Lincoln Borges , Matthew Logan , Samuel Weber , Steven Lewis , Clark Fang , Lourenço Correr-Sobrinho , Carmem Pfeifer
{"title":"Multi-acrylamides improve bond stability through collagen reinforcement under physiological conditions","authors":"Lincoln Borges , Matthew Logan , Samuel Weber , Steven Lewis , Clark Fang , Lourenço Correr-Sobrinho , Carmem Pfeifer","doi":"10.1016/j.dental.2024.05.002","DOIUrl":null,"url":null,"abstract":"<div><h3>Objectives</h3><p>Acrylamides were shown to significantly improve bonding stability in adhesive restorations, but the reinforcement mechanism has not been fully elucidated. We tested the hypothesis that hydrogen bonding reinforcement of the collagen network (with secondary or tertiary acrylamides), as well as degree of crosslinking of the polymer network (with di- or tri-functional acrylamides), can be two of the factors at play.</p></div><div><h3>Methods</h3><p>Two-step total etch adhesives comprising UDMA (60 wt%) and 40 wt% of: TAAEA, TMAAEA (secondary, tertiary tri-acrylamides), BAAP, DEBAAP (secondary, tertiary di-acrylamides) or HEMA (mono-methacrylate - control) were formulated. Simulated composite restorations (n = 5) were tested after cyclic mechanical and biological (<em>S. mutans</em> biofilm) challenges. Gap formation before and after aging was assessed with SEM imaging. Micro-tensile bond strength (μTBS, n = 6) was assessed after seven-day incubation in water or <em>S. mutans</em>-containing culture medium. Collagen reinforcement was assessed with hydroxyproline assay (n = 10) and rheology (n = 3). Data were analyzed with one-way/two-way ANOVA/Tukey’s test (alpha=5%).</p></div><div><h3>Results</h3><p>Gap formation increased and bond strength decreased for all monomers after biofilm incubation (p < 0.001). Except for DEBAAP, secondary and tertiary di/tri-acrylamides showed lower occlusal gap width values, but no significant differences overall gap length compared to HEMA. μTBS increased for tri-acrylamides compared with HEMA. Samples treated with multi-acrylamides had lower concentration of hydroxyproline (by-product of collagen degradation) (p < 0.001), except for DEBAAP, which showed values close to HEMA (p > 0.05). Dentin shear modulus increased for all acrylamides after 72 h, especially TMAAEA.</p></div><div><h3>Significance</h3><p>In general, multi-acrylamides promote collagen reinforcement, leading to reduced gap formation, and stabilize the bond strength under physiological conditions.</p></div>","PeriodicalId":298,"journal":{"name":"Dental Materials","volume":null,"pages":null},"PeriodicalIF":4.6000,"publicationDate":"2024-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Dental Materials","FirstCategoryId":"5","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S0109564124001039","RegionNum":1,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"DENTISTRY, ORAL SURGERY & MEDICINE","Score":null,"Total":0}
引用次数: 0
Abstract
Objectives
Acrylamides were shown to significantly improve bonding stability in adhesive restorations, but the reinforcement mechanism has not been fully elucidated. We tested the hypothesis that hydrogen bonding reinforcement of the collagen network (with secondary or tertiary acrylamides), as well as degree of crosslinking of the polymer network (with di- or tri-functional acrylamides), can be two of the factors at play.
Methods
Two-step total etch adhesives comprising UDMA (60 wt%) and 40 wt% of: TAAEA, TMAAEA (secondary, tertiary tri-acrylamides), BAAP, DEBAAP (secondary, tertiary di-acrylamides) or HEMA (mono-methacrylate - control) were formulated. Simulated composite restorations (n = 5) were tested after cyclic mechanical and biological (S. mutans biofilm) challenges. Gap formation before and after aging was assessed with SEM imaging. Micro-tensile bond strength (μTBS, n = 6) was assessed after seven-day incubation in water or S. mutans-containing culture medium. Collagen reinforcement was assessed with hydroxyproline assay (n = 10) and rheology (n = 3). Data were analyzed with one-way/two-way ANOVA/Tukey’s test (alpha=5%).
Results
Gap formation increased and bond strength decreased for all monomers after biofilm incubation (p < 0.001). Except for DEBAAP, secondary and tertiary di/tri-acrylamides showed lower occlusal gap width values, but no significant differences overall gap length compared to HEMA. μTBS increased for tri-acrylamides compared with HEMA. Samples treated with multi-acrylamides had lower concentration of hydroxyproline (by-product of collagen degradation) (p < 0.001), except for DEBAAP, which showed values close to HEMA (p > 0.05). Dentin shear modulus increased for all acrylamides after 72 h, especially TMAAEA.
Significance
In general, multi-acrylamides promote collagen reinforcement, leading to reduced gap formation, and stabilize the bond strength under physiological conditions.
期刊介绍:
Dental Materials publishes original research, review articles, and short communications.
Academy of Dental Materials members click here to register for free access to Dental Materials online.
The principal aim of Dental Materials is to promote rapid communication of scientific information between academia, industry, and the dental practitioner. Original Manuscripts on clinical and laboratory research of basic and applied character which focus on the properties or performance of dental materials or the reaction of host tissues to materials are given priority publication. Other acceptable topics include application technology in clinical dentistry and dental laboratory technology.
Comprehensive reviews and editorial commentaries on pertinent subjects will be considered.