Corrosion behavior of selective laser melting-manufactured bio-applicable 316L stainless steel in ionized simulated body fluid

IF 6.8 3区 医学 Q1 ENGINEERING, BIOMEDICAL
R. Kocich, L. Kuncická, Marek Benč, Adam Weiser, Gergely Németh
{"title":"Corrosion behavior of selective laser melting-manufactured bio-applicable 316L stainless steel in ionized simulated body fluid","authors":"R. Kocich, L. Kuncická, Marek Benč, Adam Weiser, Gergely Németh","doi":"10.36922/ijb.1416","DOIUrl":null,"url":null,"abstract":"Additive manufacturing (AM) is gaining increasing popularity in various fields, including biomedical engineering. Although AM enables fabrication of tailored components with complex geometries, the manufactured parts typically feature several internal issues, such as unpredictable distribution of residual stress and printing defects. However, these issues can be reduced or eliminated by post-processing via thermomechanical treatment. The study investigated the effects of combinations of AM and post-processing by the intensive plastic deformation method of rotary swaging (variable swaging ratios) on microstructures, residual stress, and corrosion behaviors of AISI 316L stainless steel workpieces; the corrosion tests were performed in an ionized simulated body fluid. The results showed that the gradual swaging process favorably refined the grains and homogenized the grain size. The imposed swaging ratio also directly influenced the development of substructure and dislocations density. A high density of dislocations positively affected the corrosion resistance, whereas annihilation of dislocations and formation of subgrains had a negative effect on the corrosion behavior. The first few swaging passes homogenized the distribution of residual stress within the workpiece and acted toward imparting a predominantly compressive stress state, which also favorably influenced the corrosion behavior. Lastly, the presence of the {111}||swaging direction texture fiber (of a high intensity) increased the resistance to pitting corrosion. Overall, the most favorable corrosion behavior was acquired for the AM sample subjected to the swaging ratio of 0.8, exhibiting a strong fiber texture and a high density of dislocations.","PeriodicalId":48522,"journal":{"name":"International Journal of Bioprinting","volume":"73 5","pages":""},"PeriodicalIF":6.8000,"publicationDate":"2024-01-05","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Bioprinting","FirstCategoryId":"5","ListUrlMain":"https://doi.org/10.36922/ijb.1416","RegionNum":3,"RegionCategory":"医学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q1","JCRName":"ENGINEERING, BIOMEDICAL","Score":null,"Total":0}
引用次数: 0

Abstract

Additive manufacturing (AM) is gaining increasing popularity in various fields, including biomedical engineering. Although AM enables fabrication of tailored components with complex geometries, the manufactured parts typically feature several internal issues, such as unpredictable distribution of residual stress and printing defects. However, these issues can be reduced or eliminated by post-processing via thermomechanical treatment. The study investigated the effects of combinations of AM and post-processing by the intensive plastic deformation method of rotary swaging (variable swaging ratios) on microstructures, residual stress, and corrosion behaviors of AISI 316L stainless steel workpieces; the corrosion tests were performed in an ionized simulated body fluid. The results showed that the gradual swaging process favorably refined the grains and homogenized the grain size. The imposed swaging ratio also directly influenced the development of substructure and dislocations density. A high density of dislocations positively affected the corrosion resistance, whereas annihilation of dislocations and formation of subgrains had a negative effect on the corrosion behavior. The first few swaging passes homogenized the distribution of residual stress within the workpiece and acted toward imparting a predominantly compressive stress state, which also favorably influenced the corrosion behavior. Lastly, the presence of the {111}||swaging direction texture fiber (of a high intensity) increased the resistance to pitting corrosion. Overall, the most favorable corrosion behavior was acquired for the AM sample subjected to the swaging ratio of 0.8, exhibiting a strong fiber texture and a high density of dislocations.
离子化模拟体液中选择性激光熔化制造的生物应用 316L 不锈钢的腐蚀行为
快速成型制造(AM)在包括生物医学工程在内的各个领域越来越受欢迎。虽然增材制造可以制造出具有复杂几何形状的定制部件,但制造出的部件通常会出现一些内部问题,如不可预知的残余应力分布和打印缺陷。不过,这些问题可以通过热机械处理的后处理方法来减少或消除。该研究调查了 AM 与旋转锻造(可变锻造比)强化塑性变形方法后处理的组合对 AISI 316L 不锈钢工件的微观结构、残余应力和腐蚀行为的影响;腐蚀测试在离子化模拟体液中进行。结果表明,渐进式锻造过程有利于细化晶粒和均匀晶粒尺寸。所施加的锻造比率也直接影响了亚结构和位错密度的发展。位错密度高会对耐腐蚀性产生积极影响,而位错湮灭和亚晶粒的形成则会对腐蚀行为产生消极影响。前几道锻造工序使工件内部的残余应力分布均匀化,并形成了以压应力为主的应力状态,这也对腐蚀行为产生了有利影响。最后,{111}|||浇铸方向纹理纤维(高强度)的存在提高了抗点蚀能力。总体而言,采用 0.8 拉伸比的 AM 样品具有最理想的腐蚀性能,表现出较强的纤维纹理和较高的位错密度。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
CiteScore
6.90
自引率
4.80%
发文量
81
期刊介绍: The International Journal of Bioprinting is a globally recognized publication that focuses on the advancements, scientific discoveries, and practical implementations of Bioprinting. Bioprinting, in simple terms, involves the utilization of 3D printing technology and materials that contain living cells or biological components to fabricate tissues or other biotechnological products. Our journal encompasses interdisciplinary research that spans across technology, science, and clinical applications within the expansive realm of Bioprinting.
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信