{"title":"Manufacturing of Continuous Core–Shell Hydrated Salt Fibers for Room Temperature Thermal Energy Storage","authors":"Michael D. Toomey, Nihal Kanbargi, Logan T. Kearney, Holly Hinton, Sumit Gupta, Reyad Sawafta, Amit K. Naskar, Jaswinder Sharma","doi":"10.1002/adem.202470068","DOIUrl":null,"url":null,"abstract":"<p><b>Room Temperature Thermal Energy Storage</b>\n </p><p>In article number 2400012, Michael D. Toomey, Jaswinder Sharma, and co-workers demonstrate the first example of wet-spun PCM fibers comprised of a polymer sheath and a salt hydrate core for thermal energy storage applications. Fibers produced using this scalable production method achieve enthalpies of melting of ca. 130 J/g, melting onset at 29°C, and supercooling of 4.8°C while retaining 96.5% of its phase change capacity after 1000 cycles.\n\n <figure>\n <div><picture>\n <source></source></picture><p></p>\n </div>\n </figure></p>","PeriodicalId":7275,"journal":{"name":"Advanced Engineering Materials","volume":"26 24","pages":""},"PeriodicalIF":3.4000,"publicationDate":"2024-12-18","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://onlinelibrary.wiley.com/doi/epdf/10.1002/adem.202470068","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Advanced Engineering Materials","FirstCategoryId":"88","ListUrlMain":"https://onlinelibrary.wiley.com/doi/10.1002/adem.202470068","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0
Abstract
Room Temperature Thermal Energy Storage
In article number 2400012, Michael D. Toomey, Jaswinder Sharma, and co-workers demonstrate the first example of wet-spun PCM fibers comprised of a polymer sheath and a salt hydrate core for thermal energy storage applications. Fibers produced using this scalable production method achieve enthalpies of melting of ca. 130 J/g, melting onset at 29°C, and supercooling of 4.8°C while retaining 96.5% of its phase change capacity after 1000 cycles.
期刊介绍:
Advanced Engineering Materials is the membership journal of three leading European Materials Societies
- German Materials Society/DGM,
- French Materials Society/SF2M,
- Swiss Materials Federation/SVMT.