不同材料压缩氢在管道输送过程中的损失对比分析

V. Bolobov, A. Petkova, G. G. Popov, V. Zlotin, I. U. Latipov, A. O. Sherstneva, I. Zhuikov
{"title":"不同材料压缩氢在管道输送过程中的损失对比分析","authors":"V. Bolobov, A. Petkova, G. G. Popov, V. Zlotin, I. U. Latipov, A. O. Sherstneva, I. Zhuikov","doi":"10.22349/1994-6716-2023-113-1-124-133","DOIUrl":null,"url":null,"abstract":"The authors estimate possible losses of transported compressed hydrogen (P = 10 MPa) due to diffusion through the pipe wall applying Sieverts law and Arrhenius equation and using tabular data on the coefficients of permeability and solubility. The calculation was carried out for pipelines made of various metallic and non-metallic materials at room and elevated temperatures. It is shown that the volume of the diffused gas at T = 298°K (25°С) is only fractions of a percent of the pumped hydrogen volume. At the same time, the biggest loss occurs in a pipeline made of polyethylene (~0.03%), and the most insignificant one in austenitic steels (~10-6%). For carbon and low-alloy steels, the main materials of gas pipelines, these losses are at the level of 10-4–10-5 %. When the temperature rises to 683°K (410°C), the losses in steel pipelines increase to 0.25%, in polymer pipelines to 20%.","PeriodicalId":23679,"journal":{"name":"Voprosy Materialovedeniya","volume":"1 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"2023-04-27","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Comparative analysis of compressed hydrogen losses during its transportation through the pipelines from different materials\",\"authors\":\"V. Bolobov, A. Petkova, G. G. Popov, V. Zlotin, I. U. Latipov, A. O. Sherstneva, I. Zhuikov\",\"doi\":\"10.22349/1994-6716-2023-113-1-124-133\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"The authors estimate possible losses of transported compressed hydrogen (P = 10 MPa) due to diffusion through the pipe wall applying Sieverts law and Arrhenius equation and using tabular data on the coefficients of permeability and solubility. The calculation was carried out for pipelines made of various metallic and non-metallic materials at room and elevated temperatures. It is shown that the volume of the diffused gas at T = 298°K (25°С) is only fractions of a percent of the pumped hydrogen volume. At the same time, the biggest loss occurs in a pipeline made of polyethylene (~0.03%), and the most insignificant one in austenitic steels (~10-6%). For carbon and low-alloy steels, the main materials of gas pipelines, these losses are at the level of 10-4–10-5 %. When the temperature rises to 683°K (410°C), the losses in steel pipelines increase to 0.25%, in polymer pipelines to 20%.\",\"PeriodicalId\":23679,\"journal\":{\"name\":\"Voprosy Materialovedeniya\",\"volume\":\"1 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2023-04-27\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Voprosy Materialovedeniya\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.22349/1994-6716-2023-113-1-124-133\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Voprosy Materialovedeniya","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.22349/1994-6716-2023-113-1-124-133","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0

摘要

作者利用Sieverts定律和Arrhenius方程,并利用渗透性系数和溶解度系数的表格数据,估计了由于通过管壁扩散而输送的压缩氢(P = 10 MPa)的可能损失。在室温和高温条件下,对各种金属和非金属材料制成的管道进行了计算。结果表明,在T = 298°K(25°С)时,扩散气体的体积仅为抽吸氢体积的百分之一。同时,聚乙烯管道损耗最大(~0.03%),奥氏体钢管道损耗最小(~10-6%)。对于输气管道的主要材料碳素钢和低合金钢,这些损失在10-4 - 10- 5%水平。当温度升高到683°K(410°C)时,钢管管道的损失增加到0.25%,聚合物管道的损失增加到20%。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
Comparative analysis of compressed hydrogen losses during its transportation through the pipelines from different materials
The authors estimate possible losses of transported compressed hydrogen (P = 10 MPa) due to diffusion through the pipe wall applying Sieverts law and Arrhenius equation and using tabular data on the coefficients of permeability and solubility. The calculation was carried out for pipelines made of various metallic and non-metallic materials at room and elevated temperatures. It is shown that the volume of the diffused gas at T = 298°K (25°С) is only fractions of a percent of the pumped hydrogen volume. At the same time, the biggest loss occurs in a pipeline made of polyethylene (~0.03%), and the most insignificant one in austenitic steels (~10-6%). For carbon and low-alloy steels, the main materials of gas pipelines, these losses are at the level of 10-4–10-5 %. When the temperature rises to 683°K (410°C), the losses in steel pipelines increase to 0.25%, in polymer pipelines to 20%.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
确定
请完成安全验证×
copy
已复制链接
快去分享给好友吧!
我知道了
右上角分享
点击右上角分享
0
联系我们:info@booksci.cn Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。 Copyright © 2023 布克学术 All rights reserved.
京ICP备2023020795号-1
ghs 京公网安备 11010802042870号
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术官方微信