L. M. Khoiroh, Asmaul Dwi Ayu Sholekah, E. Yulianti
{"title":"车床废渣中纳米赤铁矿颜料的结构与形貌","authors":"L. M. Khoiroh, Asmaul Dwi Ayu Sholekah, E. Yulianti","doi":"10.5539/IJC.V13N1P21","DOIUrl":null,"url":null,"abstract":"Hematite coated PEG was synthesized by the sonication-calcination method. A variation of Na2CO3 is investigated to know the effect on structure and morphology. Characterization of samples are using X-ray fluorescence, X-ray diffraction, Scanning electron microscopy, and color reader techniques. XRF data showed that iron is the highest element in the precursor. The X-ray diffraction data confirm that Fe(OH)3, α-FeOOH, and Fe3O4 established at the sonication stage are then transformed into the α-Fe2O3 phase after calcination. The X-ray diffraction data also was found that α-Fe2O3 at 0.5 M formed with the highest crystallinity degree. The scanning electron microscopy showed that the particle's shape is spherical, bar-shaped, and aggregate. However, the distribution of particles is not uniform and still displays agglomeration. The Color reader shows the highest degree of lightness obtained is at 1 M variation.","PeriodicalId":13866,"journal":{"name":"International Journal of Chemistry","volume":"39 1","pages":"21"},"PeriodicalIF":0.0000,"publicationDate":"2021-03-25","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"2","resultStr":"{\"title\":\"Structure and Morphology Properties of Nanoparticle Hematite Pigment from Lathe Waste\",\"authors\":\"L. M. Khoiroh, Asmaul Dwi Ayu Sholekah, E. Yulianti\",\"doi\":\"10.5539/IJC.V13N1P21\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Hematite coated PEG was synthesized by the sonication-calcination method. A variation of Na2CO3 is investigated to know the effect on structure and morphology. Characterization of samples are using X-ray fluorescence, X-ray diffraction, Scanning electron microscopy, and color reader techniques. XRF data showed that iron is the highest element in the precursor. The X-ray diffraction data confirm that Fe(OH)3, α-FeOOH, and Fe3O4 established at the sonication stage are then transformed into the α-Fe2O3 phase after calcination. The X-ray diffraction data also was found that α-Fe2O3 at 0.5 M formed with the highest crystallinity degree. The scanning electron microscopy showed that the particle's shape is spherical, bar-shaped, and aggregate. However, the distribution of particles is not uniform and still displays agglomeration. The Color reader shows the highest degree of lightness obtained is at 1 M variation.\",\"PeriodicalId\":13866,\"journal\":{\"name\":\"International Journal of Chemistry\",\"volume\":\"39 1\",\"pages\":\"21\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2021-03-25\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"2\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"International Journal of Chemistry\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.5539/IJC.V13N1P21\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"International Journal of Chemistry","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.5539/IJC.V13N1P21","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
Structure and Morphology Properties of Nanoparticle Hematite Pigment from Lathe Waste
Hematite coated PEG was synthesized by the sonication-calcination method. A variation of Na2CO3 is investigated to know the effect on structure and morphology. Characterization of samples are using X-ray fluorescence, X-ray diffraction, Scanning electron microscopy, and color reader techniques. XRF data showed that iron is the highest element in the precursor. The X-ray diffraction data confirm that Fe(OH)3, α-FeOOH, and Fe3O4 established at the sonication stage are then transformed into the α-Fe2O3 phase after calcination. The X-ray diffraction data also was found that α-Fe2O3 at 0.5 M formed with the highest crystallinity degree. The scanning electron microscopy showed that the particle's shape is spherical, bar-shaped, and aggregate. However, the distribution of particles is not uniform and still displays agglomeration. The Color reader shows the highest degree of lightness obtained is at 1 M variation.