Binggang Shang, Longlin Lei, Xiangyu Wang, Pei He, Xinzhe Yuan, Wei Dai, Jin Li, Yiming Jiang, Yangting Sun
{"title":"晶界特征随冷轧变形变化对443超纯铁素体不锈钢抗晶间腐蚀性能的影响","authors":"Binggang Shang, Longlin Lei, Xiangyu Wang, Pei He, Xinzhe Yuan, Wei Dai, Jin Li, Yiming Jiang, Yangting Sun","doi":"10.1016/j.corcom.2022.07.002","DOIUrl":null,"url":null,"abstract":"<div><p>The relationship between evolution in grain boundary characteristics and intergranular corrosion properties of cold rolled 443 ultra-pure ferritic stainless steel was investigated. The results showed that low-angle (LA) grain boundaries, special grain boundaries (SGB), and high-angle (HA) grain boundaries had a high intergranular corrosion sensitivity after cold deformation in reducing acid medium. In oxidative acid medium, the LA and SGB boundaries had a high intergranular corrosion resistance in comparison to HA boundaries, and their inhibitory effect on the corrosion continuance of the dynamic recrystallization high-angle (RHA) grain boundaries can improve the corrosion resistance of the RHA grain boundaries.</p></div>","PeriodicalId":100337,"journal":{"name":"Corrosion Communications","volume":"8 ","pages":"Pages 27-39"},"PeriodicalIF":0.0000,"publicationDate":"2022-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"https://www.sciencedirect.com/science/article/pii/S2667266922000524/pdfft?md5=db8fa0aff2c5817b9f9f5687114daa7e&pid=1-s2.0-S2667266922000524-main.pdf","citationCount":"10","resultStr":"{\"title\":\"Effects of grain boundary characteristics changing with cold rolling deformation on intergranular corrosion resistance of 443 ultra-pure ferritic stainless steel\",\"authors\":\"Binggang Shang, Longlin Lei, Xiangyu Wang, Pei He, Xinzhe Yuan, Wei Dai, Jin Li, Yiming Jiang, Yangting Sun\",\"doi\":\"10.1016/j.corcom.2022.07.002\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"<div><p>The relationship between evolution in grain boundary characteristics and intergranular corrosion properties of cold rolled 443 ultra-pure ferritic stainless steel was investigated. The results showed that low-angle (LA) grain boundaries, special grain boundaries (SGB), and high-angle (HA) grain boundaries had a high intergranular corrosion sensitivity after cold deformation in reducing acid medium. In oxidative acid medium, the LA and SGB boundaries had a high intergranular corrosion resistance in comparison to HA boundaries, and their inhibitory effect on the corrosion continuance of the dynamic recrystallization high-angle (RHA) grain boundaries can improve the corrosion resistance of the RHA grain boundaries.</p></div>\",\"PeriodicalId\":100337,\"journal\":{\"name\":\"Corrosion Communications\",\"volume\":\"8 \",\"pages\":\"Pages 27-39\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"https://www.sciencedirect.com/science/article/pii/S2667266922000524/pdfft?md5=db8fa0aff2c5817b9f9f5687114daa7e&pid=1-s2.0-S2667266922000524-main.pdf\",\"citationCount\":\"10\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Corrosion Communications\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://www.sciencedirect.com/science/article/pii/S2667266922000524\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Corrosion Communications","FirstCategoryId":"1085","ListUrlMain":"https://www.sciencedirect.com/science/article/pii/S2667266922000524","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Effects of grain boundary characteristics changing with cold rolling deformation on intergranular corrosion resistance of 443 ultra-pure ferritic stainless steel
The relationship between evolution in grain boundary characteristics and intergranular corrosion properties of cold rolled 443 ultra-pure ferritic stainless steel was investigated. The results showed that low-angle (LA) grain boundaries, special grain boundaries (SGB), and high-angle (HA) grain boundaries had a high intergranular corrosion sensitivity after cold deformation in reducing acid medium. In oxidative acid medium, the LA and SGB boundaries had a high intergranular corrosion resistance in comparison to HA boundaries, and their inhibitory effect on the corrosion continuance of the dynamic recrystallization high-angle (RHA) grain boundaries can improve the corrosion resistance of the RHA grain boundaries.