248 nm和488 nm五羰基铁沉积铁基薄膜的比较研究

I. Voicu, R. Alexandrescu, R. Cireasa, I. Morjan, D. Dumitras, S. Mulenko, A. N. Pogorelyǐ, A. Andrei
{"title":"248 nm和488 nm五羰基铁沉积铁基薄膜的比较研究","authors":"I. Voicu, R. Alexandrescu, R. Cireasa, I. Morjan, D. Dumitras, S. Mulenko, A. N. Pogorelyǐ, A. Andrei","doi":"10.1051/JPHYSCOL:1995581","DOIUrl":null,"url":null,"abstract":"Thin film deposition by laser irradiation of Fe(CO) 5 at two radiation wavelengths (248 nm and 488 nm) was performed. A perpendicular geometry of irradiation was used. Maximum deposition rates of 14 A/s at λ = 248 nm and 1.5 A/s at λ = 488 nm were obtained, indicating a diffusion limited process. SEM analysis of film morphologies showed significant differencies in the nucleation and growth of films deposited at 248 nm and 488 nm. XPS surface analysis revealed a higher carbon content and carbidic phases in the surface of films deposited at 488 nm on SiO 2 (quartz) substrates. Oxidized surface Fe phases were found in films, with increasing the exposure time to laser radiation. The film properties are discussed in connection with irradiation conditions and specific mechanisms involved.","PeriodicalId":17944,"journal":{"name":"Le Journal De Physique Colloques","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"1995-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"3","resultStr":"{\"title\":\"A Comparative Study of Iron-Based Film Deposition from Iron Pentacarbonyl at 248 nm and 488 nm\",\"authors\":\"I. Voicu, R. Alexandrescu, R. Cireasa, I. Morjan, D. Dumitras, S. Mulenko, A. N. Pogorelyǐ, A. Andrei\",\"doi\":\"10.1051/JPHYSCOL:1995581\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Thin film deposition by laser irradiation of Fe(CO) 5 at two radiation wavelengths (248 nm and 488 nm) was performed. A perpendicular geometry of irradiation was used. Maximum deposition rates of 14 A/s at λ = 248 nm and 1.5 A/s at λ = 488 nm were obtained, indicating a diffusion limited process. SEM analysis of film morphologies showed significant differencies in the nucleation and growth of films deposited at 248 nm and 488 nm. XPS surface analysis revealed a higher carbon content and carbidic phases in the surface of films deposited at 488 nm on SiO 2 (quartz) substrates. Oxidized surface Fe phases were found in films, with increasing the exposure time to laser radiation. The film properties are discussed in connection with irradiation conditions and specific mechanisms involved.\",\"PeriodicalId\":17944,\"journal\":{\"name\":\"Le Journal De Physique Colloques\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1995-06-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"3\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Le Journal De Physique Colloques\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1051/JPHYSCOL:1995581\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Le Journal De Physique Colloques","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1051/JPHYSCOL:1995581","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 3

摘要

用激光在248 nm和488 nm两个波长下辐照Fe(CO) 5,制备了Fe(CO) 5薄膜。辐照采用垂直几何形状。在λ = 248 nm处沉积速率最高为14 A/s,在λ = 488 nm处沉积速率最高为1.5 A/s,为扩散受限过程。薄膜形貌的SEM分析表明,在248 nm和488 nm处沉积的薄膜在成核和生长方面存在显著差异。XPS表面分析表明,在488nm sio2(石英)衬底上沉积的薄膜表面具有较高的碳含量和碳化物相。随着激光照射时间的延长,薄膜表面出现氧化铁相。讨论了膜的性能与辐照条件和具体机理的关系。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
A Comparative Study of Iron-Based Film Deposition from Iron Pentacarbonyl at 248 nm and 488 nm
Thin film deposition by laser irradiation of Fe(CO) 5 at two radiation wavelengths (248 nm and 488 nm) was performed. A perpendicular geometry of irradiation was used. Maximum deposition rates of 14 A/s at λ = 248 nm and 1.5 A/s at λ = 488 nm were obtained, indicating a diffusion limited process. SEM analysis of film morphologies showed significant differencies in the nucleation and growth of films deposited at 248 nm and 488 nm. XPS surface analysis revealed a higher carbon content and carbidic phases in the surface of films deposited at 488 nm on SiO 2 (quartz) substrates. Oxidized surface Fe phases were found in films, with increasing the exposure time to laser radiation. The film properties are discussed in connection with irradiation conditions and specific mechanisms involved.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信