{"title":"HgGa2S4中的二次谐波产生","authors":"E. Takaoka, K. Kato","doi":"10.1364/cleo_europe.1998.cfh7","DOIUrl":null,"url":null,"abstract":"This paper reports what is believed to be the first attainment of tunable SHG in HgGa2S41,2. The HgGa2S4 crystal used in this experiment was 8 × 8 × 8 mm3 and fabricated at θ = 67.5° (θ = 22.5°) and ϕ = 0° with polished four side surfaces. The transmission range is 0.55 – 12.4 μm.","PeriodicalId":10610,"journal":{"name":"Conference on Lasers and Electro-Optics Europe","volume":"24 1","pages":""},"PeriodicalIF":0.0000,"publicationDate":"1998-01-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":"{\"title\":\"Second-Harmonic Generation in HgGa2S4\",\"authors\":\"E. Takaoka, K. Kato\",\"doi\":\"10.1364/cleo_europe.1998.cfh7\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"This paper reports what is believed to be the first attainment of tunable SHG in HgGa2S41,2. The HgGa2S4 crystal used in this experiment was 8 × 8 × 8 mm3 and fabricated at θ = 67.5° (θ = 22.5°) and ϕ = 0° with polished four side surfaces. The transmission range is 0.55 – 12.4 μm.\",\"PeriodicalId\":10610,\"journal\":{\"name\":\"Conference on Lasers and Electro-Optics Europe\",\"volume\":\"24 1\",\"pages\":\"\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1998-01-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"0\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Conference on Lasers and Electro-Optics Europe\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1364/cleo_europe.1998.cfh7\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Conference on Lasers and Electro-Optics Europe","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1364/cleo_europe.1998.cfh7","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
This paper reports what is believed to be the first attainment of tunable SHG in HgGa2S41,2. The HgGa2S4 crystal used in this experiment was 8 × 8 × 8 mm3 and fabricated at θ = 67.5° (θ = 22.5°) and ϕ = 0° with polished four side surfaces. The transmission range is 0.55 – 12.4 μm.