Effect of Yb Addition on the Microstructure and Mechanical Properties of the Mg–4Sm–3Gd–0.5Zr Alloy

IF 3.3 3区 材料科学 Q2 MATERIALS SCIENCE, MULTIDISCIPLINARY
Nana Zhang, Quanan Li, Xiaoya Chen, Wanwan Mei, Zeyu Zheng, Zheng Wu
{"title":"Effect of Yb Addition on the Microstructure and Mechanical Properties of the Mg–4Sm–3Gd–0.5Zr Alloy","authors":"Nana Zhang,&nbsp;Quanan Li,&nbsp;Xiaoya Chen,&nbsp;Wanwan Mei,&nbsp;Zeyu Zheng,&nbsp;Zheng Wu","doi":"10.1007/s12540-024-01706-9","DOIUrl":null,"url":null,"abstract":"<div><p>The microstructure and mechanical properties of Mg-4Sm-3Gd-<i>x</i>Yb-0.5Zr (<i>x</i> = 0, 1, 2, 3 wt%) alloys under different heat treatment states were systematically investigated, as well as the influence mechanism of the Yb on the mechanical properties. The results show that the addition of Yb can obviously refine the grain size, homogenize the microstructure and improve the strength and plasticity. The addition of Yb changed the lattice constant, reduced the value of <i>c/a</i>, shortened the peak aging time, and accelerated the precipitation of β′ phase. With the increase of the Yb content, the number of β′ phases increases. The spacing between adjacent β′ phases decreases, and the critical shear stress <span>\\(\\Delta {\\tau }_{p}\\)</span> demanded for the basal dislocation to bypass the β′ phase increases. The β′ phase improves the strength of the aged alloy through the Orowan mechanism. And the β′ phase forms a nearly closed triangular prism space along the three directions of [1<span>\\(\\bar{1}\\)</span>00] <sub>Mg</sub>, [01<span>\\(\\bar{1}\\)</span>0] <sub>Mg</sub> and [<span>\\(\\overline{1 }\\)</span>010] <sub>Mg</sub>. During the process of tensile deformation, the basal dislocations are trapped in a closed triangular prism space and it was difficult to escape. The aged Mg–4Sm–3Gd–2Yb–0.5Zr alloy showed the optimal mechanical properties, and its yield strength, ultimate tensile strength and elongation were 198 MPa, 275 MPa and 6.6%.</p><h3>Graphical Abstract</h3><div><figure><div><div><picture><source><img></source></picture></div></div></figure></div></div>","PeriodicalId":703,"journal":{"name":"Metals and Materials International","volume":"30 11","pages":"3094 - 3106"},"PeriodicalIF":3.3000,"publicationDate":"2024-05-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Metals and Materials International","FirstCategoryId":"88","ListUrlMain":"https://link.springer.com/article/10.1007/s12540-024-01706-9","RegionNum":3,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q2","JCRName":"MATERIALS SCIENCE, MULTIDISCIPLINARY","Score":null,"Total":0}
引用次数: 0

Abstract

The microstructure and mechanical properties of Mg-4Sm-3Gd-xYb-0.5Zr (x = 0, 1, 2, 3 wt%) alloys under different heat treatment states were systematically investigated, as well as the influence mechanism of the Yb on the mechanical properties. The results show that the addition of Yb can obviously refine the grain size, homogenize the microstructure and improve the strength and plasticity. The addition of Yb changed the lattice constant, reduced the value of c/a, shortened the peak aging time, and accelerated the precipitation of β′ phase. With the increase of the Yb content, the number of β′ phases increases. The spacing between adjacent β′ phases decreases, and the critical shear stress \(\Delta {\tau }_{p}\) demanded for the basal dislocation to bypass the β′ phase increases. The β′ phase improves the strength of the aged alloy through the Orowan mechanism. And the β′ phase forms a nearly closed triangular prism space along the three directions of [1\(\bar{1}\)00] Mg, [01\(\bar{1}\)0] Mg and [\(\overline{1 }\)010] Mg. During the process of tensile deformation, the basal dislocations are trapped in a closed triangular prism space and it was difficult to escape. The aged Mg–4Sm–3Gd–2Yb–0.5Zr alloy showed the optimal mechanical properties, and its yield strength, ultimate tensile strength and elongation were 198 MPa, 275 MPa and 6.6%.

Graphical Abstract

Abstract Image

添加镱对 Mg-4Sm-3Gd-0.5Zr 合金微观结构和力学性能的影响
系统研究了不同热处理状态下 Mg-4Sm-3Gd-xYb-0.5Zr(x = 0、1、2、3 wt%)合金的微观结构和力学性能,以及 Yb 对力学性能的影响机理。结果表明,添加镱能明显细化晶粒尺寸,均匀化微观结构,提高强度和塑性。Yb 的加入改变了晶格常数,降低了 c/a 值,缩短了峰值时效时间,加速了 β′ 相的析出。随着镱含量的增加,β′相的数量也随之增加。相邻β′相之间的间距减小,基底位错绕过β′相所需的临界剪切应力增加。β′相通过奥罗恩机制提高了老化合金的强度。β′相沿着[1(bar{1}/00] Mg、[01(bar{1}/0] Mg和[01(overline{1 })010] Mg这三个方向形成了一个近乎封闭的三角形棱柱空间。在拉伸变形过程中,基底位错被困在一个封闭的三角棱柱空间中,很难逃脱。老化后的 Mg-4Sm-3Gd-2Yb-0.5Zr 合金显示出最佳的力学性能,其屈服强度、极限抗拉强度和伸长率分别为 198 MPa、275 MPa 和 6.6%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Metals and Materials International
Metals and Materials International 工程技术-材料科学:综合
CiteScore
7.10
自引率
8.60%
发文量
197
审稿时长
3.7 months
期刊介绍: Metals and Materials International publishes original papers and occasional critical reviews on all aspects of research and technology in materials engineering: physical metallurgy, materials science, and processing of metals and other materials. Emphasis is placed on those aspects of the science of materials that are concerned with the relationships among the processing, structure and properties (mechanical, chemical, electrical, electrochemical, magnetic and optical) of materials. Aspects of processing include the melting, casting, and fabrication with the thermodynamics, kinetics and modeling.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信