Pengaruh Nilai Carbon Equivalen (CE) Dari Cast Iron Pada Proses Penangkaian Anoda Di Rodding Plant

D. I. Muthawali
{"title":"Pengaruh Nilai Carbon Equivalen (CE) Dari Cast Iron Pada Proses Penangkaian Anoda Di Rodding Plant","authors":"D. I. Muthawali","doi":"10.30596/AGRINTECH.V1I2.2010","DOIUrl":null,"url":null,"abstract":"Addition of the substance will effect the value of carbon equivalent (CE) cast iron. Carbon equivalent value is a parameter that tells us how much carbon is cointained in the cast iron. Carbon equivalent values were determined between 4,7 to 4,9. When the carbon equivalent (CE) on the cast iron is less than 4.7 to 4.9 then it will be easy to cast iron, causing cracks in the baked anode rod will come loose. And usage cast iron is not optimal. And when more than that value so cast iron will difficult loose from the anode rod. From the observations that have been made obtainable carbon equivalent (CE) cast iron are 3,76 and 4,7. This indicates that the value of carbon equivalent (CE) cast iron still eligible and meet the standars that have been established which is between 4,7 to 4,9.","PeriodicalId":295960,"journal":{"name":"Agrintech: Jurnal Teknologi Pangan dan Hasil Pertanian","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2018-06-19","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Agrintech: Jurnal Teknologi Pangan dan Hasil Pertanian","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.30596/AGRINTECH.V1I2.2010","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1

Abstract

Addition of the substance will effect the value of carbon equivalent (CE) cast iron. Carbon equivalent value is a parameter that tells us how much carbon is cointained in the cast iron. Carbon equivalent values were determined between 4,7 to 4,9. When the carbon equivalent (CE) on the cast iron is less than 4.7 to 4.9 then it will be easy to cast iron, causing cracks in the baked anode rod will come loose. And usage cast iron is not optimal. And when more than that value so cast iron will difficult loose from the anode rod. From the observations that have been made obtainable carbon equivalent (CE) cast iron are 3,76 and 4,7. This indicates that the value of carbon equivalent (CE) cast iron still eligible and meet the standars that have been established which is between 4,7 to 4,9.
添加该物质会影响铸铁的碳当量(CE)值。碳当量是一个参数,它告诉我们铸铁中含有多少碳。碳当量在4,7到4,9之间测定。当铸铁上的碳当量(CE)低于4.7 ~ 4.9时,就容易铸铁,造成烘烤后的阳极棒出现裂纹,出现松动。而且使用铸铁也不是最优的。而当超过这个值时,那么铸铁将难以从阳极棒上松动。从已取得的观察来看,可获得的碳当量(CE)铸铁是3.76和4.7。这表明,碳当量(CE)铸铁的价值仍然是合格的,并符合已建立的标准,即4,7至4,9之间。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信