{"title":"Isothermal and thermally stimulated discharge of pure and anthracene doped poly(methyl methacrylate) foils","authors":"J. Keller, K. Vyas, R. DeBey, S. Datt","doi":"10.1109/ISE.1996.578052","DOIUrl":null,"url":null,"abstract":"The charge storage and transport behaviour of 100 /spl mu/m thick pure and 0.1 wt% anthracene doped poly(methyl methacrylate) (PMMA) foils has been investigated by absorption current, isothermal surface charge decay and thermally stimulated discharge current (TSDC) measurement techniques over a temperature range of 298 to 393 K, with fields ranging from 8 to 50 kV/cm.","PeriodicalId":425004,"journal":{"name":"9th International Symposium on Electrets (ISE 9) Proceedings","volume":"19 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1996-09-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"9th International Symposium on Electrets (ISE 9) Proceedings","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ISE.1996.578052","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
The charge storage and transport behaviour of 100 /spl mu/m thick pure and 0.1 wt% anthracene doped poly(methyl methacrylate) (PMMA) foils has been investigated by absorption current, isothermal surface charge decay and thermally stimulated discharge current (TSDC) measurement techniques over a temperature range of 298 to 393 K, with fields ranging from 8 to 50 kV/cm.