{"title":"Exploration of hypereutectoid compositions for achieving and enhancing superelasticity in biomedical Ti–Au–Mo alloys","authors":"Naoki Nohira ,&nbsp;Wan-Ting Chiu ,&nbsp;Akira Umise ,&nbsp;Masaki Tahara ,&nbsp;Hideki Hosoda","doi":"10.1016/j.msea.2025.148095","DOIUrl":null,"url":null,"abstract":"<div><div>β (bcc) Ti–Au based biomedical alloys are attractive due to their excellent biocompatibility, X-ray radiographic imaging properties, and shape memory effects. However, increasing the Au content beyond the eutectoid composition (4.2 mol% Au, β-Ti = α-Ti (hcp) + Ti<sub>3</sub>Au, in the binary system) presents a challenge because the intermetallic compound Ti<sub>3</sub>Au readily forms at hypereutectoid compositions, leading to increased brittleness in the alloys. Thus, the feasibility of hypereutectoid compositions was explored in this work using the Ti–Au–Mo ternary system. The addition of Mo was expected to significantly suppress the eutectoid reaction by enhancing the stability of the β phase. In solution-treated alloys, it was found that Ti–Au–5Mo alloys with up to 6 mol% Au (approximately 20 mass% Au, 5 karat) exhibited good cold workability, achieving a 95 % reduction in thickness. Furthermore, in the Ti–6Au–5Mo alloy, a β single phase was successfully quenched without the formation of Ti<sub>3</sub>Au. The stability of the β phase increased with higher Au content, with the reduction rate in the martensitic transformation temperature of −85 K/mol% Au. Additionally, the Ti–6Au–5Mo alloy exhibited clear superelasticity at room temperature, with a 4.8 % shape recovery strain and a 2.7 % superelastic strain. Besides, the effect of Ti<sub>3</sub>Au precipitation through heat treatment on mechanical properties was also evaluated. These findings provide a solid foundation for the development of functional low-karat Ti–Au alloys for advanced medical devices.</div></div>","PeriodicalId":385,"journal":{"name":"Materials Science and Engineering: A","volume":"928 ","pages":"Article 148095"},"PeriodicalIF":6.1000,"publicationDate":"2025-02-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Materials Science and Engineering: A","FirstCategoryId":"5","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0921509325003132","RegionNum":2,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

β (bcc) Ti–Au based biomedical alloys are attractive due to their excellent biocompatibility, X-ray radiographic imaging properties, and shape memory effects. However, increasing the Au content beyond the eutectoid composition (4.2 mol% Au, β-Ti = α-Ti (hcp) + Ti3Au, in the binary system) presents a challenge because the intermetallic compound Ti3Au readily forms at hypereutectoid compositions, leading to increased brittleness in the alloys. Thus, the feasibility of hypereutectoid compositions was explored in this work using the Ti–Au–Mo ternary system. The addition of Mo was expected to significantly suppress the eutectoid reaction by enhancing the stability of the β phase. In solution-treated alloys, it was found that Ti–Au–5Mo alloys with up to 6 mol% Au (approximately 20 mass% Au, 5 karat) exhibited good cold workability, achieving a 95 % reduction in thickness. Furthermore, in the Ti–6Au–5Mo alloy, a β single phase was successfully quenched without the formation of Ti3Au. The stability of the β phase increased with higher Au content, with the reduction rate in the martensitic transformation temperature of −85 K/mol% Au. Additionally, the Ti–6Au–5Mo alloy exhibited clear superelasticity at room temperature, with a 4.8 % shape recovery strain and a 2.7 % superelastic strain. Besides, the effect of Ti3Au precipitation through heat treatment on mechanical properties was also evaluated. These findings provide a solid foundation for the development of functional low-karat Ti–Au alloys for advanced medical devices.
求助全文
约1分钟内获得全文 求助全文
来源期刊
Materials Science and Engineering: A
Materials Science and Engineering: A 工程技术-材料科学:综合
CiteScore
11.50
自引率
15.60%
发文量
1811
审稿时长
31 days
期刊介绍: Materials Science and Engineering A provides an international medium for the publication of theoretical and experimental studies related to the load-bearing capacity of materials as influenced by their basic properties, processing history, microstructure and operating environment. Appropriate submissions to Materials Science and Engineering A should include scientific and/or engineering factors which affect the microstructure - strength relationships of materials and report the changes to mechanical behavior.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信