M. Vilmay, D. Roy, C. Besset, D. Galpin, C. Monget, P. Vannier, Y. Le Friec, G. Imbert, M. Mellier, S. Petitdidier, O. Robin, J. Guillan, S. Chhun, L. Arnaud, F. Volpi, J. Chaix
{"title":"Key Process steps for high reliable SiOCH low-k dielectrics for the sub 45nm technology nodes","authors":"M. Vilmay, D. Roy, C. Besset, D. Galpin, C. Monget, P. Vannier, Y. Le Friec, G. Imbert, M. Mellier, S. Petitdidier, O. Robin, J. Guillan, S. Chhun, L. Arnaud, F. Volpi, J. Chaix","doi":"10.1109/IITC.2009.5090359","DOIUrl":null,"url":null,"abstract":"The introduction of SiOCH low-k dielectrics in copper interconnects associated to the reduction of the critical dimensions in advanced technology nodes is becoming a major reliability concern. The interconnect realization requires a consequent number of critical process steps [1]. Since porous low-k dielectrics are used as Inter-Metal Dielectric (IMD) each process step can be a source of degradation for the dielectric. This paper describes critical process steps influencing the low-k reliability. All the processes affecting the dielectric's interfaces are also evidenced to degrade the low-k interconnect robustness. Some process examples as the direct chemical and mechanical polishing (CMP), the slurry chemistry and the TaN/Ta barrier etching are details in this paper. Moreover, some process options are given to strongly improve low-k dielectric reliability without degradation of its electrical performances.","PeriodicalId":301012,"journal":{"name":"2009 IEEE International Interconnect Technology Conference","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2009-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"4","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2009 IEEE International Interconnect Technology Conference","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/IITC.2009.5090359","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 4
Abstract
The introduction of SiOCH low-k dielectrics in copper interconnects associated to the reduction of the critical dimensions in advanced technology nodes is becoming a major reliability concern. The interconnect realization requires a consequent number of critical process steps [1]. Since porous low-k dielectrics are used as Inter-Metal Dielectric (IMD) each process step can be a source of degradation for the dielectric. This paper describes critical process steps influencing the low-k reliability. All the processes affecting the dielectric's interfaces are also evidenced to degrade the low-k interconnect robustness. Some process examples as the direct chemical and mechanical polishing (CMP), the slurry chemistry and the TaN/Ta barrier etching are details in this paper. Moreover, some process options are given to strongly improve low-k dielectric reliability without degradation of its electrical performances.