{"title":"FOR THE STUDY OF PECULIARITIES OF STRUCTURE FORMATION OF COMPOSITE BINDERS FOR NON-AUTOCLAVED AERATED CONCRETE","authors":"V. Lesovik, M. Absimetov, M. Elistratkin, S. Shatalova","doi":"10.34031/2618-7183-2019-2-3-41-47","DOIUrl":null,"url":null,"abstract":"the basis of the modern market of cellular concrete is autoclaved gas silicate. At the same time, non-autoclaved aerated concrete is largely a more technological material, allowing the variation of its properties within a wide range, having a potentially wider field of application, less costly in the organization of production, which is of great importance for small and medium-sized businesses. The main problem of non-autoclaved aerated concrete is a higher cost of raw materials compared to silicate, and 20...30% lower strength performance. The proposed solution to this problem is the development of special composite binders with a limited content of clinker and mineral additives of various genetic types, taking into account the peculiarities of the two-stage structure formation of the material – gas porization and the formation of the microstructure of the stone. The article deals with some aspects of the interaction in the system “mineral additive – gypsum – by-products of the gas release reaction” in terms of the effect on the viscosity of the swelling mass and the strength of the stone at different times of hardening. Recommendations are given on the preferred compositions of composite binders and dosages of gypsum in the molding mixture when producing a material with an average density in the range of 500...700 kg/m3.","PeriodicalId":127090,"journal":{"name":"Construction Materials and Products","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2020-06-04","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"9","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Construction Materials and Products","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.34031/2618-7183-2019-2-3-41-47","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 9

Abstract

the basis of the modern market of cellular concrete is autoclaved gas silicate. At the same time, non-autoclaved aerated concrete is largely a more technological material, allowing the variation of its properties within a wide range, having a potentially wider field of application, less costly in the organization of production, which is of great importance for small and medium-sized businesses. The main problem of non-autoclaved aerated concrete is a higher cost of raw materials compared to silicate, and 20...30% lower strength performance. The proposed solution to this problem is the development of special composite binders with a limited content of clinker and mineral additives of various genetic types, taking into account the peculiarities of the two-stage structure formation of the material – gas porization and the formation of the microstructure of the stone. The article deals with some aspects of the interaction in the system “mineral additive – gypsum – by-products of the gas release reaction” in terms of the effect on the viscosity of the swelling mass and the strength of the stone at different times of hardening. Recommendations are given on the preferred compositions of composite binders and dosages of gypsum in the molding mixture when producing a material with an average density in the range of 500...700 kg/m3.
对非蒸压加气混凝土复合粘结剂的结构形成特性进行了研究
现代泡沫混凝土市场的基础是蒸压气体硅酸盐。同时,非蒸压加气混凝土在很大程度上是一种更具技术性的材料,允许其性能在很大范围内变化,具有潜在的更广泛的应用领域,在生产组织中成本更低,这对中小型企业非常重要。与硅酸盐相比,非蒸压加气混凝土的主要问题是原材料成本较高。降低30%强度性能。解决这一问题的方法是考虑到材料的两阶段结构形成的特殊性——气体孔隙化和石头微观结构的形成,开发具有有限含量的熟料和各种成因类型的矿物添加剂的特殊复合粘结剂。本文论述了“矿物添加剂-石膏-气体释放反应副产物”体系中相互作用对溶胀体粘度和不同硬化时期石材强度的影响。当生产平均密度在500…范围内的材料时,给出了复合粘结剂的优选成分和石膏在成型混合物中的用量。700公斤/立方米。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
求助全文
约1分钟内获得全文 求助全文
来源期刊
CiteScore
1.40
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信