{"title":"Pengaruh Variasi Waktu Pemeraman Terhadap Daya Dukung Tanah Lunak Gambut Kalimantan Selatan Distabilisasi Menggunakan Semen Portland","authors":"Akhmad Gazali, R. Adawiyah","doi":"10.33084/mits.v7i1.680","DOIUrl":null,"url":null,"abstract":"Stabilization is an attempt to improve the physical and mechanical properties of the soil so that it meets specific technical requirements. One method of stabilization is the addition of portland cement additives. This study aimed to compare the CBR values of soft soil of peat before and after stabilization with portland cement and to determine the effect of variations in ripening time on carrying capacity of soft soil peat. Soft peat soil used was taken from Handil Bakti Village, Alalak District, Barito Kuala District, South Kalimantan Province. Variations in the addition of cement levels used 5%, 10%, and 15%, while the variety of curing time starts from 7 days, 14 days and 21 days. In the results of the modified Proctor compaction test, the addition of cement levels in the soft soil of peat was shown to increase the maximum dry weight volume (?d) value continuously. While the value of optimum water content (?opt) has decreased which is not too significant at each addition of cement content. For the value of the soft soil type of peat mixed with cement, the increase in weight compared with the original soil type weight. In CBR Laboratory testing using modified Proctor compaction at 15% cement content addition and 21 days curing time, the maximum CBR value of the Laboratory was 18.039%. The addition of Portland cement has been shown to increase the CBR value and the carrying capacity of the soil","PeriodicalId":380506,"journal":{"name":"Media Ilmiah Teknik Sipil","volume":"171 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2018-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Media Ilmiah Teknik Sipil","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.33084/mits.v7i1.680","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

Abstract

Stabilization is an attempt to improve the physical and mechanical properties of the soil so that it meets specific technical requirements. One method of stabilization is the addition of portland cement additives. This study aimed to compare the CBR values of soft soil of peat before and after stabilization with portland cement and to determine the effect of variations in ripening time on carrying capacity of soft soil peat. Soft peat soil used was taken from Handil Bakti Village, Alalak District, Barito Kuala District, South Kalimantan Province. Variations in the addition of cement levels used 5%, 10%, and 15%, while the variety of curing time starts from 7 days, 14 days and 21 days. In the results of the modified Proctor compaction test, the addition of cement levels in the soft soil of peat was shown to increase the maximum dry weight volume (?d) value continuously. While the value of optimum water content (?opt) has decreased which is not too significant at each addition of cement content. For the value of the soft soil type of peat mixed with cement, the increase in weight compared with the original soil type weight. In CBR Laboratory testing using modified Proctor compaction at 15% cement content addition and 21 days curing time, the maximum CBR value of the Laboratory was 18.039%. The addition of Portland cement has been shown to increase the CBR value and the carrying capacity of the soil
保护时间的变化对南加里曼丹软泥炭土壤的支持的影响是由波特兰水泥稳定下来的
稳定是试图改善土壤的物理和机械特性,使其符合特定的技术要求。稳定的一种方法是添加波特兰水泥添加剂。本研究旨在比较硅酸盐水泥稳定前后泥炭软土的CBR值,确定成熟时间的变化对泥炭软土承载能力的影响。所使用的软泥炭土取自南加里曼丹省巴里托瓜拉区Alalak区的Handil Bakti村。水泥掺量分别为5%、10%和15%,养护时间分别为7天、14天和21天。改进的Proctor压实试验结果表明,泥炭软土中水泥水平的增加使其最大干重体积(?d)值不断增加。而最佳含水率(?opt)值随着水泥掺量的增加而减小,但减小幅度不大。对于软土型泥炭掺入水泥后,其重量较原土型重量增加。在水泥掺量为15%、养护时间为21 d的情况下,采用改良Proctor压实法进行CBR实验室测试,实验室CBR最大值为18.039%。波特兰水泥的加入提高了CBR值和土壤的承载能力
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信