{"title":"双碳化物基硬质合金的高温氧化","authors":"L. Bodrova, H. Kramar, I. Koval, S. Marynenko, O. Mul, Y. Kovalchuk, M. Prokopiv","doi":"10.33108/visnyk_tntu2023.01.005","DOIUrl":null,"url":null,"abstract":"Dependences of the oxidation kinetics in air of titanium and vanadium carbide based hard alloys with a nickel-chromium binder and the structure, phase and chemical composition of the formed scale in the temperature range 800–1100 ̊С were found. The regularities of the oxidation process were determined by the weight method, the main kinetic characteristics were calculated.","PeriodicalId":21595,"journal":{"name":"Scientific journal of the Ternopil national technical university","volume":"12 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"High temperature oxidation of double carbide based hard alloys\",\"authors\":\"L. Bodrova, H. Kramar, I. Koval, S. Marynenko, O. Mul, Y. Kovalchuk, M. Prokopiv\",\"doi\":\"10.33108/visnyk_tntu2023.01.005\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Dependences of the oxidation kinetics in air of titanium and vanadium carbide based hard alloys with a nickel-chromium binder and the structure, phase and chemical composition of the formed scale in the temperature range 800–1100 ̊С were found. The regularities of the oxidation process were determined by the weight method, the main kinetic characteristics were calculated.\",\"PeriodicalId\":21595,\"journal\":{\"name\":\"Scientific journal of the Ternopil national technical university\",\"volume\":\"12 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Scientific journal of the Ternopil national technical university\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.33108/visnyk_tntu2023.01.005\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Scientific journal of the Ternopil national technical university","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.33108/visnyk_tntu2023.01.005","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
High temperature oxidation of double carbide based hard alloys
Dependences of the oxidation kinetics in air of titanium and vanadium carbide based hard alloys with a nickel-chromium binder and the structure, phase and chemical composition of the formed scale in the temperature range 800–1100 ̊С were found. The regularities of the oxidation process were determined by the weight method, the main kinetic characteristics were calculated.