抗弯屈曲强度混凝土用粗骨料代替废塑料袋

Sudarmono Sudarmono, Karnawan Joko Setyono, Anung Suwarno
{"title":"抗弯屈曲强度混凝土用粗骨料代替废塑料袋","authors":"Sudarmono Sudarmono, Karnawan Joko Setyono, Anung Suwarno","doi":"10.32497/wahanats.v27i2.4146","DOIUrl":null,"url":null,"abstract":"Mix concrete practical 1pc: 2 ps: 3split, people used to build houses, has a specific gravity of 22-24 kN/m3. Density large concrete impact severity construction was, blend ingredients lightweight aggregates to produce lightweight concrete. One is used for lightweight aggregate material is waste plastic bags. Because the amount of waste plastic bags or piled carelessly discarded in landfills (TPA) impact of environmental pollution. This paper presents the study of the flexural strength and buckling the use of waste plastic bags as a partial replacement of coarse aggregate mix. The percentage of coarse aggregate replacement with waste plastic bag of approximately 30% is expected to produce flexural strength and buckling optimum reinforcement variation different. Bending beam size 10/15 cm length of 70 cm, variations in the tested reinforcement bending strength. While buckling strength using the dimensions of length 70 cm 10/10 with a variety of symmetrical and non symmetrical reinforcement. Effective capacity reinforcement ratio press the tensile reinforcement that generates maximum torque is 66.67%.","PeriodicalId":34836,"journal":{"name":"Prokons","volume":"18 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2022-12-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"BENDING AND BUCKLING STRENGTH CONCRETE WITH COARSE AGGREGATE REPLACEMENT WASTE PLASTIC BAGS\",\"authors\":\"Sudarmono Sudarmono, Karnawan Joko Setyono, Anung Suwarno\",\"doi\":\"10.32497/wahanats.v27i2.4146\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Mix concrete practical 1pc: 2 ps: 3split, people used to build houses, has a specific gravity of 22-24 kN/m3. Density large concrete impact severity construction was, blend ingredients lightweight aggregates to produce lightweight concrete. One is used for lightweight aggregate material is waste plastic bags. Because the amount of waste plastic bags or piled carelessly discarded in landfills (TPA) impact of environmental pollution. This paper presents the study of the flexural strength and buckling the use of waste plastic bags as a partial replacement of coarse aggregate mix. The percentage of coarse aggregate replacement with waste plastic bag of approximately 30% is expected to produce flexural strength and buckling optimum reinforcement variation different. Bending beam size 10/15 cm length of 70 cm, variations in the tested reinforcement bending strength. While buckling strength using the dimensions of length 70 cm 10/10 with a variety of symmetrical and non symmetrical reinforcement. Effective capacity reinforcement ratio press the tensile reinforcement that generates maximum torque is 66.67%.\",\"PeriodicalId\":34836,\"journal\":{\"name\":\"Prokons\",\"volume\":\"18 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2022-12-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Prokons\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.32497/wahanats.v27i2.4146\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Prokons","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.32497/wahanats.v27i2.4146","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

混合混凝土实用1pc: 2ps: 3split,人们用来建造房屋,比重为22-24 kN/m3。密度大的混凝土采用冲击烈度施工,掺加配料轻骨料制成轻混凝土。一种用于轻质集料的材料是废旧塑料袋。因为大量的废弃塑料袋或随意堆放在垃圾填埋场(TPA)影响环境污染。本文对废塑料袋部分替代粗骨料混合料的抗弯强度和屈曲性能进行了研究。粗骨料替换废塑料袋的比例约为30%,预计会产生不同的抗弯强度和屈曲最佳配筋变化。弯曲梁的尺寸为10/15 cm,长度为70 cm,受测钢筋的抗弯强度变化。同时屈曲强度采用尺寸长度为70 cm的10/10配以各种对称和非对称的钢筋。产生最大扭矩的受拉钢筋的有效容量配筋率为66.67%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
BENDING AND BUCKLING STRENGTH CONCRETE WITH COARSE AGGREGATE REPLACEMENT WASTE PLASTIC BAGS
Mix concrete practical 1pc: 2 ps: 3split, people used to build houses, has a specific gravity of 22-24 kN/m3. Density large concrete impact severity construction was, blend ingredients lightweight aggregates to produce lightweight concrete. One is used for lightweight aggregate material is waste plastic bags. Because the amount of waste plastic bags or piled carelessly discarded in landfills (TPA) impact of environmental pollution. This paper presents the study of the flexural strength and buckling the use of waste plastic bags as a partial replacement of coarse aggregate mix. The percentage of coarse aggregate replacement with waste plastic bag of approximately 30% is expected to produce flexural strength and buckling optimum reinforcement variation different. Bending beam size 10/15 cm length of 70 cm, variations in the tested reinforcement bending strength. While buckling strength using the dimensions of length 70 cm 10/10 with a variety of symmetrical and non symmetrical reinforcement. Effective capacity reinforcement ratio press the tensile reinforcement that generates maximum torque is 66.67%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
6
审稿时长
8 weeks
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:604180095
Book学术官方微信