{"title":"Evaluasi Retak Pada Slab Beton Lantai Kendaraan Gedung Parkir dan Metode Perbaikannya","authors":"Sulardi Sulardi","doi":"10.33084/mits.v7i1.679","DOIUrl":null,"url":null,"abstract":"The aim to be achieved from this research activity is to provide an overview of the factors and causes of cracks, labar and crack depth on the concrete slab of the vehicle floor of the parking building and recommendations for improvement methods. This research method is a used research method and is a success story of crack evaluation and handling methods that have been carried out. The results showed that the crack width that occurred was 0.624-1.022 mm vs. 0.33 mm, out of tolerance. The results of the deflection measurements also show an average deflection in the concrete slab of the vehicle floor is 5.8-10.5 Cm and indicates that the crack has reached the concrete reinforcement, out of tolerance. With the results of this study, it is recommended that improvements be made with crack injection methods using low-pressure injection tools and specifications of an epoxy resin material.","PeriodicalId":380506,"journal":{"name":"Media Ilmiah Teknik Sipil","volume":"302 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2018-12-15","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"1","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Media Ilmiah Teknik Sipil","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.33084/mits.v7i1.679","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 1
Abstract
The aim to be achieved from this research activity is to provide an overview of the factors and causes of cracks, labar and crack depth on the concrete slab of the vehicle floor of the parking building and recommendations for improvement methods. This research method is a used research method and is a success story of crack evaluation and handling methods that have been carried out. The results showed that the crack width that occurred was 0.624-1.022 mm vs. 0.33 mm, out of tolerance. The results of the deflection measurements also show an average deflection in the concrete slab of the vehicle floor is 5.8-10.5 Cm and indicates that the crack has reached the concrete reinforcement, out of tolerance. With the results of this study, it is recommended that improvements be made with crack injection methods using low-pressure injection tools and specifications of an epoxy resin material.
本次研究活动的目的是概述停车楼车辆底板混凝土板裂缝的因素和原因、裂缝宽度和裂缝深度,并提出改进方法建议。该研究方法是一种常用的研究方法,是已开展的裂缝评价和处理方法的成功案例。结果表明:出现的裂缝宽度为0.624 ~ 1.022 mm vs. 0.33 mm,超出公差范围;挠度测量结果还表明,车辆底板混凝土板的平均挠度为5.8 ~ 10.5 Cm,表明裂缝已经到达混凝土钢筋,超出公差范围。根据本研究的结果,建议使用低压注射工具和环氧树脂材料的规格来改进裂纹注射方法。