observed between Group III and Group IV (P = 0.308). Group II had the lowest compressive strength (163.9 Mpa).
Conclusion: It is not recommended to use a thermoplastic retainer as a bleaching tray during the initial phase of retention. However, since there were no further harmful effects of bleaching agents observed after thermocycling, it is possible to recommend the use of a thermoplastic retainer as a bleaching tray toward the end of the retention phase.
期刊介绍:
Dental Research Journal, a publication of Isfahan University of Medical Sciences, is a peer-reviewed online journal with Bimonthly print on demand compilation of issues published. The journal’s full text is available online at http://www.drjjournal.net. The journal allows free access (Open Access) to its contents and permits authors to self-archive final accepted version of the articles on any OAI-compliant institutional / subject-based repository. The journal will cover technical and clinical studies related to health, ethical and social issues in field of Dentistry. Articles with clinical interest and implications will be given preference.