{"title":"硝酸法从Morowali红土矿中提取镍","authors":"I. W. Wirawan, D. K. Walanda, M. Napitupulu","doi":"10.22487/j24775185.2022.v11.i2.pp91-95","DOIUrl":null,"url":null,"abstract":"Nickel extraction from Morowali laterite ore has been carried out with nitric acid as the solvent. This study aims to determine the effect of nitric acid concentration, temperature, and stirring time on nickel content in laterite ore originating from Morowali. Morowali laterite seeds were extracted using the leaching method using nitric acid as the solvent with various concentrations of 0.5, 1, and 2, temperatures of 30, 60, and 95, and stirring times of 3, 6, and 12. Taguchi analysis was used in this study to obtain the effect of the three parameters used. The results showed that the optimum conditions were obtained at a concentration of 2 molars nitric acid, a temperature of 95°C, and a stirring time of 12 hours, with a nickel content of 16.469 ppm and a nickel recovery percent of 3.88%.","PeriodicalId":17695,"journal":{"name":"Jurnal Akademika Kimia","volume":null,"pages":null},"PeriodicalIF":0.0000,"publicationDate":"2022-05-30","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Extraction of Nickel from Morowali Laterite Ore with Nitric Acid\",\"authors\":\"I. W. Wirawan, D. K. Walanda, M. Napitupulu\",\"doi\":\"10.22487/j24775185.2022.v11.i2.pp91-95\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Nickel extraction from Morowali laterite ore has been carried out with nitric acid as the solvent. This study aims to determine the effect of nitric acid concentration, temperature, and stirring time on nickel content in laterite ore originating from Morowali. Morowali laterite seeds were extracted using the leaching method using nitric acid as the solvent with various concentrations of 0.5, 1, and 2, temperatures of 30, 60, and 95, and stirring times of 3, 6, and 12. Taguchi analysis was used in this study to obtain the effect of the three parameters used. The results showed that the optimum conditions were obtained at a concentration of 2 molars nitric acid, a temperature of 95°C, and a stirring time of 12 hours, with a nickel content of 16.469 ppm and a nickel recovery percent of 3.88%.\",\"PeriodicalId\":17695,\"journal\":{\"name\":\"Jurnal Akademika Kimia\",\"volume\":null,\"pages\":null},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-05-30\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Jurnal Akademika Kimia\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.22487/j24775185.2022.v11.i2.pp91-95\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Akademika Kimia","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.22487/j24775185.2022.v11.i2.pp91-95","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

以硝酸为溶剂从Morowali红土矿石中提取镍。本研究旨在确定硝酸浓度、温度和搅拌时间对Morowali红土矿石镍含量的影响。采用浸出法提取Morowali红土种子,溶剂为硝酸,浓度为0.5、1、2,温度为30、60、95,搅拌次数为3、6、12。本研究采用田口分析来获得所使用的三个参数的影响。结果表明,最佳工艺条件为:硝酸浓度为2 mol / l,温度为95℃,搅拌时间为12 h,镍含量为16.469 ppm,镍回收率为3.88%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Extraction of Nickel from Morowali Laterite Ore with Nitric Acid
Nickel extraction from Morowali laterite ore has been carried out with nitric acid as the solvent. This study aims to determine the effect of nitric acid concentration, temperature, and stirring time on nickel content in laterite ore originating from Morowali. Morowali laterite seeds were extracted using the leaching method using nitric acid as the solvent with various concentrations of 0.5, 1, and 2, temperatures of 30, 60, and 95, and stirring times of 3, 6, and 12. Taguchi analysis was used in this study to obtain the effect of the three parameters used. The results showed that the optimum conditions were obtained at a concentration of 2 molars nitric acid, a temperature of 95°C, and a stirring time of 12 hours, with a nickel content of 16.469 ppm and a nickel recovery percent of 3.88%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信