{"title":"Investigation of defect formation in the form of longitudinal folds at the ends of semi-finished pipes during rolling on an automatic TPA mill","authors":"N. I. Sherbutaev","doi":"10.32339/0135-5910-2023-9-755-760","DOIUrl":null,"url":null,"abstract":"The article presents an elimination method aimed at addressing the defects in the form of longitudinal folds at the ends of semi-finished pipes during rolling on automatic mills of a pipe rolling plant (TPA). Currently, this issue is relevant, as it significantly affects the quality of the pipes produced. The developed solution is based on the implementation of a special design that prevents the occurrence of longitudinal folds at the ends of semi-finished pipes. Experimental studies have been conducted to confirm the effectiveness of the proposed technical solution. The obtained results demonstrate a significant reduction in the number of defective pipes and an increase in the overall volume of high-quality production. The developed technical solution represents a significant contribution to the improvement of pipe rolling technology on automatic TPA mills and can be applied in production conditions to enhance outcomes and resource efficiency","PeriodicalId":429631,"journal":{"name":"Ferrous Metallurgy. Bulletin of Scientific , Technical and Economic Information","volume":"93 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-10-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Ferrous Metallurgy. Bulletin of Scientific , Technical and Economic Information","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.32339/0135-5910-2023-9-755-760","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The article presents an elimination method aimed at addressing the defects in the form of longitudinal folds at the ends of semi-finished pipes during rolling on automatic mills of a pipe rolling plant (TPA). Currently, this issue is relevant, as it significantly affects the quality of the pipes produced. The developed solution is based on the implementation of a special design that prevents the occurrence of longitudinal folds at the ends of semi-finished pipes. Experimental studies have been conducted to confirm the effectiveness of the proposed technical solution. The obtained results demonstrate a significant reduction in the number of defective pipes and an increase in the overall volume of high-quality production. The developed technical solution represents a significant contribution to the improvement of pipe rolling technology on automatic TPA mills and can be applied in production conditions to enhance outcomes and resource efficiency