Waleed A. Salih, Sabah M. Aman Allah, Salih Y. Darweesh
{"title":"Effect of Spray Angle on Some Physical Properties of a Ceramic System Produced by Thermal spraying Coating","authors":"Waleed A. Salih, Sabah M. Aman Allah, Salih Y. Darweesh","doi":"10.55810/2313-0083.1022","DOIUrl":null,"url":null,"abstract":"The angle of thermal spraying by the flame is considered one of the important influences on the coating layer, where alumina (Al2O3)% was used as a base material, and it was reinforced with two metals (TiAl) with weight ratios of (25%) in order to produce a cermet composite material with a final thickness ranging between (300-400) µm and with a fixed thermal spray distance of 16cm, the samples resulting from the paint were thermally sintered at a temperature of (1000°C) for an hour and a half, after the samples were taken out of the oven and some mechanical operation was performed on them, some physical tests were conducted, the most important of which included an examination X-ray diffraction, as well as porosity, hardness, and adhesion strength, to show through laboratory tests that the best thermal spray angle is 90°, at a mixing ratio of 25% after thermal sintering.","PeriodicalId":218143,"journal":{"name":"Al-Bahir Journal for Engineering and Pure Sciences","volume":"107 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-04-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Al-Bahir Journal for Engineering and Pure Sciences","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.55810/2313-0083.1022","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
The angle of thermal spraying by the flame is considered one of the important influences on the coating layer, where alumina (Al2O3)% was used as a base material, and it was reinforced with two metals (TiAl) with weight ratios of (25%) in order to produce a cermet composite material with a final thickness ranging between (300-400) µm and with a fixed thermal spray distance of 16cm, the samples resulting from the paint were thermally sintered at a temperature of (1000°C) for an hour and a half, after the samples were taken out of the oven and some mechanical operation was performed on them, some physical tests were conducted, the most important of which included an examination X-ray diffraction, as well as porosity, hardness, and adhesion strength, to show through laboratory tests that the best thermal spray angle is 90°, at a mixing ratio of 25% after thermal sintering.