{"title":"研究了处理、烧结等工艺参数对铁基粉末结构的影响","authors":"A. Stanula, W. Pilarczyk, Mark Jager, T. Wilk","doi":"10.37904/metal.2020.3626","DOIUrl":null,"url":null,"abstract":"The subject of this article is the failed bushing used in the car suspension. The claim of the broken bushing came from the car producer. The main aim of this paper was to know if the failure was a green crack as evidenced by steam treatment oxide on the crack interfaces. To check, these items a Scanning Electron Microscope (SEM), hardness testers, and optical microscope were used. The density of the upper edge where the crack occurred was checked. Based on this investigation it was found that the crack was not caused by the rollover application.","PeriodicalId":18449,"journal":{"name":"METAL 2020 Conference Proeedings","volume":"48 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2020-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"The influence of technological parameters as the handling and sintering process on the structure of iron based powders\",\"authors\":\"A. Stanula, W. Pilarczyk, Mark Jager, T. Wilk\",\"doi\":\"10.37904/metal.2020.3626\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The subject of this article is the failed bushing used in the car suspension. The claim of the broken bushing came from the car producer. The main aim of this paper was to know if the failure was a green crack as evidenced by steam treatment oxide on the crack interfaces. To check, these items a Scanning Electron Microscope (SEM), hardness testers, and optical microscope were used. The density of the upper edge where the crack occurred was checked. Based on this investigation it was found that the crack was not caused by the rollover application.\",\"PeriodicalId\":18449,\"journal\":{\"name\":\"METAL 2020 Conference Proeedings\",\"volume\":\"48 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2020-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"METAL 2020 Conference Proeedings\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.37904/metal.2020.3626\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"METAL 2020 Conference Proeedings","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.37904/metal.2020.3626","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
The influence of technological parameters as the handling and sintering process on the structure of iron based powders
The subject of this article is the failed bushing used in the car suspension. The claim of the broken bushing came from the car producer. The main aim of this paper was to know if the failure was a green crack as evidenced by steam treatment oxide on the crack interfaces. To check, these items a Scanning Electron Microscope (SEM), hardness testers, and optical microscope were used. The density of the upper edge where the crack occurred was checked. Based on this investigation it was found that the crack was not caused by the rollover application.