Patricia Llancari-Alonzo, Daniel Alvítez-Temoche, Marysela Ladera-Castañeda, Leonor Castro-Ramirez, Carlos López-Gurreonero, César Cayo-Rojas
{"title":"Fluoride release and flexural strength of four ion-releasing restorative materials: An in vitro comparative study.","authors":"Patricia Llancari-Alonzo, Daniel Alvítez-Temoche, Marysela Ladera-Castañeda, Leonor Castro-Ramirez, Carlos López-Gurreonero, César Cayo-Rojas","doi":"10.4317/jced.61818","DOIUrl":null,"url":null,"abstract":"<p><strong>Background: </strong>This study aimed to determine the fluoride release and flexural strength of four ion-releasing restorative materials.</p><p><strong>Material and methods: </strong>A total of 80 samples of four different materials were prepared in standardized molds: Ketac Universal, Beautifil II, Cention N, and Equia Forte Fil. The fluoride release was quantified at 1, 3, 7, 14, and 28 days post-immersion using an ion-selective electrode. The flexural strength was measured with a universal testing machine after 7 days of immersion in deionized water. A one-factor intergroup ANOVA with Welch's robust variance and Games-Howell's post hoc was employed. To compare related measures, a Friedman test with Bonferroni's adjusted post hoc was employed. The <i>p</i>-value was set at 0.05.</p><p><strong>Results: </strong>At 7 days, significant differences were observed in the flexural strength of the four ion-releasing restorative materials (<i>p</i><0.001). The flexural strength values from highest to lowest were as follows: Cention N (97.10 ± 4.99 MPa), Beautifil (82.77 ± 5.30 MPa), Equia Forte Fil (31.38 ± 7.68 MPa), and Ketac Universal (19.23 ± 2.94 MPa). In addition, at 3 and 7 days, the highest amount of fluoride released was observed for Cention N compared to the other ion-releasing restorative materials (<i>p</i><0.05). Conversely, Beautifil II released the lowest amount of fluoride at 3, 7, 14, and 28 days (<i>p</i><0.05) compared to the other ion-releasing restorative materials.</p><p><strong>Conclusions: </strong>The immersion of all ion-releasing restorative materials in deionized water for seven days resulted in significant differences in flexural strength. Cention N had the highest value, while Ketac Universal had the lowest. All ion-releasing restorative materials released fluoride at all test times, with Ketac Universal releasing the most at 1, 14, and 28 days, and Cention N releasing it at 3 and 7 days. Beautifil II showed the lowest fluoride release at all evaluated times, exhibiting a nearly constant release over time compared to the other materials. <b>Key words:</b>Fluoride release, flexural strength, glass ionomer.</p>","PeriodicalId":15376,"journal":{"name":"Journal of Clinical and Experimental Dentistry","volume":"16 10","pages":"e1207-e1216"},"PeriodicalIF":0.0000,"publicationDate":"2024-10-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.ncbi.nlm.nih.gov/pmc/articles/PMC11559120/pdf/","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Journal of Clinical and Experimental Dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.4317/jced.61818","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 0
Abstract
Background: This study aimed to determine the fluoride release and flexural strength of four ion-releasing restorative materials.
Material and methods: A total of 80 samples of four different materials were prepared in standardized molds: Ketac Universal, Beautifil II, Cention N, and Equia Forte Fil. The fluoride release was quantified at 1, 3, 7, 14, and 28 days post-immersion using an ion-selective electrode. The flexural strength was measured with a universal testing machine after 7 days of immersion in deionized water. A one-factor intergroup ANOVA with Welch's robust variance and Games-Howell's post hoc was employed. To compare related measures, a Friedman test with Bonferroni's adjusted post hoc was employed. The p-value was set at 0.05.
Results: At 7 days, significant differences were observed in the flexural strength of the four ion-releasing restorative materials (p<0.001). The flexural strength values from highest to lowest were as follows: Cention N (97.10 ± 4.99 MPa), Beautifil (82.77 ± 5.30 MPa), Equia Forte Fil (31.38 ± 7.68 MPa), and Ketac Universal (19.23 ± 2.94 MPa). In addition, at 3 and 7 days, the highest amount of fluoride released was observed for Cention N compared to the other ion-releasing restorative materials (p<0.05). Conversely, Beautifil II released the lowest amount of fluoride at 3, 7, 14, and 28 days (p<0.05) compared to the other ion-releasing restorative materials.
Conclusions: The immersion of all ion-releasing restorative materials in deionized water for seven days resulted in significant differences in flexural strength. Cention N had the highest value, while Ketac Universal had the lowest. All ion-releasing restorative materials released fluoride at all test times, with Ketac Universal releasing the most at 1, 14, and 28 days, and Cention N releasing it at 3 and 7 days. Beautifil II showed the lowest fluoride release at all evaluated times, exhibiting a nearly constant release over time compared to the other materials. Key words:Fluoride release, flexural strength, glass ionomer.
期刊介绍:
Indexed in PUBMED, PubMed Central® (PMC) since 2012 and SCOPUSJournal of Clinical and Experimental Dentistry is an Open Access (free access on-line) - http://www.medicinaoral.com/odo/indice.htm. The aim of the Journal of Clinical and Experimental Dentistry is: - Periodontology - Community and Preventive Dentistry - Esthetic Dentistry - Biomaterials and Bioengineering in Dentistry - Operative Dentistry and Endodontics - Prosthetic Dentistry - Orthodontics - Oral Medicine and Pathology - Odontostomatology for the disabled or special patients - Oral Surgery