Effect of Hydrothermal, Chemical, and Mechanical Degradation on Flexural Strength and Phase Transformation of Ground, Glazed, and Polished Zirconia

Q3 Dentistry
Nioosha Sarabi, M. Mohammadi-Bassir, Forough Fadavi, M. Rezvani, Fahimeh Dehestani-Ardakani, Hossein Labbaf
{"title":"Effect of Hydrothermal, Chemical, and Mechanical Degradation on Flexural Strength and Phase Transformation of Ground, Glazed, and Polished Zirconia","authors":"Nioosha Sarabi, M. Mohammadi-Bassir, Forough Fadavi, M. Rezvani, Fahimeh Dehestani-Ardakani, Hossein Labbaf","doi":"10.18502/fid.v21i16.15483","DOIUrl":null,"url":null,"abstract":"Objectives: Evaluation of the effect of grinding on flexural strength of zirconia after low temperature degradation (LTD) and pH-cycling. \nMaterials and Methods: Sixty-four bar-shaped specimens of yttria-stabilized tetragonal polycrystalline zirconia were milled, sintered, wet-polished, and divided into 8 groups (N=8). The four control groups were not aged while artificial aging was performed in the 4 experimental groups in three steps including  LTD in steam for 40h, pH-cycling, and tooth brushing for artificial aging. All groups underwent surface preparations as follows: standard polishing without surface treatment (Sp), grinding with a blue-yellow band diamond instrument (Gr); grinding with a diamond rotary instrument (DRI) and then over-glazing (Gl); grinding with a DRI followed by two-step intraoral polishing (Po); standard polishing and aging (Sp-Ag); grinding and aging (Gr-Ag), grinding, over-glazing and aging (Gl-Ag); and grinding, polishing and aging (Po-Ag). Monoclinic content was assessed in one specimen of each group by X-ray diffraction (XRD). The 3-point flexural strength test was performed in a universal testing machine. The results were analyzed with two-way ANOVA and Tukey’s test (α=0.05). \nResults: Mean flexural strength (Mpa) was significantly higher in groups Gr and Po compared to group Sp (both, P<0.0001) and group Gl (both, P<0.0001). In XRD analyses, the highest monoclinic phase before aging was observed in group Gr (12.6%), and after aging in group Gr-Ag (51.2%). \nConclusion: Grinding and polishing increased the flexural strength, while glazing did not exhibit any significant effect on this parameter.  Furthermore, aging did not adversely affect flexural strength.","PeriodicalId":12445,"journal":{"name":"Frontiers in Dentistry","volume":"109 15","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2024-05-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Frontiers in Dentistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.18502/fid.v21i16.15483","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"Dentistry","Score":null,"Total":0}
引用次数: 0

Abstract

Objectives: Evaluation of the effect of grinding on flexural strength of zirconia after low temperature degradation (LTD) and pH-cycling. Materials and Methods: Sixty-four bar-shaped specimens of yttria-stabilized tetragonal polycrystalline zirconia were milled, sintered, wet-polished, and divided into 8 groups (N=8). The four control groups were not aged while artificial aging was performed in the 4 experimental groups in three steps including  LTD in steam for 40h, pH-cycling, and tooth brushing for artificial aging. All groups underwent surface preparations as follows: standard polishing without surface treatment (Sp), grinding with a blue-yellow band diamond instrument (Gr); grinding with a diamond rotary instrument (DRI) and then over-glazing (Gl); grinding with a DRI followed by two-step intraoral polishing (Po); standard polishing and aging (Sp-Ag); grinding and aging (Gr-Ag), grinding, over-glazing and aging (Gl-Ag); and grinding, polishing and aging (Po-Ag). Monoclinic content was assessed in one specimen of each group by X-ray diffraction (XRD). The 3-point flexural strength test was performed in a universal testing machine. The results were analyzed with two-way ANOVA and Tukey’s test (α=0.05). Results: Mean flexural strength (Mpa) was significantly higher in groups Gr and Po compared to group Sp (both, P<0.0001) and group Gl (both, P<0.0001). In XRD analyses, the highest monoclinic phase before aging was observed in group Gr (12.6%), and after aging in group Gr-Ag (51.2%). Conclusion: Grinding and polishing increased the flexural strength, while glazing did not exhibit any significant effect on this parameter.  Furthermore, aging did not adversely affect flexural strength.
水热、化学和机械降解对研磨、上釉和抛光氧化锆挠曲强度和相变的影响
目的:评估低温降解(LTD)和 pH 循环后研磨对氧化锆抗弯强度的影响。材料与方法:对 64 块条形钇稳定四方多晶氧化锆试样进行研磨、烧结和湿法抛光,并将其分为 8 组(N=8)。4 个对照组未进行人工老化,而 4 个实验组则分三个步骤进行人工老化,包括在蒸汽中 LTD 40 小时、pH 循环和刷牙进行人工老化。所有实验组都进行了以下表面处理:不进行表面处理的标准抛光(Sp),使用蓝黄带金刚石器械进行研磨(Gr);使用金刚石旋转器械(DRI)进行研磨,然后上釉(Gl);使用 DRI 进行研磨,然后进行两步口内抛光(Po);标准抛光和老化(Sp-Ag);研磨和老化(Gr-Ag),研磨、上釉和老化(Gl-Ag);以及研磨、抛光和老化(Po-Ag)。通过 X 射线衍射 (XRD) 评估了每组中一个试样的单斜含量。在万能试验机上进行了三点抗弯强度测试。结果采用双向方差分析和 Tukey 检验(α=0.05)进行分析。结果与 Sp 组(均为 P<0.0001)和 Gl 组(均为 P<0.0001)相比,Gr 组和 Po 组的平均抗折强度(Mpa)明显更高。在 XRD 分析中,老化前 Gr 组的单斜相最高(12.6%),老化后 Gr-Ag 组的单斜相最高(51.2%)。结论研磨和抛光提高了抗弯强度,而上釉对这一参数没有明显影响。 此外,老化也不会对抗弯强度产生不利影响。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
Frontiers in Dentistry
Frontiers in Dentistry Dentistry-General Dentistry
CiteScore
1.00
自引率
0.00%
发文量
34
审稿时长
12 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信